# US 2010/0139815 A1 · Conversion Process for heat treatable L12 aluminum aloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0139815 A1
- Document ID: US20100139815A1
- Status: Published application
- Kind: A1
- Application number: 12/316,020
- Filed: 2008-12-09
- Published: 2010-06-10
- Earliest claimed: 2008-12-09
- Assignees: United Technologies Corporation
- Inventors: Awadh B. Pandey
- Web page: https://patentgrep.com/patent/US20100139815A1

## CPC

- C22C 21/00: Alloys based on aluminium
- C22C 1/0416: {Aluminium-based alloys}
- C22C 1/1094: {comprising an after-treatment}
- C22C 21/02: with silicon as the next major constituent
- C22C 21/06: with magnesium as the next major constituent
- C22C 21/10: with zinc as the next major constituent
- C22C 21/12: with copper as the next major constituent
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/043: of alloys with silicon as the next major constituent
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F 1/053: of alloys with zinc as the next major constituent
- C22F 1/057: of alloys with copper as the next major constituent
- B22F 2998/10: Processes characterised by the sequence of their steps
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A method for producing high strength aluminum alloy containing L12 intermetallic dispersoids by using gas atomization to produce powder that is then consolidated into L12 aluminum alloy billets or by casting the alloy into molds to produce L12 aluminum alloy billets or by casting the alloy into directly useable parts.

## Claims

### Claim 1

A method for forming a heat treatable high strength aluminum alloy containing L12 dispersoids, comprising the steps of:
preparing an aluminum alloy composition containing:
at least one first element selected from the group consisting of about 0.1 to about 0.5 weight percent scandium, about 0.1 to about 6.0 weight percent erbium, about 0.1 to about 10.0 weight percent thulium, about 0.1 to about 15.0 weight percent ytterbium, and about 0.1 to about 12.0 weight percent lutetium;
at least one second element selected from the group consisting of about 0.1 to about 4.0 weight percent gadolinium, about 0.1 to about 4.0 weight percent yttrium, about 0.05 to about 1.0 weight percent zirconium, about 0.05 to about 2.0 weight percent titanium, about 0.05 to about 2.0 weight percent hafnium, and about 0.05 to about 1.0 weight percent niobium to the aluminum alloy;
at least one third element selected from the group consisting of about 4 to about 18 weight percent silicon, about 0.4 to about 3 weight percent magnesium, about 1 to about 2 weight percent lithium, about 3.5 to about 6.5 weight percent copper, about 4 to about 10 weight percent zinc, and about 1 to about 8 weight percent nickel;
melting the composition to form an alloy;
casting the alloy to form a solid product; and
heat treating the alloy to form L12 dispersoids.

### Claim 2 (depends on 1)

The method of claim 1, wherein the solid product is selected from the group comprising:
a usable part;
a billet for deformation processing; and
a powder.

### Claim 3 (depends on 1)

The method of claim 1, wherein casting comprises pouring the melted alloy into a mold.

### Claim 4 (depends on 1)

The method of claim 1, wherein casting comprises rapid solidification with cooling rates greater than 103° C/second by gas atomization formation of aluminum alloy powder.

### Claim 5 (depends on 4)

The method of claim 4, wherein the gas atomization process is an inert gas atomization process comprising:
inert gas consisting of at least one of argon, nitrogen and helium;
melt superheat temperature from about 100° F. (38° C.) to about 300° F. (149° C.);
gas pressure of about 50 psi (0.35 MPa) to about 750 psi (5.2 MPa);
metal flow rate of about from 0.5 pounds (0.23 kg) per minute to 25 pounds (11.3 kg) per minute; and
gas pressure to metal weight ratio is about 100 psi/lb/min (1.52 MPa/kg/min) to about 1500 psi/lbs/min (22.8 MPa/kg/min).

### Claim 6 (depends on 5)

The method of claim 5, wherein oxygen is introduced during atomization such that the oxygen content of the powder is between 1 ppm and 2000 ppm and the hydrogen content is about 1 ppm to about 1000 ppm.

### Claim at position 7

7-8. (canceled)

### Claim 9 (depends on 1)

The method of claim 1, wherein the heat treating comprises:
solution heat treatment at about 800° F. (426° C.) to about 1100° F. (593° C.) for about thirty minutes to four hours;
quenching; and
aging at a temperature of about 200° F. (93° C.) to about 600° F. (315° C.) for about two to forty eight hours.

### Claim 10 (depends on 9)

The method of claim 9, wherein heat treatment results in formation of L12 A13X strengthening dispersoids to form in the aged alloy.

### Claim at position 10

11-14. (canceled)

### Claim 15 (depends on 18)

The method of claim 18, wherein the heat treating comprises:
solution heat treatment at about 800° F. (426° C.) to about 1100° F. (593° C.) for about thirty minutes to four hours;
quenching; and
aging at a temperature of about 200° F. (93° C.) to about 600° F. (315° C.) for about two to forty eight hours.

### Claim at position 12

16-17. (canceled)

### Claim 18

A method for producing a heat treatable high strength aluminum alloy billet containing L12 dispersoids, comprising the steps of:
(a) forming a melt comprising:
at least one first element selected from the group comprising about 0.1 to about 0.35 weight percent scandium, about 0.1 to about 4.0 weight percent erbium, about 0.1 to about 6.0 weight percent thulium, about 0.2 to about 8.0 weight percent ytterbium, and about 0.2 to about 8.0 weight percent lutetium;
at least one second element selected from the group comprising about 0.2 to about 2.0 weight percent gadolinium, about 0.2 to about 2.0 weight percent yttrium, about 0.1 to about 0.75 weight percent zirconium, about 0.1 to about 1.0 weight percent titanium, about 0.1 to about 1.0 weight percent hafnium, and about 0.1 to about 0.75 weight percent niobium
at least one third element selected from the group consisting of about 4 to about 18 weight percent silicon, about 0.4 to about 3 weight percent magnesium, about 1 to about 2 weight percent lithium, about 3.5 to about 6.5 weight percent copper, about 4 to about 10 weight percent zinc, and about 1 to about 8 weight percent nickel;
the balance substantially aluminum;
(b) solidifying the melt to form a solid body; and
(c) heat treating the solid body.

### Claim 19 (depends on 18)

The method of claim 18, wherein solidifying comprises rapid solidification process with cooling rates greater than about 103° C/second by gas atomization formation of aluminum alloy powder.

### Claim at position 15

20-25. (canceled)