# US 2010/0143219 A1 · Process for the production of nano lead oxides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0143219 A1
- Document ID: US20100143219A1
- Status: Published application
- Kind: A1
- Application number: 12/448,713
- Filed: 2008-01-03
- Published: 2010-06-10
- Earliest claimed: 2007-01-05
- Assignees: Tai-Kwong-Yokohama Battery Industried Sdn Bhd
- Inventors: Siew Hon Chow
- Web page: https://patentgrep.com/patent/US20100143219A1

## CPC

- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- H01M 10/06: Lead-acid accumulators (semi-lead accumulators H01M10/20)
- Y02E 60/10: Energy storage using batteries
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Provided is a process for producing fine particles of pure lead oxide from a waste lead oxide paste obtained from exhausted lead-acid batteries. The lead oxide particles so produced are substantially spherical and have a weight average particle size from about 13 nm to about 100 nm, which, are of nano-particle dimensions. The process according to the present invention is capable to produce pure lead oxide of PbO2 and lead oxide of Pb3O4 or commonly known as red lead.

## Claims

### Claim 1

A process for producing fine particles of pure lead oxide from a waste lead oxide paste obtained from exhausted lead-acid batteries characterizes in that said lead oxide particles are substantially spherical and have a weight average particle size from about 13 nm to about 100 nm.

### Claim 2 (depends on 1)

A process for producing fine particles of pure lead oxide as defined in claim 1 characterizes in that at least 80 weight percent of said particles are not larger than twice said average particle size.

### Claim 3 (depends on 1)

A process for producing fine particles of pure lead oxide as defined in claim 1 characterizes in that said lead oxide is PbO2.

### Claim 4 (depends on 1)

A process for producing fine particles of pure lead oxide as denied in claim 1 characterizes in that said lead Oxide is Pb3O4.

### Claim 5

A process for producing fine particles of pure lead oxide from waste lead oxide paste as starting material characterizes by the following steps;
reacting said starting material with a sodium-based solution to convert the lead compounds therein to insoluble lead carbonate;
dissolving said insoluble lead carbonate by reacting with an acid-based solution to form lead-based solution;
recovering lead oxide powder from said lead-based solution by process of crystallization;
reacting said lead oxide powder with chlorine and rinsing the resultant lead bearing compound with water; and
heating said resultant lead bearing powder to form nano lead oxide particles

### Claim 6 (depends on 5)

A process for producing fine particles of pure lead oxide as defined by claim 5 characterizes in that said sodium-based solution is sodium hydroxide NaOH.

### Claim 7 (depends on 5)

A process for producing fine particles of pure lead oxide as defined by claim 5 characterizes in that said acid-based solution is acetic acid.

### Claim 8 (depends on 5)

A process for producing fine particles of pure lead oxide as defined by claim 5 characterizes in that the heating of said lead bearing compound is conducted under temperature of not more than 150 degree C. for about 10 to 15 hours to produce nano particles of PbO2.

### Claim 9 (depends on 5)

A process for producing fine particles of pure lead oxide as defined by claim 5 characterizes in that the heating of said lead bearing compound is conducted under temperature range of 420 to 520 degree C. for about 14 to 18 hours to produce nano particles of Pb3O4.