# US 2010/0163843 A1 · Room temperature-operating single-electron device and the fabrication method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0163843 A1
- Document ID: US20100163843A1
- Status: Published application
- Kind: A1
- Application number: 12/305,770
- Filed: 2008-09-11
- Published: 2010-07-01
- Earliest claimed: 2007-09-14
- Assignees: Chungbuk National University Industry-Academic Cooperation Foundation
- Inventors: Jung Bum Choi; Chang Keun Lee; Min Sik Kim
- Web page: https://patentgrep.com/patent/US20100163843A1

## CPC

- H10D 30/402: {Single electron transistors; Coulomb blockade transistors}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/014: {of FETs having zero-dimensional [0D] or one-dimensional [1D] channels, e.g. quantum wire FETs, single-electron transistors [SET] or Coulomb blockade transistors}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

The present invention relates to a room temperature-operating single-electron device and a fabrication method thereof, and more particularly, to a room temperature-operating single-electron device in which a plurality of metal silicide dots formed serially is used as multiple quantum dots, and a fabrication method thereof.

## Claims

### Claim 1

A fabrication method of a room temperature-operating single-electron device, the method comprising:
a first step of arming an SOI substrate by sequentially stacking an insulating layer 11 and a silicon layer 10 on a silicon substrate 12, and etching the silicon layer 10 of the SOI substrate to thereby form an active region 10a;
a second step of forming a mask 20 on a central channel portion of the active region 10a, and injecting impurity ions into a part of the active region 10a to form a source region and a drain region;
a third step of arming a silicon oxide film 30 on the entire top surface of the SOI substrate;
a fourth step of etching the channel portion of the active region 10a to form a silicide trench 31;
a fifth step of depositing an oxide film 40 on the entire top surface of the SOI substrate;
a sixth step of depositing a metal film 42 on the entire top surface of the oxide film;
a seventh step of thermally treating a part of the metal film 42 to achieve silicidization of the metal dots, and removing the silicon oxide film 30 and the metal film 42 which is not silicidized to form serially-arrayed silicide quantum dots 41;
an eighth step of depositing gate oxide films 50a and 50b on the entire top surface of the SOI substrate;
a ninth step of etching a part of the gate oxide films 50a and 50b positioned on the top of a source 13 and a drain 14 formed on both ends of the active region 10a to form each contact hole, and depositing a metal film to fill the contact hole to form a source pad 60 and a drain pad 61; and
a tenth step of forming a resist pattern on the silicide trench 31 to form a gate.

### Claim 2 (depends on 1)

The fabrication method according to claim 1, wherein the active region 10a has a length of 1 to 100 nm and a width of 10 to 15 nm.

### Claim 3 (depends on 1)

The fabrication method according to claim 1, wherein the active region 10a is formed by means of photolithography, electronic beam lithography or reactive ion etching.

### Claim 4 (depends on 1)

The fabrication method according to claim 1, wherein the silicon oxide film 30 has a thickness of 2 to 10 nm.

### Claim 5 (depends on 1)

The fabrication method according to claim 1, wherein in the third step, the silicon layer 10 has a thickness of 40 to 45 nm and a width of 6 to 10 nm.

### Claim 6 (depends on 1)

The fabrication method according to claim 1, wherein in the fourth step, the channel portion of the active region 10a is etched by means of reactive ion etching to have a thickness of 2 to 10 nm.

### Claim 7 (depends on 1)

The fabrication method according to claim 1, wherein in the fifth step, the oxide film 40 is formed in such a fashion as to be left to stand in a hydrogen peroxide solution (H2O2) or in the air.

### Claim 8 (depends on 1)

The fabrication method according to claim 1, wherein in the sixth step, the metal film 42 is made of cobalt.

### Claim 9 (depends on 1)

The fabrication method according to claim 1, wherein in the sixth step, the meal film 42 is deposited by means of electronic beam evaporator or molecular beam epitaxy (MBE) equipment in such a fashion that its thickness is within a range from 0.1 to 1 nm.

### Claim 10 (depends on 1)

The fabrication method according to claim 1, wherein in the seventh step, the metal film 42 is thermally treated through an electronic beam lithography process to form the silicide quantum dots 41.

### Claim 11 (depends on 1)

The fabrication method according to claim 1, wherein the silicon oxide film 30 is removed by using a buffered oxide etchant (BOE) and the non-silicidized metal film 42 is removed by using a mixed solution of sulfuric acid and hydrogen peroxide solution.

### Claim 12 (depends on 11)

The fabrication method according to claim 11, wherein each of the silicide quantum dots 41 has a diameter of 2 to 10 nm and the number of the silicide quantum dots is 1 to 50.

### Claim 13 (depends on 1)

The fabrication method according to claim 1, wherein in the eighth step, the gate oxide film is formed to a thickness of 30 to 50 nm by a chemical vapor deposition (CVD).

### Claim 14 (depends on 1)

The fabrication method according to claim 1, wherein in the eighth step, the gate oxide film has a thickness of 100 to 300 nm, and the gate oxide film on the silicide trench 31 is formed to a thickness of 30 to 50 nm by a chemical vapor deposition (CVD).

### Claim 15 (depends on 2)

The fabrication method according to claim 2, wherein in the tenth step, the gate is a control gate 62 or a ‘T’-shaped gate 63.

### Claim 16 (depends on 1)

The fabrication method according to claim 1, wherein the gate has a thickness of 100 to 500 nm.

### Claim 17

A fabrication method of a room temperature-operating single-electron device, the method comprising:
a first step of forming an SOI substrate by sequentially stacking an insulating layer 11 and a silicon layer 10 on a silicon substrate 12, and etching the silicon layer 10 of the SOI substrate to thereby form an active region 10a;
a second step of forming a mask 20 on a central channel portion of the active region 10a, and injecting impurity ions into the active region 10a to form a source region and a drain region;
a third step of forming a silicon oxide film 30 on the entire top surface of the SOI substrate;
a fourth step of etching the channel portion of the active region 10a by using the silicon oxide film 30 of the channel portion as a mask to form a silicide trench 31;
a fifth step of depositing a metal film 42 on the entire top surface of the SOI substrate and subjecting the metal film to silicidization;
a sixth step of removing the silicon oxide film 30 and the metal film 42 which is not silicidized to form serially-arrayed silicide quantum dots 41;
a seventh step of forming a protective film 70 on the entire top surface of the SOI substrate;
an eighth step of etching the protective film 70 positioned on the top of a source and a drain formed on both ends of the active region 10a to form each contact hole, and depositing a metal film to fill the contact hole to form a source pad 60 and a drain pad 61; and
a ninth step of depositing a metal film on the underside of the SOI substrate to form a bottom gate.

### Claim 18 (depends on 1)

A room temperature-operating single-electron device fabricated by the fabrication method according to claim 1.

### Claim 19 (depends on 17)

A room temperature-operating single-electron device fabricated by the fabrication method according to claim 17.