# US 2010/0163974 A1 · Semiconductor device with vertical channel transistor and method for fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0163974 A1
- Document ID: US20100163974A1
- Status: Published application
- Kind: A1
- Application number: 12/492,831
- Filed: 2009-06-26
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Inventors: Seung-Chul Oh
- Web page: https://patentgrep.com/patent/US20100163974A1

## CPC

- H10D 30/63: Vertical IGFETs (H10D30/66 {, H10D30/6728, H10D30/689, H10D30/693} take precedence)
- H10B 12/053: {the transistor being at least partially in a trench in the substrate (vertical transistor in combination with a capacitor formed in a substrate trench H10B12/0383)}
- H10D 30/025: {of vertical IGFETs (of VDMOS H10D30/0291; of vertical TFTs H10D30/0318)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A method for fabricating a semiconductor device including a vertical channel transistor includes providing a substrate including a semiconductor pillar, forming a gate electrode surrounding the semiconductor pillar, forming an impurity region for a bit line by doping impurities into the substrate and forming a device isolation trench by etching a portion of the substrate including the impurity region to a certain depth, thereby defining the bit line, wherein the impurity doping is performed with given concentration so as to form the impurity region under the semiconductor pillar.

## Claims

### Claim 1

A method for fabricating a semiconductor device including a vertical channel transistor, the method comprising:
providing a substrate including a semiconductor pillar;
forming a gate electrode surrounding the semiconductor pillar;
forming an impurity region for a bit line by doping impurities into the substrate; and
forming a device isolation trench by etching a portion of the substrate including the impurity region to a certain depth, thereby defining the bit line,
wherein the impurity doping is performed with given concentration so as to form the impurity region under the semiconductor pillar.

### Claim 2 (depends on 1)

The method of claim 1, wherein the impurities are N type impurities.

### Claim 3 (depends on 1)

The method of claim 1, wherein the given concentration is greater than approximately 1015 atoms/cm2.

### Claim 4

A semiconductor device including a vertical channel transistor, the semiconductor device comprising:
a substrate including a semiconductor pillar;
a gate electrode surrounding the semiconductor pillar; and
a bit line defined by a device isolation trench and formed by doping impurities into the substrate,
wherein the doping concentration of the impurities has a given value so as to form the bit line under the semiconductor pillar.

### Claim 5 (depends on 4)

The semiconductor device of claim 4, wherein the impurities are N type impurities.

### Claim 6 (depends on 4)

The semiconductor device of claim 4, wherein the given value is greater than approximately 1015 atoms/cm2.

### Claim 7 (depends on 4)

The semiconductor device of claim 4, wherein the semiconductor pillar surrounded by the gate electrode includes a fully depleted channel.

### Claim 8

A semiconductor device including a vertical channel transistor, the semiconductor device comprising:
a substrate including a semiconductor pillar;
a gate electrode surrounding the semiconductor pillar; and
a bit line bounded by a device isolation trench and formed by doping impurities into the substrate,
wherein the bit line extends across an entire width of an area of the substrate covered by the semiconductor pillar.

### Claim 9 (depends on 8)

The semiconductor device of claim 8, wherein the impurities are N type impurities.

### Claim 10 (depends on 8)

The semiconductor device of claim 8, wherein the impurity doping is performed with an impurity concentration greater than approximately 1015 atoms/cm2.

### Claim 11 (depends on 8)

The semiconductor device of claim 8, wherein the semiconductor pillar surrounded by the gate electrode includes a fully depleted channel.