# US 2010/0139823 A1 · Pyrophoric metal-carbon foam composites and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0139823 A1
- Document ID: US20100139823A1
- Status: Published application
- Kind: A1
- Application number: 12/329,437
- Filed: 2008-12-05
- Published: 2010-06-10
- Earliest claimed: 2008-12-05
- Assignees: Lawrence Livermore National Security, LLC
- Inventors: Alexander E. Gash; Joe H. Satcher, JR.; Randall L. Simpson; Theodore F. Baumann; Marcus A. Worsley
- Web page: https://patentgrep.com/patent/US20100139823A1

## CPC

- C06C 15/00: Pyrophoric compositions; Flints (chemical lighters C06C9/00)
- C06B 45/00: Compositions or products which are defined by structure or arrangement of component of product (explosive charges of particular form or shape F42B1/00, F42B3/00)
- C06C: DETONATING OR PRIMING DEVICES; FUSES (ammunition fuzes F42C); CHEMICAL LIGHTERS; PYROPHORIC COMPOSITIONS
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})

## Abstract

A method for creating a pyrophoric material according to one embodiment includes thermally activating a carbon foam for creating micropores therein; contacting the activated carbon foam with a liquid solution comprising a metal salt for depositing metal ions in the carbon foam; and reducing the metal ions in the foam to metal particles. A pyrophoric material in yet another embodiment includes a pyrophoric metal-carbon foam composite comprising a carbon foam having micropores and mesopores and a surface area of greater than or equal to about 2000 m2/g, and metal particles in the pores of the carbon foam. Additional methods and materials are also disclosed.

## Claims

### Claim 1

A method for creating a pyrophoric material, comprising:
thermally activating a carbon foam for creating micropores therein;
contacting the activated carbon foam with a liquid solution comprising a metal salt for depositing metal ions in the carbon foam; and
reducing the metal ions in the foam to metal particles.

### Claim 2 (depends on 1)

A method as recited in claim 1, further comprising forming the carbon foam using a sol-gel chemistry process.

### Claim 3 (depends on 2)

A method as recited in claim 2, wherein the sol-gel chemistry includes an acid-catalyzed polymerization of precursors.

### Claim 4 (depends on 2)

A method as recited in claim 2, further comprising drying a gel formed using the sol-gel chemistry process, wherein the gel is dried under ambient conditions.

### Claim 5 (depends on 2)

A method as recited in claim 2, further comprising pyrolyzing a gel formed using the sol-gel chemistry process for producing the carbon foam, the carbon foam being primarily macroporous.

### Claim 6 (depends on 1)

A method as recited in claim 1, wherein the activating is performed by contacting the carbon foam with a heated gas.

### Claim 7 (depends on 6)

A method as recited in claim 6, wherein the heated gas is selected from a group consisting of carbon dioxide and steam.

### Claim 8 (depends on 1)

A method as recited in claim 1, wherein an internal surface area of the foam after the activating and before the contacting is greater than about 2000 m2/gram.

### Claim 9 (depends on 1)

A method as recited in claim 1, further comprising drying the activated carbon foam after the contacting and before the reducing.

### Claim 10 (depends on 1)

A method as recited in claim 1, wherein the reducing includes contacting the metal ions with a gaseous reductant.

### Claim 11 (depends on 1)

A method as recited in claim 1, further comprising storing the carbon foam with metal particles therein in an inert atmosphere.

### Claim 12

A method for creating a pyrophoric material, comprising:
forming a carbonaceous gel using a sol-gel chemistry process;
pyrolyzing the gel for producing a primarily macroporous carbon foam;
thermally activating the carbon foam for creating micropores therein;
contacting the activated carbon foam with a liquid solution comprising a metal salt for depositing metal ions in the carbon foam; and
reducing the metal ions in the foam to metal particles.

### Claim 13 (depends on 12)

A method as recited in claim 12, wherein the sol-gel chemistry process includes an acid-catalyzed polymerization of precursors.

### Claim 14 (depends on 12)

A method as recited in claim 12, wherein the activating is performed by contacting the carbon foam with a heated gas.

### Claim 15 (depends on 14)

A method as recited in claim 14, wherein the heated gas is selected from a group consisting of carbon dioxide and steam.

### Claim 16 (depends on 12)

A method as recited in claim 12, wherein an internal surface area of the foam after the activating and before the contacting is greater than about 2000 m2/gram.

### Claim 17 (depends on 12)

A method as recited in claim 12; wherein the reducing includes contacting the metal ions with a gaseous reductant.

### Claim 18 (depends on 12)

A method as recited in claim 12, further comprising storing the carbon foam with metal particles therein in an inert atmosphere.

### Claim 19

A method for creating a pyrophoric material, comprising:
contacting a carbon foam with a solution comprising a metal alkoxide or a solution comprising a metal salt and a proton scavenger, for forming an interpenetrating network of metal oxide gel in the carbon foam;
drying the gel; and
pyrolyzing for reducing the metal oxide network to a native metal thereof.

### Claim 20 (depends on 19)

A method as recited in claim 19, further comprising forming the carbon foam using a sol-gel chemistry process.

### Claim 21 (depends on 20)

A method as recited in claim 20, wherein the sol-gel chemistry includes an acid-catalyzed polymerization of precursors.

### Claim 22 (depends on 20)

A method as recited in claim 20, further comprising pyrolyzing a gel formed using the sol-gel chemistry process for producing the carbon foam.

### Claim 23 (depends on 19)

A method as recited in claim 19, wherein drying the gel includes supercritical extraction.

### Claim 24 (depends on 19)

A method as recited in claim 19, further comprising storing the carbon foam in an inert atmosphere after the pyrolyzing.

### Claim 25

A method for creating a pyrophoric material, comprising:
contacting a carbon foam with a solution comprising a metal alkoxide or a solution comprising a metal salt and a proton scavenger for forming an interpenetrating network of metal oxide gel in the carbon foam, the metal oxide comprising at least one of titanium and iron;
drying the gel using supercritical extraction; and
pyrolyzing for reducing the metal oxide network to a native metal thereof.

### Claim 26

A pyrophoric material, comprising:
a pyrophoric metal-carbon foam composite comprising a carbon foam having micropores and mesopores and a surface area of greater than or equal to about 2000 m2/g, and metal particles in the pores of the carbon foam.

### Claim 27 (depends on 26)

A material as recited in claim 26, wherein the carbon foam is a pyrollized aerogel or xerogel.

### Claim 28 (depends on 26)

A material as recited in claim 26, wherein the carbon foam has micropores characteristic of thermal activation thereof.

### Claim 29 (depends on 26)

A material as recited in claim 26, wherein the metal is selected from a group consisting of iron, platinum, titanium, nickel, tin, and zirconium.