# US 2010/0133096 A1 · Use of Austenitic Stainless Steel as Construction Material in a Device or Structural Component Which is Exposed to an Oxygen and/or Hydrogen and/or Hydrofluoric Acid Environment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0133096 A1
- Document ID: US20100133096A1
- Status: Published application
- Kind: A1
- Application number: 12/308,895
- Filed: 2007-06-27
- Published: 2010-06-03
- Earliest claimed: 2006-06-28
- Assignees: Hydrogen Technologies LLC
- Inventors: Rolf Steen Hansen; Sten Egil Johnsen; Hans Jörg Fell; Egil Rasten
- Web page: https://patentgrep.com/patent/US20100133096A1

## CPC

- C22C 38/44: with molybdenum or tungsten
- C22C 19/056: {with the maximum Cr content being at least 10% but less than 20%}
- C22C 30/00: Alloys containing less than 50% by weight of each constituent
- C22C 30/02: containing copper
- C22C 38/42: with copper
- C22C 38/58: with more than 1.5% by weight of manganese
- C25B 9/00: Cells or assemblies of cells; Constructional parts of cells; Assemblies of constructional parts, e.g. electrode-diaphragm assemblies; Process-related cell features
- H01M 8/2475: Enclosures, casings or containers of fuel cell stacks
- Y02E 60/36: Hydrogen production from non-carbon containing sources, e.g. by water electrolysis
- Y02E 60/50: Fuel cells
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Use of an austenitic stainless steel wherein the chemical composition comprises 10-20 weight % nickel, 10-20 weight % chromium, 30-50 weight % iron, maximum 17 weight % of another element or elements and the balance iron and/or chromium and/or nickel as construction material in a device or structural components that are exposed to an oxygen and/or a hydrogen and/or a hydrofluoric acid environment.

## Claims

### Claim at position 1

1-8. (canceled)

### Claim 9

A method of inhibiting degradation of a construction material in a device or structural component that is exposed to an environment comprising hydrofluoric acid and oxygen and/or hydrogen, which comprises fabricating the construction material of an austenitic stainless steel having a chemical composition which comprises
10-31.0 weight % nickel,
10-27.3 weight % chromium,
30-52.8 weight % iron, and
maximum 17 weight % of another element or elements, selected among N, Mn, Mo, Cu, Nb, Ti, V, Ce, B, W, Si and Co.

### Claim 10 (depends on 9)

The method according to claim 9,
wherein said composition comprises 0.5-2 weight % copper.

### Claim 11 (depends on 9)

The method according to claim 9,
wherein said composition comprises 3-8 weight % molybdenum.

### Claim 12 (depends on 9)

The method according to claim 9,
wherein said composition comprises maximum 12.5 weight % of another element or elements.

### Claim 13 (depends on 9)

The method according to claim 9,
wherein said composition comprises maximum 12 weight % of another element or elements.

### Claim 14 (depends on 9)

The method according to claim 9,
wherein said composition comprises maximum 9 weight % of another element or elements.

### Claim 15 (depends on 9)

An electrolyser comprising a housing and a cell stack having at least one electrochemical cell for electrolysis of water at a temperature between 5-100° C. and at a pressure between ambient and 50 bar,
characterised in that
said housing and other structural components of said electrolyser are made of a material which is an austenitic stainless steel in accordance with claim 9.

### Claim 16 (depends on 10)

The method according to claim 10,
wherein said composition comprises 3-8 weight % molybdenum.

### Claim 17 (depends on 10)

The method according to claim 10,
wherein said composition comprises maximum 9 weight % of another element or elements.

### Claim 18 (depends on 11)

The method according to claim 11,
wherein said composition comprises maximum 9 weight % of another element or elements.

### Claim 19 (depends on 10)

An electrolyser comprising a housing and a cell stack having at least one electrochemical cell for electrolysis of water at a temperature between 5-100° C. and at a pressure between ambient and 50 bar,
characterised in that
said housing and other structural components of said electrolyser are made of a material which is an austenitic stainless steel in accordance with claim 10.

### Claim 20 (depends on 11)

An electrolyser comprising a housing and a cell stack having at least one electrochemical cell for electrolysis of water at a temperature between 5-100° C. and at a pressure between ambient and 50 bar,
characterised in that
said housing and other structural components of said electrolyser are made of a material which is an austenitic stainless steel in accordance with claim 11.

### Claim 21 (depends on 12)

An electrolyser comprising a housing and a cell stack having at least one electrochemical cell for electrolysis of water at a temperature between 5-100° C. and at a pressure between ambient and 50 bar,
characterised in that
said housing and other structural components of said electrolyser are made of a material which is an austenitic stainless steel in accordance with claim 12.

### Claim 22 (depends on 13)

An electrolyser comprising a housing and a cell stack having at least one electrochemical cell for electrolysis of water at a temperature between 5-100° C. and at a pressure between ambient and 50 bar,
characterised in that
said housing and other structural components of said electrolyser are made of a material which is an austenitic stainless steel in accordance with claim 13.

### Claim 23 (depends on 14)

An electrolyser comprising a housing and a cell stack having at least one electrochemical cell for electrolysis of water at a temperature between 5-100° C. and at a pressure between ambient and 50 bar,
characterised in that
said housing and other structural components of said electrolyser are made of a material which is an austenitic stainless steel in accordance with claim 14.