# US 2010/0163868 A1 · Semiconductor device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0163868 A1
- Document ID: US20100163868A1
- Status: Published application
- Kind: A1
- Application number: 12/646,085
- Filed: 2009-12-23
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Shunpei YAMAZAKI; Junichiro SAKATA; Jun KOYAMA
- Web page: https://patentgrep.com/patent/US20100163868A1

## CPC

- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10D 62/80: characterised by the materials
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/441: {Interconnections, e.g. scanning lines}
- H10D 86/60: wherein the TFTs are in active matrices
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/3426: {Oxides}
- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device which includes a thin film transistor having an oxide semiconductor layer and excellent electrical characteristics is provided. Further, a method for manufacturing a semiconductor device in which plural kinds of thin film transistors of different structures are formed over one substrate to form plural kinds of circuits and in which the number of steps is not greatly increased is provided. After a metal thin film is formed over an insulating surface, an oxide semiconductor layer is formed thereover. Then, oxidation treatment such as heat treatment is performed to oxidize the metal thin film partly or entirely. Further, structures of thin film transistors are different between a circuit in which emphasis is placed on the speed of operation, such as a logic circuit, and a matrix circuit.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, comprising:
forming a gate electrode over an insulating surface;
forming an insulating layer over the gate electrode;
forming a metal thin film over the insulating layer;
forming an oxide semiconductor layer over the metal thin film; and
performing oxidation treatment on at least a part of the metal thin film after forming the oxide semiconductor layer.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor device, according to claim 1,
wherein the oxidation treatment is heat treatment which is performed in any one of an atmosphere containing oxygen, air, and a nitrogen atmosphere.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor device, according to claim 1,
wherein the oxide semiconductor layer contains at least one of indium, gallium, and zinc.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor device, according to claim 1,
wherein the metal thin film contains at least one of indium, zinc, tin, molybdenum, and tungsten.

### Claim 5 (depends on 1)

The method for manufacturing a semiconductor device, according to claim 1,
wherein at least one of elements which are contained in the oxide semiconductor layer is the same as an element contained in the metal thin film.

### Claim 6 (depends on 1)

The method for manufacturing a semiconductor device, according to claim 1,
wherein the metal thin film is formed by any one of a sputtering method, a vacuum vapor deposition method, and a coating method.

### Claim 7 (depends on 1)

The method for manufacturing a semiconductor device, according to claim 1,
wherein a thickness of the oxide semiconductor layer is 30 nm to 150 nm, inclusive.

### Claim 8 (depends on 1)

The method for manufacturing a semiconductor device, according to claim 1,
wherein a thickness of the metal thin film is smaller than a thickness of the oxide semiconductor layer.

### Claim 9

A semiconductor device comprising:
a matrix circuit and a driver circuit which drives the matrix circuit over an insulating surface,
wherein the driver circuit comprises a first thin film transistor including a stack of a first oxide semiconductor layer and a second oxide semiconductor layer, the stack overlapping with a first gate electrode with a first gate insulating film interposed therebetween,
wherein the matrix circuit includes a second thin film transistor, the second thin film transistor including a third oxide semiconductor layer overlapping with a second gate electrode with a second gate insulating film interposed therebetween,
wherein the first oxide semiconductor layer comprises a first material,
wherein the second oxide semiconductor layer comprises a second material being different from the first material, and
wherein the third oxide semiconductor layer comprises the second material.

### Claim 10 (depends on 9)

The semiconductor device according to claim 9,
wherein electrical resistivity of the first oxide semiconductor layer is lower than electrical resistivity of the second oxide semiconductor layer.

### Claim 11 (depends on 9)

The semiconductor device according to claim 9,
wherein the first gate insulating film is over the first gate electrode,
wherein the first oxide semiconductor layer is over the first gate insulating film, and
wherein the second oxide semiconductor layer is over the first oxide semiconductor layer.

### Claim 12 (depends on 9)

The semiconductor device according to claim 9,
wherein the second gate insulating film is over the second gate electrode, and
wherein the third oxide semiconductor layer is over the second gate insulating film.

### Claim 13 (depends on 9)

The semiconductor device according to claim 9,
wherein the second oxide semiconductor layer contains at least one of indium, gallium, and zinc.

### Claim 14 (depends on 9)

The semiconductor device according to claim 9,
wherein a thickness of the second oxide semiconductor layer and a thickness of the third oxide semiconductor layer are each 30 nm to 150 nm, inclusive.

### Claim 15 (depends on 9)

The semiconductor device according to claim 9,
wherein a thickness of the first oxide semiconductor layer is smaller than a thickness of the second oxide semiconductor layer.

### Claim 16

A method for manufacturing a semiconductor device comprising a matrix circuit and a driver circuit configured to drive the matrix circuit over a substrate, comprising:
forming a first oxide semiconductor layer over the substrate in a matrix circuit region and a driver circuit region;
removing the first oxide semiconductor layer from the matrix circuit region by etching; and
forming a second oxide semiconductor layer and a third oxide semiconductor layer, the second oxide semiconductor layer being formed over the first oxide semiconductor layer in the driver circuit region and the third oxide semiconductor layer being formed over the substrate in the matrix circuit region,
wherein a first thin film transistor in the driver circuit region comprises a stack of the first oxide semiconductor layer and the second oxide semiconductor layer, and
wherein a second thin film transistor in the matrix circuit region comprises the third oxide semiconductor layer.

### Claim 17 (depends on 16)

The method for manufacturing a semiconductor device, according to claim 16,
wherein electrical resistivity of the first oxide semiconductor layer is lower than electrical resistivity of the second oxide semiconductor layer.

### Claim 18 (depends on 16)

The method for manufacturing a semiconductor device, according to claim 16,
wherein the first oxide semiconductor layer comprises a first material,
wherein the second oxide semiconductor layer comprises a second material being different from the first material, and
wherein the third oxide semiconductor layer comprises the second material.

### Claim 19

A method for manufacturing a semiconductor device which includes a matrix circuit and a driver circuit configured to drive the matrix circuit over a substrate, comprising:
forming a metal thin film over the substrate in a matrix circuit region and a driver circuit region;
removing the metal thin film from the matrix circuit region by etching;
forming a first oxide semiconductor layer over the metal thin film in the driver circuit region and over the substrate in the matrix circuit region; and
forming a second oxide semiconductor layer by performing oxidation treatment on the metal thin film after forming the oxide semiconductor layer,
wherein a first thin film transistor comprises a stack of the first oxide semiconductor layer and the second oxide semiconductor layer in the driver circuit region, and
wherein a second thin film transistor comprises a third oxide semiconductor layer in the matrix circuit region.

### Claim 20 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein the oxidation treatment is heat treatment which is performed in any one of an atmosphere containing oxygen, air, and a nitrogen atmosphere.

### Claim 21 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein the first oxide semiconductor layer contains at least one of indium, gallium, and zinc.

### Claim 22 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein the metal thin film contains at least one of indium, zinc, tin, molybdenum, and tungsten.

### Claim 23 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein at least one of elements which are contained in the second oxide semiconductor layer is the same as an element contained in the metal thin film.

### Claim 24 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein the metal thin film is formed by any one of a sputtering method, a vacuum vapor deposition method, and a coating method.

### Claim 25 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein a thickness of the first oxide semiconductor layer is 30 nm to 150 nm, inclusive.

### Claim 26 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein a thickness of the metal thin film is smaller than a thickness of the first oxide semiconductor layer.

### Claim 27 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein electrical resistivity of the second oxide semiconductor layer is lower than electrical resistivity of the first oxide semiconductor layer.

### Claim 28 (depends on 19)

The method for manufacturing a semiconductor device, according to claim 19,
wherein the first oxide semiconductor layer comprises a first material,
wherein the second oxide semiconductor layer comprises a second material being different from the first material, and
wherein the third oxide semiconductor layer comprises the first material.