# US 2010/0163102 A1 · Solar cell and the method of manufacturing thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0163102 A1
- Document ID: US20100163102A1
- Status: Published application
- Kind: A1
- Application number: 12/346,796
- Filed: 2008-12-30
- Published: 2010-07-01
- Earliest claimed: 2008-12-30
- Assignees: Taiwan Textile Research Institute
- Inventors: Wen-Hsien HO; Chi-Sheng Jiang
- Web page: https://patentgrep.com/patent/US20100163102A1

## CPC

- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/34: Sputtering
- H01G 9/2031: {comprising titanium oxide, e.g. TiO2 (H01G9/2036 takes precedence)}
- H01G 9/2059: {comprising an organic dye as the active light absorbing material, e.g. adsorbed on an electrode or dissolved in solution}
- Y02E 10/542: Dye sensitized solar cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solar cell comprises a substrate, a titanium oxide sputtering layer, at least one titanium oxide porous layer, a counter electrode and an electrolyte. The titanium oxide sputtering layer is sputtered on the substrate. The titanium oxide porous layer comprises a stack of titanium dioxide particles on the titanium oxide sputtering layer. The counter electrode is arranged on the titanium oxide porous layer. The electrolyte is filled between the counter electrode and the substrate.

## Claims

### Claim 1

A solar cell, comprising:
a substrate;
a titanium oxide sputtering layer sputtered on the substrate;
at least one titanium oxide porous layer comprising a plurality of titanium dioxide particles stacked on the titanium oxide sputtering layer;
a counter electrode arranged on the titanium oxide porous layer; and
an electrolyte filled between the counter electrode and the substrate.

### Claim 2 (depends on 1)

The solar cell of claim 1, wherein the thickness of the titanium oxide sputtering layer is less than 100 nm.

### Claim 3 (depends on 1)

The solar cell of claim 1, wherein the titanium oxide sputtering layer is made of titanium dioxide.

### Claim 4 (depends on 1)

The solar cell of claim 1, wherein the thickness of the titanium oxide porous layer is less than 20 μm.

### Claim 5 (depends on 1)

The solar cell of claim 1, wherein the crystalline phase of the titanium dioxide particles are rutile or anatase.

### Claim 6 (depends on 1)

The solar cell of claim 1, wherein the specific surface area of the titanium dioxide particles is 2.0-165 cm2/g.

### Claim 7 (depends on 1)

The solar cell of claim 1, further comprising a dye which is dispersed on the surface of the titanium dioxide particles.

### Claim 8 (depends on 7)

The solar cell of claim 7, wherein the dye is N719 (tris(2,2′bipyridyl-4,4′dicarboxylato) ruthenium (II) dichloride).

### Claim 9 (depends on 1)

The solar cell of claim 1, wherein the material of the substrate is indium tin oxide/poly(ethylene naphthalene-2,6-dicarboxylate), transparent conductive oxide or metal.

### Claim 10 (depends on 1)

The solar cell of claim 1, wherein the electrolyte comprises LiI, I2, 4-tert-Butylpyridine and acetonitrile.

### Claim 11 (depends on 1)

The solar cell of claim 1, wherein the material of the counter electrode is Pt, C, conductive polymer or transparent conductive oxide.

### Claim 12

A method of manufacturing a solar cell, comprising:
providing a substrate;
sputtering titanium oxide on the substrate to form a titanium oxide sputtering layer;
coating a titanium oxide particle solution on the titanium oxide sputtering layer;
compressing the titanium oxide particle solution to form a titanium oxide porous layer;
absorbing a dye; and
assemble a counter electrode.

### Claim 13 (depends on 12)

The method of claim 12, wherein the step of sputtering titanium oxide on the substrate is performed at a room temperature by using a titanium oxide target.

### Claim 14 (depends on 12)

The method of claim 12, wherein the step of sputtering is performed at a chamber pressure of 1-7 mTorr.

### Claim 15 (depends on 12)

The method of claim 12, wherein the thickness of the titanium oxide sputtering layer is less than 100 nm.

### Claim 16 (depends on 12)

The method of claim 12, wherein the titanium oxide particle solution is prepared by dissolving a plurality of titanium dioxide particles in an absolute alcohol.

### Claim 17 (depends on 16)

The method of claim 16, wherein the concentration of titanium oxide particle solution is 1%-20%.

### Claim 18 (depends on 16)

The method of claim 16, wherein the specific surface area of the titanium dioxide particles is 2.0-165 cm2/g.

### Claim 19 (depends on 16)

The method of claim 16, wherein the crystalline phase of the titanium dioxide particles are rutile or anatase.

### Claim 20 (depends on 12)

The method of claim 12, wherein at the step of coating a titanium oxide particle solution, the coating height of the titanium oxide particle solution is 10 μm.

### Claim 21 (depends on 12)

The method of claim 12, wherein at the step of compressing the titanium oxide particle solution, the compressing duration is 30-60 seconds.

### Claim 22 (depends on 12)

The method of claim 12, wherein at the step of compressing the titanium oxide particle solution, the compressing force is 50 kg/cm2-150 kg/cm2.

### Claim 23 (depends on 12)

The method of claim 12, further comprising repeating the step of coating a titanium oxide particle solution and the step of compressing the titanium oxide particle solution sequentially before performing the step of absorbing a dye until the titanium oxide porous layer has a thickness less than 20 μm.

### Claim 24 (depends on 12)

The method of claim 12, wherein the material of the substrate is indium tin oxide/poly(ethylene naphthalene-2,6-dicarboxylate), transparent conductive oxide or metal.

### Claim 25 (depends on 12)

The method of claim 12, wherein the material of the counter electrode is Pt, C, conductive polymer or transparent conductive oxide.

### Claim 26 (depends on 12)

The method of claim 12, wherein the dye is N719 (tris(2,2′bipyridyl-4,4′dicarboxylato) ruthenium (II) dichloride).

### Claim 27 (depends on 12)

The method of claim 12, further comprising injecting an electrolyte between the counter electrode and the substrate.

### Claim 28 (depends on 27)

The method of claim 27, wherein the electrolyte comprises LiI, I2, 4-tert-Butylpyridine and acetonitrile.

### Claim 29 (depends on 12)

The method of claim 12, wherein the step of sputtering titanium oxide on the substrate comprises applying a bias of 0-50 V to the substrate.