# US 2010/0143849 A1 · Semiconductor device manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0143849 A1
- Document ID: US20100143849A1
- Status: Published application
- Kind: A1
- Application number: 12/631,463
- Filed: 2009-12-04
- Published: 2010-06-10
- Earliest claimed: 2008-12-05
- Inventors: Tatsuhiko Ema; Yuriko Seino; Shinichi Ito; Hirokazu Kato
- Web page: https://patentgrep.com/patent/US20100143849A1

## CPC

- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A semiconductor device manufacturing method includes: forming a foundation film on a semiconductor wafer; after forming the foundation film, forming a reaction layer of the semiconductor wafer and the foundation film therebetween; removing the foundation film and leaving the reaction layer on the semiconductor wafer; forming a resist film on the reaction layer; patterning the resist film; and using the patterned resist film as a mask to perform processing on the semiconductor wafer.

## Claims

### Claim 1

A semiconductor device manufacturing method comprising:
forming a foundation film on a semiconductor wafer;
forming a reaction layer of the semiconductor wafer and the foundation film between the semiconductor wafer and the foundation film after forming the foundation film;
removing the foundation film and leaving the reaction layer on the semiconductor wafer;
forming a resist film on the reaction layer;
patterning the resist film; and
using the patterned resist film as a mask to perform processing on the semiconductor wafer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the foundation film is soluble in a developer used in patterning the resist film.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the foundation film has anti-reflection capability for exposure light used in patterning the resist film.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the foundation film is supplied onto the semiconductor wafer in a liquid state, and then subjected to baking treatment.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the baking treatment allows the semiconductor wafer to interact with the foundation film to form the reaction layer.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the foundation film is removed by wet processing.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the reaction layer is insoluble in a processing liquid used in the wet processing.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the reaction layer is an organic layer containing carbon.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the reaction layer has anti-reflection capability for exposure light used in patterning the resist film.

### Claim 10 (depends on 1)

The method according to claim 1, wherein after the foundation film is removed, the reaction layer remains on the entire surface of the semiconductor wafer.

### Claim 11 (depends on 1)

The method according to claim 1, wherein
the patterning the resist film includes performing selective exposure on the resist film and, after the exposure, developing the resist film using a developer, and
the resist film includes an acid-generating agent which generates acid by the exposure, and a portion of the resist film where the acid is generated upon the exposure becomes soluble in the developer and is removed.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising:
forming an anti-reflection coating on the resist film after the forming the resist film,
exposure and development being performed on the resist film to pattern the resist film with the anti-reflection coating formed.

### Claim 13 (depends on 1)

The method according to claim 1, wherein a surface of the semiconductor wafer is a silicon oxide film.

### Claim 14

A semiconductor device manufacturing method comprising:
forming a foundation film on a semiconductor wafer;
removing the foundation film while leaving a portion of the foundation film as an adhesive layer on the semiconductor wafer;
forming a resist film on the adhesive layer;
patterning the resist film; and
using the patterned resist film as a mask to perform processing on the semiconductor wafer.

### Claim 15 (depends on 14)

The method according to claim 14, wherein
the patterning the resist film includes bringing a template having a feature pattern into contact with the resist film, curing the resist film, and separating the template from the resist film.

### Claim 16 (depends on 14)

The method according to claim 14, further comprising:
performing exposure on the entire surface of the foundation film after the forming the foundation film.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the foundation film is removed by developing treatment using a developer after the exposure.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the adhesive layer is insoluble in the developer.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the adhesive layer has a lower etching rate in the developer than the foundation film.

### Claim 20 (depends on 14)

The method according to claim 14, wherein the adhesive layer is formed at an interface between the foundation film and the semiconductor wafer by reaction therebetween.