# US 2010/0148396 A1 · Methods of making articles having toughened and untoughened regions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0148396 A1
- Document ID: US20100148396A1
- Status: Published application
- Kind: A1
- Application number: 11/830,874
- Filed: 2007-07-31
- Published: 2010-06-17
- Earliest claimed: 2007-04-17
- Assignees: General Electric Company
- Inventors: Ming Xie; Donald George Lachapelle; Stephen Craig Mitchell
- Web page: https://patentgrep.com/patent/US20100148396A1

## CPC

- B29C 70/887: {locally reinforced, e.g. by fillers (filler concentrated near the surface B29C70/64)}
- B29B 11/16: comprising fillers or reinforcement {(non-woven fabrics per se D04H1/00, D04H3/00)}
- B29C 70/025: {with particular filler}
- B29K 2995/0089: Impact strength or toughness
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Methods of making an article having at least one toughened region and at least one untoughened region involving providing a material, applying a toughening agent to a portion of the material, shaping the material to produce a preform, applying an untoughened resin to the preform, and curing the preform having the applied untoughened resin to produce the at least one toughened region and the at least one untoughened region wherein the toughened region comprises a toughened resin having a fracture toughness of at least about 1.0 MPa-m1/2.

## Claims

### Claim 1

A method of making an article having at least one toughened region and at least one untoughened region comprising:
providing a material;
applying a toughening agent to a portion of the material;
shaping the material to produce a preform;
applying an untoughened resin to the preform; and
curing the preform having the applied untoughened resin to produce the at least one toughened region and the at least one untoughened region wherein the toughened region comprises a toughened resin having a fracture toughness of at least about 1.0 MPa-m1/2.

### Claim 2 (depends on 1)

The method of claim 1 wherein the toughening agent is selected from the group consisting of polymers, nano fibers, nano particles, and combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1 wherein the material is selected from the group consisting of carbon fiber, glass fiber, ceramic fiber, graphite fiber, aramid fiber, and combinations thereof.

### Claim 4 (depends on 1)

The method of claim 1 wherein the untoughened resin is a resin selected from the group consisting of vinyl ester resins, polyester resins, acrylic resins, epoxy resins, polyurethane resins, bismaelimide resins, polyimide resins, and combinations thereof.

### Claim 5 (depends on 1)

The method of claim 1 wherein applying the toughening agent comprises joining the toughening agent to the material such that when the untoughened resin is applied the toughened resin is produced in the portion of the material comprising the toughening agent.

### Claim 6 (depends on 1)

The method of claim 1 wherein applying the toughening agent comprises combining the toughening agent with the untoughened resin to produce a toughened resin and applying the toughened resin to the portion of the material.

### Claim 7 (depends on 1)

The method of claim 1 wherein the article is a turbine engine component selected from the group consisting of fan casings and airfoils.

### Claim 8 (depends on 1)

The method of claim 1 further comprising a transition region between each toughened region and untoughened region.

### Claim 9 (depends on 1)

The method of claim 1 wherein the toughened region corresponds to the portion of the material comprising the toughening agent.

### Claim 10 (depends on 1)

The method of claim 1 further comprising coupling at least one toughened flange to the at least one toughened region wherein the toughened flange is selected from the group consisting of mounting flanges, attachment end flanges, and combinations thereof.

### Claim 11 (depends on 1)

The method of claim 1 wherein applying the toughening agent comprises spraying the toughening agent on the material such that when the untoughened resin is applied the toughened resin is produced in the portion of the material comprising the toughening agent.

### Claim 12 (depends on 1)

The method of claim 1 wherein the untoughened region of the article comprises an impact zone.

### Claim 13 (depends on 6)

The method of claim 6 wherein the toughened resin comprises from about 5% to about 20% by weight of the toughening agent.

### Claim 14

A method of making an article having at least one toughened region and at least one untoughened region comprising:
providing a material;
applying a toughening agent to a portion of the material;
shaping the material to produce a preform;
applying an untoughened resin to the preform; and
curing the preform having the applied untoughened resin to produce the at least one toughened region and the at least one untoughened region
wherein the toughened region corresponds to the portion of the material comprising the toughening agent, the composite material comprises a transition region between each toughened region and untoughened region, and the toughened region comprises a toughened resin having a fracture toughness of at least about 1.0 MPa-m1/2.

### Claim 15 (depends on 14)

The method of claim 14 wherein the toughening agent is selected from the group consisting of polymers, nano fibers, nano particles, and combinations thereof.

### Claim 16 (depends on 14)

The method of claim 14 wherein each transition region is positioned in an orientation selected from the group consisting of planar, normal to the plane, and combinations thereof.

### Claim 17 (depends on 14)

The method of claim 14 wherein the material is selected from the group consisting of carbon fiber, glass fiber, ceramic fiber, graphite fiber, aramid fiber, and combinations thereof.

### Claim 18 (depends on 14)

The method of claim 14 wherein applying the toughening agent to a portion of the material and shaping the material occur concurrently.

### Claim 19 (depends on 14)

The method of claim 14 further comprising coupling at least one toughened flange to the at least one toughened region wherein the toughened flange is selected from the group consisting of mounting flanges, attachment end flanges, and combinations thereof.

### Claim 20

A method of making a fan casing having at least one toughened region and at least one untoughened region comprising:
providing a material;
applying a toughening agent to a portion of the material;
shaping the material to produce a fan casing preform;
applying an untoughened resin to the fan casing preform; and
curing the fan casing preform having the applied untoughened resin to produce the at least one toughened region and the at least one untoughened region
wherein the toughened region corresponds to the portion of the material comprising the toughening agent and wherein the toughened region comprises a toughened resin having a fracture toughness of at least about 1.0 MPa-m1/2.