# US 2010/0133466 A1 · Cerium carbonate powder, method for preparing the same, cerium oxide powder made therefrom, method for preparing the same, and CMP slurry comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0133466 A1
- Document ID: US20100133466A1
- Status: Published application
- Kind: A1
- Application number: 12/591,227
- Filed: 2009-11-12
- Published: 2010-06-03
- Earliest claimed: 2005-09-20
- Assignees: LG Chem, Ltd.
- Inventors: Myoung Hwan Oh; Jun Seok Nho; Jong Pil Kim; Jang Yul Kim; Seung Beom Cho
- Web page: https://patentgrep.com/patent/US20100133466A1

## CPC

- C01F 17/247: Carbonates
- C01F 17/235: Cerium oxides or hydroxides
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/03: obtained by SEM
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/80: Compositional purity
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Disclosed is a method for preparing cerium carbonate powder by mixing a cerium precursor solution with a carbonate precursor solution to cause precipitation, wherein at least one solvent used in the cerium precursor solution and the carbonate precursor solution is an organic solvent. Cerium carbonate powder obtained from the method, cerium oxide powder obtained from the cerium carbonate powder, a method for preparing the cerium oxide powder, and CMP slurry comprising the cerium oxide powder are also disclosed. The method for preparing cerium carbonate using an organic solvent, allows the resultant cerium carbonate powder to have a size and shape controllable from the initial nucleation step. Additionally, it is possible to easily control the size and shape of cerium oxide powder obtained from the cerium carbonate powder.

## Claims

### Claim 1

A method for preparing cerium carbonate powder comprising mixing a cerium precursor solution with a carbonate precursor solution to cause precipitation,
wherein at least one solvent used in the cerium precursor solution and the carbonate precursor solution is a water-soluble organic solvent, and
the cerium precursor solution and the carbonate precursor solution contains only continuous phase, not containing non-continuous phase.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the organic solvent has a dielectric constant ranging from 20 to 80.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the organic solvent has at least one hydrophilic group selected from the group consisting of hydroxyl group (—OH), ketone group (—CO—), carboxyl group (—COOH), sulfonic acid group (—SO3H), amino group (—NH2) and ammonium group (—NH4).

### Claim 4 (depends on 1)

The method according to claim 1, wherein the organic solvent is at least one solvent selected from the group consisting of alcohols, glycols, acetone, glycerol, formic acid and ethyl acetate.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the cerium carbonate solution and the carbonate precursor solution are used in a molar ratio ranging from 1:0.5 to 1:5.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the precipitation is carried out at a temperature ranging from 60° C. to the boiling point of the organic solvent used therein.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the precipitation is carried out for 30 minutes˜60 hours.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the cerium carbonate powder obtained from the method has a size of 50 nm˜5 μm.

### Claim 9

Cerium carbonate powder in which carbon residue other than carbonate group (—CO3) remains in an amount of 0.1 ppm˜100 ppm.

### Claim 10 (depends on 9)

The cerium carbonate powder according to claim 9, which is obtained by mixing a cerium precursor solution with a carbonate precursor solution to cause precipitation,
wherein at least one solvent used in the cerium precursor solution and the carbonate precursor solution is a water-soluble organic solvent, and
the cerium precursor solution and the carbonate precursor solution contains only continuous phase, not containing non-continuous phase.

### Claim 11

A method for preparing cerium oxide powder, which comprises the steps of:
(a) preparing cerium carbonate powder by mixing a cerium precursor solution with a carbonate precursor solution to cause precipitation, wherein at least one solvent used in the cerium precursor solution and the carbonate precursor solution is an water-soluble organic solvent, and the cerium precursor solution and the carbonate precursor solution contains only continuous phase, not containing non-continuous phase; and
(b) firing the cerium carbonate powder obtained from the step(a) at a heat treatment temperature of 300° C.˜1000° C.

### Claim 12 (depends on 11)

The method for preparing cerium oxide powder according to claim 11, wherein the organic solvent has a dielectric constant ranging from 20 to 80.

### Claim 12 (depends on 11)

The method for preparing cerium oxide powder according to claim 11, wherein the organic solvent has a dielectric constant ranging from 20 to 80.

### Claim 13 (depends on 11)

The method for preparing cerium oxide powder according to claim 11, wherein the organic solvent has at least one hydrophilic group selected from the group consisting of hydroxyl group (—OH), ketone group (—CO—), carboxyl group (—COOH), sulfonic acid group (—SO3H), amino group (—NH2) and ammonium group (—NH4).

### Claim 14 (depends on 11)

The method for preparing cerium oxide powder according to claim 11, wherein the organic solvent is at least one solvent selected from the group consisting of alcohols, glycols, acetone, glycerol, formic acid and ethyl acetate.

### Claim 15 (depends on 12)

Cerium oxide powder obtained by the method as defined in claim 12.

### Claim 16 (depends on 12)

CMP slurry comprising 100 parts by weight of cerium oxide powder obtained by the method as defined in claim 12, and 0.001˜10 parts by weight of a dispersant.