# US 2010/0149460 A1 · Liquid Crystal Display Device and Method for Manufacturing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0149460 A1
- Document ID: US20100149460A1
- Status: Published application
- Kind: A1
- Application number: 12/704,937
- Filed: 2010-02-12
- Published: 2010-06-17
- Earliest claimed: 2007-12-11
- Assignees: Toppan Printing Co., Ltd.
- Inventors: Sosuke Akao; Hironobu Suda; Yuji Kubo; Godai Fukunaga; Kazuhiro Osato; Yuki Yasu; Takao Taguchi; Masashi Aimatsu
- Web page: https://patentgrep.com/patent/US20100149460A1

## CPC

- G02F 1/13363: Birefringent elements, e.g. for optical compensation
- G02B 5/3016: {involving passive liquid crystal elements (optical properties of liquid crystals G02F1/0063; polarising elements associated with active liquid crystal devices G02F1/133528)}
- C09K 2323/05: Bonding or intermediate layer characterised by chemical composition, e.g. sealant or spacer
- C09K 2323/06: Substrate layer characterised by chemical composition
- G02F 1/133514: {Colour filters}
- G02F 1/133631: {with a spatial distribution of the retardation value}
- G02F 1/133633: {using mesogenic materials}
- G02F 1/133634: {the refractive index Nz perpendicular to the element surface being different from in-plane refractive indices Nx and Ny, e.g. biaxial or with normal optical axis}
- G02F 1/133638: {Waveplates, i.e. plates with a retardation value of lambda/n}
- G02F 2413/01: Number of plates being 1
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A liquid crystal display device may include a first substrate; a second substrate; a first polarizing plate on the first substrate; a second polarizing plate arranged on the second substrate, and so that a direction of an absorption axis of the second polarizing plate being perpendicular to a direction of an absorption axis of the first polarizing plate; a liquid crystal layer arranged between the first substrate and the second substrate; a color filter layer arranged between the liquid crystal layer and the first or the second substrate, the color filter layer having a plurality of pixels of two or more colors. The retardation thin film has in-plane birefringence index satisfying 0.75≦Δn[fr]/λd[fr]≦1.35 for a region corresponding to a reflection part of a pixel and satisfying Δn[t]<1.2×10−3 for a region corresponding to a transmission part of a pixel.

## Claims

### Claim 1

A liquid crystal display device, comprising:
a first substrate;
a second substrate facing the first substrate;
a first polarizing plate arranged on an opposite surface to the second substrate among both sides of the first substrate;
a second polarizing plate arranged on an opposite surface to the first substrate among both sides of the second substrate, and arranged so that a direction of an absorption axis of the second polarizing plate being perpendicular to a direction of an absorption axis of the first polarizing plate;
a liquid crystal layer sandwiched between the first substrate and the second substrate;
a color filter layer arranged between the liquid crystal layer and the first or the second substrate, the color filter layer having a plurality of pixels of two or more colors and each pixel having a reflection part and a transmission part; and
a retardation thin film formed from a liquid crystal fixed layer, and arranged between the first substrate and the second substrate,
wherein, in the retardation thin film, as for at least one layer among the pixels, birefringence indexes are different due to different degree of alignment of the liquid crystal fixed layer for respective regions corresponding to any one or some of respective colors, the transmission part and the reflection part,
wherein the retardation thin film has in-plane birefringence index satisfying 0.75≦Δn[fr]/λd[fr]≦1.35 for a region corresponding to the reflection part of a pixel and satisfying Δn[t]<1.2×10−3 for a region corresponding to the transmission part of a pixel, wherein λd[fr]=(d[f1]×λ[f2])/(d[f2]×λ[f1]), and wherein Δn[t] is an in-plane birefringence in a region corresponding to an image transmission part, and wherein Δn[fr] is a ratio of an in-plane birefringence index in a region corresponding to an image reflection part of a first color to an in-plane birefringence index in a region corresponding to an image reflection part of an arbitrary second color, and wherein d[f1] and d[f2] are thicknesses of retardation layers in regions corresponding to image reflection parts of the first color and the second color, respectively, and wherein λ[f1] and λ[f2] are center wavelengths of colors of image reflection parts of the first color and the second color, respectively.

### Claim 2 (depends on 1)

The liquid crystal display device according to claim 1, wherein a direction of a phase delay axis of the retardation thin film having the in-plane birefringence is substantially identical in the entire retardation thin film.

### Claim 3 (depends on 1)

The liquid crystal display device according to claim 1, wherein the liquid crystal layer sandwiched between the first substrate and the second substrate is aligned substantially vertical to the first and second substrates when a voltage is not applied.

### Claim 4 (depends on 1)

The liquid crystal display according to claim 1, wherein the retardation thin film is formed by any one or both of polymerization and cross-linking of a compound including a thermotropic liquid crystal.

### Claim 5 (depends on 1)

A method for manufacturing the liquid crystal display device according to claim 1, comprising:
(a) forming a thin film in which a liquid crystal compound is aligned in a predetermined direction, by applying a solution including a compound showing a thermotropic liquid crystal property and capable of being any one or both of polymerized and cross-linked by at least light on the first substrate;
(b) exposing the first substrate to light so that exposure amounts are different for regions of the first substrate corresponding to predetermined patterns of respective colors of the color filter layer;
(c) heating the first substrate to a temperature equal to or greater than an isotropic phase transition temperature of the liquid crystal compound;
(d) exposing entirely the first substrate to light while the first substrate is at a temperature that keeps the liquid crystal compound in an isotropic phase; and
(e) making the first substrate face a second substrate in order to arrange the liquid crystal compound between the first and second substrates.

### Claim 6 (depends on 5)

The method for manufacturing the liquid crystal display device according to claim 5,
wherein the thin film formed in process (a) has a film thickness that is uniform over the entire first substrate.

### Claim 7 (depends on 5)

The method for manufacturing the liquid crystal display device according to claim 5,
wherein the compound showing the thermotropic liquid crystal property is capable of being any one or both of polymerized and cross-linked by both light and heat on the first substrate,
and
wherein, instead of process (d), the first substrate is heated to a temperature equal to or greater than the isotropic phase transition temperature of the liquid crystal compound and equal to or greater than a temperature at which the liquid crystal compound becomes any one or both of polymerized and cross-linked.

### Claim 8 (depends on 5)

The method for manufacturing the liquid crystal display device according to claim 5,
wherein, instead of process (d), light irradiation is performed for a portion of the first substrate other than a region of the first substrate where light irradiation of maximum exposure amount is performed during process (b), and the light irradiation is performed while the first substrate is at the temperature that keeps the liquid crystal compound in the isotropic phase.

### Claim 9 (depends on 8)

The method for manufacturing the liquid crystal display device according to claim 8,
wherein the light irradiation while the first substrate is at the temperature that keeps the liquid crystal compound in the isotropic phase, is performed such that a sum total of an exposure amount on the portion of the first substrate in claim 8 and
an exposure amount on the same portion of the first substrate during process (b) is equal to an exposure amount for the region where light irradiation of maximum exposure amount is performed during process (b).

### Claim 10 (depends on 5)

The method for manufacturing the liquid crystal display device according to claim 5,
wherein the color filter layer is formed before process (a).

### Claim 11 (depends on 5)

The method for manufacturing the liquid crystal display device according to claim 5,
wherein the color filter layer is formed after process (d).

### Claim 12 (depends on 5)

The method for manufacturing the liquid crystal display device according to claim 5,
wherein processes (a) through (d) to be performed for the first substrate is performed for the second substrate instead of the first substrate,
and
wherein a TFT layer is formed on the second substrate before the performance of process (a) on the second substrate.