# US 2010/0133714 A1 · Bimodal polyethylene compositions for blow molding applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0133714 A1
- Document ID: US20100133714A1
- Status: Published application
- Kind: A1
- Application number: 12/624,046
- Filed: 2009-11-23
- Published: 2010-06-03
- Earliest claimed: 2004-08-19
- Assignees: Univation Technologies, LLC
- Inventors: Stephen P. Jaker; Sun-Chueh Kao; Dongming Li; Daniel P. Zilker, JR.; Ching-Tai Lue
- Web page: https://patentgrep.com/patent/US20100133714A1

## CPC

- B29B 7/421: {with screw and additionally other mixing elements on the same shaft, e.g. paddles, discs, bearings, rotor blades of the Banbury type}
- B29B 7/007: {for continuous mixing}
- B29B 7/845: {Venting, degassing or removing evaporated components in devices with rotary stirrers}
- B29C 48/10: flexible, e.g. blown foils
- B29C 48/67: having incorporated mixing devices not provided for in groups B29C48/52 - B29C48/66
- B29C 49/0005: {characterised by the material}
- B29C 49/04: Extrusion blow-moulding
- C08L 23/06: Polyethylene
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/29: in liquid form
- B29C 48/295: in gaseous form
- B29C 49/06: Injection blow-moulding
- B29C 2049/7862: {characterised by temperature values or ranges}
- B29C 2949/0715: the preform having one end closed
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2023/0633: {LDPE, i.e. low density polyethylene}
- B29K 2023/065: {HDPE, i.e. high density polyethylene}
- B29K 2105/0005: {containing compounding ingredients (releasing, lubricating or separating agents B29C33/56, fibers B29K2105/08, B29K2105/12; fillers B29K2105/16, recycled material B29K2105/26)}
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2314/06: Metallocene or single site catalysts
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Bimodal polyethylene compositions and methods for making the same are provided. In at least one specific embodiment, the bimodal polyethylene composition can include a high molecular weight component having a weight average molecular weight (Mw) of from about 400,000 to about 950,000. The bimodal polyethylene composition can also include a low molecular weight component having a weight average molecular weight (Mw) of from about 3,000 to about 100,000. The high molecular weight component can be present in an amount ranging from about 25 wt % to about 40 wt % of the bimodal polyethylene composition. The bimodal polyethylene composition can also have a percent die swell of less than about 80%.

## Claims

### Claim 1

A bimodal polyethylene composition, comprising:
a high molecular weight component having a weight average molecular weight (Mw) of from about 400,000 to about 950,000;
a low molecular weight component having a weight average molecular weight (Mw) of from about 3,000 to about 100,000, wherein the high molecular weight component is present in an amount ranging from about 25 wt % to about 40 wt % of the bimodal polyethylene composition; and
a percent die swell of less than about 80%.

### Claim 2 (depends on 1)

The composition of claim 1, further comprising a ratio of the weight average molecular weight of the high molecular weight component to the weight average molecular weight of the low molecular weight component of from about 15 to about 35.

### Claim 3 (depends on 1)

The composition of claim 1, further comprising a density of from about 0.95 g/cm3 to about 0.97 g/cm3.

### Claim 4 (depends on 1)

The composition of claim 1, further comprising a weight average molecular weight (Mw) of from about 200,000 to about 450,000, a z-average molecular weight (Mz) of from 2,000,000 Daltons to about 3,500,000 Daltons, and a z+1 average molecular weight (Mz+1) of from about 2,000,000 Daltons to about 6,000,000 Daltons.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the percent die swell is greater than about 65%.

### Claim 6 (depends on 1)

The composition of claim 1, further comprising a flow index (I21) of from about 20 g/10 min to about 40 g/10 min.

### Claim 7 (depends on 1)

The composition of claim 1, further comprising an elasticity (G′/G″) of about 0.8 or more.

### Claim 8 (depends on 1)

The composition of claim 1, further comprising an environmental stress crack resistance of at least 180 hours in accordance with ASTM D-1693, Procedure B, reported as F50 hours.

### Claim 9

A method for making a bimodal polyethylene composition, comprising:
heating a bimodal polyethylene to produce a substantially melted bimodal polyethylene;
contacting the substantially melted bimodal polyethylene with a gas mixture comprising from about 8 vol % to about 20 vol % oxygen to produce an oxygen tailored bimodal polyethylene; and
cooling the oxygen tailored bimodal polyethylene to produce a bimodal polyethylene composition comprising:
a high molecular weight component having a weight average molecular weight (Mw) of from about 400,000 to about 950,000;
a low molecular weight component having a weight average molecular weight (Mw) of from about 3,000 to about 100,000, wherein the high molecular weight component is present in an amount ranging from about 25 wt % to about 40 wt % of the bimodal polyethylene composition; and
a percent die swell of less than about 80%.

### Claim 10 (depends on 9)

The method of claim 9, wherein the substantially melted bimodal polyethylene is heated to a temperature of from about 240° C. to about 260° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein the bimodal polyethylene composition further comprises an elasticity (G′/G″) of about 0.8 or more.

### Claim 12 (depends on 9)

The method of claim 9, wherein the bimodal polyethylene composition further comprises a ratio of the weight average molecular weight of the high molecular weight component to the weight average molecular weight of the low molecular weight component of from about 15 to about 35.

### Claim 13 (depends on 9)

The method of claim 9, further comprising forming the bimodal polyethylene composition into a blow molded article.

### Claim 14

A method for making a bimodal polyethylene composition, comprising:
conveying a bimodal polyethylene through a mixer/extruder, wherein the mixer/extruder comprises a melt-conveying zone, and wherein the bimodal polyethylene is substantially melted in the melt-conveying zone; and
contacting the substantially melted polyethylene with a gas mixture comprising from about 8 vol % oxygen to about 20 vol % oxygen within the melt-conveying zone, to produce a bimodal polyethylene composition comprising:
a high molecular weight component having a weight average molecular weight (Mw) of from about 400,000 to about 950,000;
a low molecular weight component having a weight average molecular weight (Mw) of from about 3,000 to about 100,000, wherein the high molecular weight component is present in an amount ranging from about 25 wt % to about 40 wt % of the bimodal polyethylene composition, and wherein a ratio of the weight average molecular weight of the high molecular weight component to the weight average molecular weight of the low molecular weight component ranges from about 15 to about 35; and
a percent die swell of less than about 80%.

### Claim 15 (depends on 14)

The method of claim 14, further comprising pelletizing the bimodal polyethylene composition to produce a pelletized polyethylene product.

### Claim 16 (depends on 15)

The method of claim 15, further comprising forming the pelletized polyethylene product into a blow molded article.

### Claim 17 (depends on 14)

The method of claim 14, wherein the bimodal polyethylene composition further comprises an elasticity (G′/G″) of about 0.8 or more.

### Claim 18 (depends on 14)

The method of claim 14, wherein the bimodal polyethylene composition further comprises a density of from about 0.95 g/cm3 to about 0.97 g/cm3.

### Claim 19 (depends on 14)

The method of claim 14, wherein the bimodal polyethylene composition further comprises a flow index (I21) of from about 20 g/10 min to about 40 g/10 min.