# US 2010/0163860 A1 · Semiconductor thin film, method for manufacturing the same, thin film transistor, and active-matrix-driven display panel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0163860 A1
- Document ID: US20100163860A1
- Status: Published application
- Kind: A1
- Application number: 12/094,228
- Filed: 2006-11-16
- Published: 2010-07-01
- Earliest claimed: 2005-11-18
- Assignees: Idemitsu Kosan Co., Ltd.
- Inventors: Koki Yano; Kazuyoshi Inoue; Nobuo Tanaka; Tokie Tanaka
- Web page: https://patentgrep.com/patent/US20100163860A1

## CPC

- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- Y10S 977/773: Nanoparticle, i.e. structure having three dimensions of 100 nm or less
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Disclosed is a semiconductor thin film which can be formed at a relatively low temperature even on a flexible resin substrate. Since the semiconductor thin film is stable to visible light and has high device characteristics such as transistor characteristics, in the case where the semiconductor thin film is used as a switching device for driving a display, even when overlapped with a pixel part, the luminance of a display panel does not deteriorate. Specifically, a transparent semiconductor thin film 40 is produced by forming an amorphous film containing zinc oxide and indium oxide and then oxidizing the film so that the resulting film has a carrier density of 10+17 cm−3 or less, a Hall mobility of 2 cm2/V·sec or higher, and an energy band gap of 2.4 EV or more.

## Claims

### Claim 1

A semiconductor thin film made by an amorphous film containing zinc oxide, and indium oxide and whose carrier density is 10+17 cm−3 or less, Hall mobility is 2 cm2/V·sec or higher, and energy band gap is 2.4 eV or more.

### Claim 2 (depends on 1)

The semiconductor thin film according to claim 1, wherein atom ratio between zinc [Zn] and indium [In] in the amorphous film is expressed as Zn/(Zn+In)=0.10 to 0.82.

### Claim 3 (depends on 1)

The semiconductor thin film according to claim 1, wherein atom ratio between zinc [Zn] and indium [In] in the amorphous film is expressed as Zn/(Zn+In)=0.51 to 0.80.

### Claim 4 (depends on 1)

The semiconductor thin film according to claim 1, wherein transmittance of wavelength of 550 nm is 75% or higher.

### Claim 5 (depends on 1)

The semiconductor thin film according to claim 1, wherein the semiconductor thin film is a non-degenerate semiconductor thin film having a work function of 3.5 to 6.5 eV.

### Claim 6 (depends on 1)

The semiconductor thin film according to claim 1, wherein nanocrystals are dispersed in the amorphous film.

### Claim 7 (depends on 1)

The semiconductor thin film according to claim 1, further containing a third metallic element [M], wherein atom ratio [M/(M+In)] between the third metallic element [M] and indium [In] is 0 to 0.5.

### Claim 8 (depends on 1)

The transparent oxide semiconductor thin film according to claim 1, further containing a third metallic element [M], wherein atom ratio [M/(M+In)] between the third metallic element [M] and indium [In] is 0 to 0.3.

### Claim 9 (depends on 1)

The semiconductor thin film according to claim 1, wherein a maximum value of a radial distribution function (RDF) obtained by X-ray scatter measurement in an atomic distance of 0.3 to 0.36 nm is A and a maximum value of the RDF in an atomic distance of 0.36 to 0.42 nm is B, relation A/B>0.8 is satisfied.

### Claim 10 (depends on 1)

A method for manufacturing a semiconductor thin film according to claim 1, wherein an amorphous film containing zinc oxide and indium oxide is formed under condition that a partial pressure of water H2O in an atmospheric gas is 10−3 Pa or less.

### Claim 11 (depends on 10)

The method for manufacturing a semiconductor thin film according to claim 10, further comprising a step of oxidizing the amorphous film physically formed at a substrate temperature of 200° C. or less.

### Claim 12 (depends on 1)

A thin film transistor comprising the semiconductor thin film according to claim 1.

### Claim 13 (depends on 12)

The thin film transistor according to claim 12, wherein the semiconductor thin film is provided on a resin substrate.

### Claim 14 (depends on 12)

An active-matrix-driven display panel comprising the thin film transistor according to claim 12.