# US 2010/0143825 A1 · Metallic separator for fuel cell and method of fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0143825 A1
- Document ID: US20100143825A1
- Status: Published application
- Kind: A1
- Application number: 11/996,691
- Filed: 2006-12-07
- Published: 2010-06-10
- Earliest claimed: 2006-09-28
- Assignees: Seoul National University Industry Foundation
- Inventors: Dae Geun Nam; Hu Chul Lee
- Web page: https://patentgrep.com/patent/US20100143825A1

## CPC

- H01M 8/0204: Non-porous and characterised by the material
- H01M 8/0208: Alloys
- H01M 8/021: Alloys based on iron
- H01M 8/0228: in the form of layered or coated products
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are a metallic separator for fuel cell in which a Cr2N layer is formed on the surface of base metals, and a method of fabricating the metallic separator for fuel cell. The method comprises: plating chromium layer on the surface of the base metal; and forming a Cr2N layer by nitriding the chromium-plated layer in properly selected nitriding conditions. Only the Cr2N layer, which has lower electrical resistivity than CrN, is selectively fabricated on the surface of the base metal. The interfacial contact resistance of the separator is reduced and the efficiency of the fuel cell can be improved. In addition, since a low-priced general metals or alloys such as stainless steels, carbon steels, alloy steels or even nonferrous alloys can be used as the base metal, the cost of the fabrication of metallic separator can be significantly reduced. The thickness of the separator can be made as small as to 0.2 mm, the weight and total thickness of a fuel cell stack can be significantly reduced.

## Claims

### Claim 1

A metallic separator for fuel cell wherein a Cr2N nitride layer is formed on the surface of a base metal.

### Claim 2 (depends on 1)

The metallic separator of claim 1, wherein the base metal is selected from the group consisting of stainless steels, carbon steels, chromium alloy steels, and nonferrous alloys.

### Claim 3

A metallic separator for fuel cell,
wherein the metallic separator is made by the method comprising the steps of:
forming nickel strike layer between a base metal and a Cr plated layer; and
nitriding the Cr plated layer to form a Cr2N nitride layer.

### Claim 4

A method of fabricating a metallic separator for fuel cell in which a Cr2N nitride layer is formed on the surface of a base metal, comprising:
plating chromium on the surface of the base metal to form a chromium-plated layer; and
forming Cr2 N layer by nitriding the chromium-plated layer.

### Claim 5 (depends on 4)

The method of claim 4, further comprising nickel striking before the step of plating of chromium on the surface of the base metal, wherein the base metal has a passive oxide film on it.

### Claim 6 (depends on 4, 5)

The method of claim 4 or 5, wherein the partial pressure of nitrogen is set to 0.001-5 atm during the nitriding treatment.

### Claim 7 (depends on 4, 5)

The method of claim 4 or 5, wherein the partial pressure of the mixed gas of nitrogen and hydrogen is set to 0.001-5 atm during the nitriding treatment.

### Claim 8 (depends on 4, 5)

The method of claim 4 or 5, further comprising cooling of the metallic separator wherein the cooling takes less than 2 hours from nitridization temperature to room temperature so that CrN nitride is not generated during the cooling step after nitridization.

### Claim 9 (depends on 4, 5)