# US 2010/0163831 A1 · Deposited semiconductor structure to minimize n-type dopant diffusion and method of making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0163831 A1
- Document ID: US20100163831A1
- Status: Published application
- Kind: A1
- Application number: 12/632,013
- Filed: 2009-12-07
- Published: 2010-07-01
- Earliest claimed: 2004-09-29
- Assignees: SanDisk 3D LLC
- Inventors: S. Brad Herner
- Web page: https://patentgrep.com/patent/US20100163831A1

## CPC

- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10B 63/20: {comprising selection components having two electrodes, e.g. diodes}
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 62/832: being Group IV materials comprising two or more elements, e.g. SiGe
- H10N 70/20: Multistable switching devices, e.g. memristors
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/883: {Oxides or nitrides}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A microelectronic structure including a layerstack is provided, the layerstack including: (a) a first layer including semiconductor material that is very heavily n-doped before being annealed, having a first-layer before-anneal dopant concentration, the first layer being between about 50 and 200 angstroms thick, wherein the first layer is above a substrate, and wherein the first layer is heavily n-doped after being annealed, having a first-layer after-anneal dopant concentration, the first-layer before-anneal dopant concentration exceeding the first-layer after-anneal concentration; (b) a second layer including semiconductor material that is not heavily doped before being annealed, having a second-layer before-anneal dopant concentration, the second layer being about as thick as the first layer, wherein the second layer is above and in contact with the first layer, and wherein the second layer includes heavily n-doped semiconductor material after being annealed, having a second-layer after-anneal dopant concentration, the second-layer after-anneal dopant concentration exceeding the second-layer before-anneal concentration; and (c) a third layer including semiconductor material that is above and in contact with the second layer and that is not heavily n-doped before or after being annealed, the third layer having a third-layer dopant concentration.

## Claims

### Claim 1

A microelectronic structure comprising a layerstack, the layerstack comprising:
a first layer comprising semiconductor material that is very heavily n-doped before being annealed, having a first-layer before-anneal dopant concentration, the first layer being between about 50 and 200 angstroms thick, wherein the first layer is above a substrate, and wherein the first layer is heavily n-doped after being annealed, having a first-layer after-anneal dopant concentration, the first-layer before-anneal dopant concentration exceeding the first-layer after-anneal concentration;
a second layer comprising semiconductor material that is not heavily doped before being annealed, having a second-layer before-anneal dopant concentration, the second layer being about as thick as the first layer, wherein the second layer is above and in contact with the first layer, and wherein the second layer comprises heavily n-doped semiconductor material after being annealed, having a second-layer after-anneal dopant concentration, the second-layer after-anneal dopant concentration exceeding the second-layer before-anneal concentration; and
a third layer comprising semiconductor material that is above and in contact with the second layer and that is not heavily n-doped before or after being annealed, the third layer having a third-layer dopant concentration.

### Claim 2 (depends on 1)

The microelectronic structure of claim 1, wherein the first layer and the second layer comprise semiconductor material comprising a similar mixture of semiconductors.

### Claim 3 (depends on 2)

The microelectronic structure of claim 2, wherein the first layer and the second layer comprise a silicon-germanium alloy that is at least 10 at % germanium.

### Claim 4 (depends on 2)

The microelectronic structure of claim 2, wherein the first layer and the second layer comprise a silicon-germanium alloy that is less than 10 at % germanium.

### Claim 5 (depends on 2)

The microelectronic structure of claim 2, wherein the third layer comprises a silicon-germanium alloy that is at least 10 at % germanium.

### Claim 6 (depends on 5)

The microelectronic structure of claim 5, wherein the third layer comprises at least 20 at % germanium.

### Claim 7 (depends on 5)

The microelectronic structure of claim 5, further comprising a fourth layer comprising a semiconductor material that is above and in contact with the third layer and that is not heavily n-doped, wherein the fourth layer comprises silicon or a silicon-germanium alloy that is less than 10 at % germanium.

### Claim 8 (depends on 7)

The microelectronic structure of claim 7, wherein the fourth layer comprises no more than 5 at % germanium.

### Claim 9 (depends on 1)

The microelectronic structure of claim 1, wherein the first, second, and third layers are portions of a vertically oriented junction diode.

### Claim 10 (depends on 9)

The microelectronic structure of claim 9, wherein the diode is a p-i-n diode, and the third layer is undoped or lightly doped.

### Claim 11 (depends on 10)

The microelectronic structure of claim 10, further comprising:
a fourth layer comprising a semiconductor material that is above and in contact with the third layer;
wherein the fourth layer comprises silicon or a silicon-germanium alloy that is less than 10 at % germanium; the fourth layer is heavily p-doped; and the fourth layer is a portion of the vertically oriented junction diode; and
wherein the third layer comprises a silicon-germanium alloy that is at least 10 at % germanium.

### Claim 12 (depends on 11)

The microelectronic structure of claim 11, wherein the diode is vertically disposed between a bottom conductor and a top conductor, wherein a nonvolatile memory cell comprises a portion of the bottom conductor, the diode, and a portion of the top conductor.

### Claim 13 (depends on 12)

The microelectronic structure of claim 12, wherein the first, second, third and fourth layers have been patterned and etched to form a pillar.

### Claim 14 (depends on 12)

The microelectronic structure of claim 12, wherein the non-volatile memory cell resides in a monolithic three dimensional memory array comprising:
a) a first memory level formed above the substrate, the first memory level comprising:
i) a plurality of the bottom conductors, the bottom conductors being substantially parallel and substantially coplanar;
ii) a plurality of the top conductors, the top conductors being substantially parallel and substantially coplanar; and
iii) a plurality of the non-volatile memory cells; and
b) at least a second memory level monolithically formed above the first memory level.

### Claim 15 (depends on 12)

The microelectronic structure of claim 12, wherein the memory cell further comprises a reversible state-change element, the reversible state-change element disposed between the diode and the bottom conductor or between the diode and the top conductor.

### Claim 16 (depends on 15)

The microelectronic structure of claim 15, wherein the reversible state-change element comprises a layer of a resistivity-switching metal oxide or nitride compound selected from the group consisting of NiO, Nb2O5, TiO2, HfO2, Al2O3, CoO, MgOx, CrO2, VO, BN, and AlN.

### Claim 17 (depends on 1)

The microelectronic structure of claim 1, wherein the second-layer before-anneal dopant concentration and the third-layer dopant concentration are less than about 5×1017 dopant atoms/cm3 of an n-type dopant, and wherein the first-layer after-anneal dopant concentration and the second-layer after-anneal dopant concentration are at least about 5×1019 dopant atoms/cm3.