# US 2010/0163141 A1 · Mg ALLOY AND METHOD OF PRODUCTION OF SAME

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0163141 A1
- Document ID: US20100163141A1
- Status: Published application
- Kind: A1
- Application number: 12/532,856
- Filed: 2008-03-26
- Published: 2010-07-01
- Earliest claimed: 2007-03-26
- Assignees: Toyota Jidosha Kabushiki Kaisha; National Institute for Materials Science
- Inventors: Tetsuya Shoji; Akira Kato; Toshiji Mukai; Hidetoshi Somekawa
- Web page: https://patentgrep.com/patent/US20100163141A1

## CPC

- C22C 23/06: with a rare earth metal as the next major constituent
- C22F 1/002: {by rapid cooling or quenching; cooling agents used therefor}
- C22F 1/06: of magnesium or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

An Mg alloy provided with high strength and high ductility by matching the strength and ductility in tensile deformation and compressive deformation at the same levels is provided. The Mg alloy of the present invention is characterized by having a chemical composition consisting of Y: 0.1 to 1.5 at % and a balance of Mg and unavoidable impurities and having a microstructure with high Y regions with Y concentrations higher than an average Y concentration distributed at nanometer order sizes and intervals. The present invention further provides an Mg alloy characterized by having a chemical composition consisting of Y: more than 0.1 at % and a valance of Mg and unavoidable impurities, having a microstructure with high Y regions with Y concentrations higher than an average Y concentration distributed at nanometer order sizes and intervals and having an average recrystallized grain size within the range satisfying the following formula 1: −0.87c+1.10<log d<1.14c+1.48, formula 1 where c: Y content (at %) and d: average recrystallized grain size (μm).

## Claims

### Claim 1

An Mg alloy characterized by having a chemical composition consisting of Y: 0.1 to 1.5 at % and a balance of Mg and unavoidable impurities and having a microstructure with high Y regions with Y concentrations higher than an average Y concentration distributed at nanometer order sizes and intervals.

### Claim 2 (depends on 1)

An Mg alloy as set: forth in claim 1, characterized by being an equiaxed grain structure and not having texture.

### Claim 3 (depends on 1, 2)

A method of production of an Mg alloy as set forth in claim 1 or 2, characterized by hot working an alloy having a chemical composition as set forth in claim 1, then isothermally heat treating it to form a microstructure as set forth in claim 1.

### Claim 4

An Mg alloy characterized by having a chemical composition consisting of Y: more than 0.1 at % and a balance of Mg and unavoidable impurities, having a microstructure with high Y regions with Y concentrations higher than an average Y concentration distributed at nanometer order sizes and intervals and having an average crystal grain size within the range satisfying the following formula 1:
−0.87c+1.10<log d<1.14c+1.48 formula 1
where c: Y content (at %) and
d: average recrystallized grain size (μm).

### Claim 5 (depends on 4)

An Mg alloy as set forth in claim 4, characterized by a Y content of more than 0.6 at % and an average recrystallized grain size within the range satisfying the following formula 2:
−0.55c+1.20<log d<1.13c+0.93. formula 2

### Claim 6 (depends on 4, 5)

A Mg alloy as set forth in claim 4 or 5, characterized by an average recrystallized grain size within the range satisfying the following formula 3:
log d>−0.31c+0.92. formula 3

### Claim 7 (depends on 6)

A Mg alloy as set forth in claim 6, characterized by an average recrystallized grain size within the range satisfying the following formula 4: