# US 2010/0144119 A1 · Method of producing bonded wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0144119 A1
- Document ID: US20100144119A1
- Status: Published application
- Kind: A1
- Application number: 12/631,478
- Filed: 2009-12-04
- Published: 2010-06-10
- Earliest claimed: 2008-12-08
- Assignees: Sumco Corporation
- Inventors: Tatsumi Kusaba; Akihiko Endo
- Web page: https://patentgrep.com/patent/US20100144119A1

## CPC

- H10P 90/1922: {using silicon etch back techniques, e.g. BESOI or ELTRAN}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In the production of a bonded wafer, a wafer for active layer after a heat treatment for bonding reinforcement followed by bonding is thinned to a given thickness by a surface polishing or an etching and then a wafer for support layer is subjected to both a minor-surface beveling and a terrace processing simultaneously.

## Claims

### Claim 1

A method of producing a bonded wafer, which comprises bonding a wafer for active layer to a wafer for support layer, conducting a heat treatment for bonding reinforcement and then thinning the wafer for active layer, wherein the wafer for active layer after the heat treatment for bonding reinforcement is thinned to a thickness of 1 to 20 μm by a surface polishing or an etching and then the wafer for support layer is subjected to both a minor-surface beveling and a terrace processing simultaneously.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a wafer not subjected to a mirror-surface beveling is used as at least a wafer for active layer in the wafer for active layer and the wafer for support layer.