# US 2010/0144096 A1 · Method of manufacturing semiconductor device in which bottom surface and side surface of semiconductor substrate are covered with resin protective film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0144096 A1
- Document ID: US20100144096A1
- Status: Published application
- Kind: A1
- Application number: 12/632,033
- Filed: 2009-12-07
- Published: 2010-06-10
- Earliest claimed: 2008-12-09
- Assignees: Casio Computer Co., Ltd.; Epas
- Inventors: Taisuke Koroku; Osamu Okada; Osamu Kuwabara; Junji Shiota; Nobumitsu Fujii
- Web page: https://patentgrep.com/patent/US20100144096A1

## CPC

- H10W 74/014: {using batch processing}
- H10W 74/121: {by multiple encapsulations, e.g. by a thin protective coating and a thick encapsulation}
- H10W 74/129: {forming a chip-scale package [CSP]}
- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- H10W 70/60: Insulating or insulated package substrates; Interposers; Redistribution layers (leadframes H10W70/40)
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/90: Bond pads, in general
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

First, a trench is formed in parts of a semiconductor wafer, a sealing film and other elements corresponding to a dicing street and both sides thereof. In this state, the semiconductor wafer is separated into silicon substrates by the formation of the trench. Then, a resin protective film is formed on the bottom surface of each silicon substrate including the inner part of the trench. In this case, the semiconductor wafer is separated into the silicon substrates. However, a support plate is affixed to the upper surfaces of the columnar electrode and the sealing film via an adhesive layer. Therefore, when the resin protective film is formed, it is possible to prevent the entire workpiece including the separated silicon substrates from being easily warped.

## Claims

### Claim 1

A semiconductor device manufacturing method comprising:
preparing an assembly having an insulating film formed on one surface of a semiconductor wafer where an integrated circuit is formed, an electrode connection pad portion formed on the insulating film in such a manner as to be connected to the integrated circuit, an external connection bump electrode formed on the electrode connection pad portion, and a sealing film formed around the external connection bump electrode;
affixing a support plate to the external connection bump electrode and the sealing film;
forming a trench reaching an intermediate position of the thickness of the sealing film on the bottom side of the semiconductor wafer in parts corresponding to a dicing street and both sides thereof;
forming a resin protective film on the bottom surface of the semiconductor wafer including the inner part of the trench;
peeling off the support plate; and
cutting the sealing film and the resin protective film in a width smaller than the width of the trench.

### Claim 2 (depends on 1)

The semiconductor device manufacturing method according to claim 1, wherein affixing the support plate includes affixing the support plate to the external connection bump electrode and the sealing film via a cohesive layer, and detaching the support plate includes detaching the cohesive layer.

### Claim 3 (depends on 2)

The semiconductor device manufacturing method according to claim 2, wherein the cohesive layer consists of a double-sided adhesive tape wherein an ultraviolet-curable cohesive agent is provided on a surface of a base material film where the external connection bump electrode and the sealing film are affixed and wherein an ultraviolet-sensitive gas-generating cohesive agent is provided on the other surface of the base material film.

### Claim 4 (depends on 3)

The semiconductor device manufacturing method according to claim 3, wherein the support plate is made of glass.

### Claim 5 (depends on 4)

The semiconductor device manufacturing method according to claim 4, wherein detaching the support plate and the cohesive layer includes radiating ultraviolet rays from the side of the support plate.

### Claim 6 (depends on 5)

The semiconductor device manufacturing method according to claim 5, wherein detaching the support plate and the cohesive layer includes detaching the cohesive layer after detaching the support plate.

### Claim 7 (depends on 6)

The semiconductor device manufacturing method according to claim 6, wherein forming the resin protective film on the bottom surface of the semiconductor wafer includes curing the resin protective film at 120 to 180° C.

### Claim 8 (depends on 2)

The semiconductor device manufacturing method according to claim 2, wherein the bottom side of the semiconductor wafer is ground to reduce the thickness of the semiconductor wafer after or before the support plate is affixed.

### Claim 9 (depends on 2)

The semiconductor device manufacturing method according to claim 2, further comprising grinding the upper side of the resin protective film to reduce the thickness of the resin protective film and planarize the upper surface of the resin protective film, after the resin protective film is formed.

### Claim 10 (depends on 2)

The semiconductor device manufacturing method according to claim 2, wherein the external connection bump electrode is a columnar electrode formed on the electrode connection pad portion.

### Claim 11 (depends on 2)