# US 2010/0143177 A1 · Method for forming high strength aluminum alloys containing L12 intermetallic dispersoids

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0143177 A1
- Document ID: US20100143177A1
- Status: Published application
- Kind: A1
- Application number: 12/316,046
- Filed: 2008-12-09
- Published: 2010-06-10
- Earliest claimed: 2008-12-09
- Assignees: United Technologies Corporation
- Inventors: Awadh B. Pandey
- Web page: https://patentgrep.com/patent/US20100143177A1

## CPC

- C22C 1/0416: {Aluminium-based alloys}
- C22C 1/047: comprising intermetallic compounds {(C22C1/0441 takes precedence)}
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A method and apparatus produces high strength aluminum alloys from a powder containing L12 intermetallic dispersoids. The powder is degassed, sealed under vacuum in a container, heated, consolidated by vacuum hot pressing, and extruded.

## Claims

### Claim 1

A method for producing a high strength aluminum alloy billet containing L12 dispersoids, comprising the steps of:
placing a quantity of an aluminum alloy powder containing an L12 dispersoid therein having a mesh size of less than 450 mesh in a container;
vacuum degassing the powder at a temperature of about 300° F. (149° C.) to about 900° F. (482° C.) for about 0.5 hours to about 8 days;
sealing the degassed powder in the container under vacuum;
heating the sealed container at about 300° F. (149° C.) to about 900° F. (482° C.) for about 15 minutes to eight hours;
vacuum hot pressing the heated container to form a billet; and
removing the container from the formed billet.

### Claim 2 (depends on 1)

The method of claim 1, wherein the container is aluminum having a configuration with a central axis, and vacuum hot pressing is done along the axis while restraining radial movement of the container.

### Claim 3 (depends on 1)

The method of claim 1, wherein the vacuum hot pressing includes blind die compaction for about 1 minute to about 8 hours at a temperature of 300° F. (149° C.) to about 900° F. (482° C.) under uni-axial pressure of about 5 ksi to about 100 ksi.

### Claim 4 (depends on 1)

The method of claim 1, wherein the vacuum hot pressing produces a billet of the aluminum alloy powder having a density of about 100 percent.

### Claim 5 (depends on 1)

The method of claim 1, wherein the degassing includes rotating the aluminum alloy powder to heat and expose all the powder to vacuum.

### Claim 6 (depends on 1)

The method of claim 1, wherein the thus formed billet is extruded at a load of about 100 tons to about 10,000 tons.

### Claim 7 (depends on 6)

The method of claim 6, wherein the extrusion temperature is about 300° F. (149° C.) to about 900° F. (482° C.), the billet soak time is about 15 minutes to about 8 hours at a rate of about 0.2 inch per minute to about 20 inches per minute and an extrusion ratio of about 2:1 to about 500:1.

### Claim 8 (depends on 1)

The method of claim 1, wherein the L12 dispersoids comprise Al3X dispersoids wherein X is at least one first element selected from the group comprising:
about 0.1 to about 4.0 weight percent scandium, about 0.1 to about 20.0 weight percent erbium, about 0.1 to about 15.0 weight percent thulium, about 0.1 to about 25.0 weight percent ytterbium, and about 0.1 to about 25.0 weight percent lutetium;
at least one second element selected from the group comprising about 0.1 to about 20.0 weight percent gadolinium, about 0.1 to about 20.0 weight percent yttrium, about 0.05 to about 4.0 weight percent zirconium, about 0.05 to about 10.0 weight percent titanium, about 0.05 to about 10.0 weight percent hafnium, and about 0.05 to about 5.0 weight percent niobium; and
the balance substantially aluminum.

### Claim 9 (depends on 8)

The method of claim 8, wherein the aluminum alloy powder contains at least one third element selected from the group consisting of silicon, magnesium, lithium, copper, zinc, and nickel.

### Claim 10 (depends on 9)

The method of claim 9, wherein the third element comprises at least one of about 4 to about 25 weight percent silicon, about 1 to about 8 weight percent magnesium, about 0.5 to about 3 weight percent lithium, about 0.2 to about 6 weight percent copper, about 3 to about 12 weight percent zinc, about 1 to about 12 weight percent nickel.

### Claim 11 (depends on 8)

The method of claim 8, wherein the L12 dispersoids comprise Al3X dispersoids wherein X is at least one first element selected from the group comprising:
about 0.1 to about 0.5 weight percent scandium, about 0.1 to about 6.0 weight percent erbium, about 0.1 to about 10.0 weight percent thulium, about 0.1 to about 15.0 weight percent ytterbium, and about 0.1 to about 12.0 weight percent lutetium;
at least one second element selected from the group comprising about 0.1 to about 4.0 weight percent gadolinium, about 0.1 to about 4.0 weight percent yttrium, about 0.05 to about 1.0 weight percent zirconium, about 0.05 to about 2.0 weight percent titanium, about 0.05 to about 2.0 weight percent hafnium, and about 0.05 to about 1.0 weight percent niobium; and
the balance substantially aluminum.

### Claim 12

Apparatus for producing a high strength aluminum alloy billet containing L12 dispersoids, comprising:
a container for holding a quantity of an aluminum alloy powder containing an L12 dispersoid therein having a mesh size of less than 450 mesh;
a vacuum and heat source for degassing the powder at a temperature of about 300° F. (149° C.) to about 900° F. (482° C.) for about 0.5 hours to about 8 days;
sealing means for sealing the degassed powder in the container under vacuum;
a heater for heating the sealed container at about 300° F. (149° C.) to about 900° F. (482° C.) for about 15 minutes to eight hours;
a vacuum hot press for forming the heated container into a billet; and
means for removing the container from the thus formed billet.

### Claim 13 (depends on 12)

The apparatus of claim 12, wherein the container is aluminum having a central axis, and vacuum hot pressing is done along the axis while restraining transverse movement of the container.

### Claim 14 (depends on 12)

The apparatus of claim 12, wherein the vacuum hot pressing includes blind die compaction for about 1 minute to about 8 hours at a temperature of 300° F. (149° C.) to about 900° F. (482° C.) under uni-axial pressure of about 5 ksi to about 100 ksi.

### Claim 15 (depends on 12)

The apparatus of claim 12, wherein the vacuum hot pressing produces a billet of the aluminum alloy powder having a density of about 100 percent.

### Claim 16 (depends on 12)

The apparatus of claim 12, wherein the degassing includes rotating the aluminum alloy powder to heat and exposing to vacuum all the powder.

### Claim 17 (depends on 12)

The apparatus of claim 12, wherein the formed billet is extruded at a load of about 100 tons to about 10,000 tons.

### Claim 18 (depends on 17)

The apparatus of claim 17, wherein the extrusion temperature is about 300° F. (149° C.) to about 900° F. (482° C.), the billet soak time is about 15 minutes to about 8 hours at a rate of about 0.2 inch per minute to about 20 inches per minute, and an extrusion ratio of about 2:1 to about 500:1.

### Claim 19 (depends on 12)

The apparatus of claim 12, wherein the L12 dispersoids comprise Al3X dispersoids wherein X is at least one first element selected from the group comprising:
about 0.1 to about 4.0 weight percent scandium, about 0.1 to about 20.0 weight percent erbium, about 0.1 to about 15.0 weight percent thulium, about 0.1 to about 25.0 weight percent ytterbium, and about 0.1 to about 25.0 weight percent lutetium;
at least one second element selected from the group comprising about 0.1 to about 20.0 weight percent gadolinium, about 0.1 to about 20.0 weight percent yttrium, about 0.05 to about 4.0 weight percent zirconium, about 0.05 to about 10.0 weight percent titanium, about 0.05 to about 10.0 weight percent hafnium, and about 0.05 to about 5.0 weight percent niobium; and
the balance substantially aluminum.

### Claim 20 (depends on 19)

The apparatus of claim 19, wherein the aluminum alloy powder contains at least one third element selected from the group consisting of silicon, magnesium, lithium, copper, zinc, and nickel.

### Claim 21 (depends on 20)

The apparatus of claim 20, wherein the third element comprises at least one of about 4 to about 25 weight percent silicon, about 1 to about 8 weight percent magnesium, about 0.5 to about 3 weight percent lithium, about 0.2 to about 6 weight percent copper, about 3 to about 12 weight percent zinc, about 1 to about 12 weight percent nickel.

### Claim 22 (depends on 19)

The apparatus of claim 19, wherein the L12 dispersoids comprise Al3X dispersoids wherein X is at least one first element selected from the group comprising:
about 0.1 to about 0.5 weight percent scandium, about 0.1 to about 6.0 weight percent erbium, about 0.1 to about 10.0 weight percent thulium, about 0.1 to about 15.0 weight percent ytterbium, and about 0.1 to about 12.0 weight percent lutetium;
at least one second element selected from the group comprising about 0.1 to about 4.0 weight percent gadolinium, about 0.1 to about 4.0 weight percent yttrium, about 0.05 to about 1.0 weight percent zirconium, about 0.05 to about 2.0 weight percent titanium, about 0.05 to about 2.0 weight percent hafnium, and about 0.05 to about 1.0 weight percent niobium; and
the balance substantially aluminum.