# US 2010/0133089 A1 · Magnetron sputtering apparatus and method for manufacturing thin film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0133089 A1
- Document ID: US20100133089A1
- Status: Published application
- Kind: A1
- Application number: 12/468,222
- Filed: 2009-05-19
- Published: 2010-06-03
- Earliest claimed: 2008-05-22
- Assignees: c/o CANON ANELVA CORPORATION
- Inventors: Seishi Horiguchi
- Web page: https://patentgrep.com/patent/US20100133089A1

## CPC

- H01J 37/3408: {Planar magnetron sputtering}
- C23C 14/067: {Borides}
- C23C 14/345: {using substrate bias}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/56: Apparatus specially adapted for continuous coating; Arrangements for maintaining the vacuum, e.g. vacuum locks
- C23C 14/5826: {Treatment with charged particles (C23C14/582 takes precedence)}
- C23C 14/584: {Non-reactive treatment}
- H01J 37/3452: {Magnet distribution}
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

In the present invention, in forming a LaB6 thin film by magnetron sputtering, the single-crystal properties in the wide domain direction in the obtained LaB6 thin film are improved. In one embodiment of the present invention, in a magnetron sputtering apparatus, parallel magnetic field strength on a surface of the substrate is set to 0.1 times or less parallel magnetic field strength on a surface of the target.

## Claims

### Claim 1

A magnetron sputtering apparatus comprising:
a substrate holder that can hold a substrate; and
a magnetron cathode having a cathode on which a target can be mounted, and a magnetic field generating apparatus,
wherein parallel magnetic field strength (in gauss) on a surface of the substrate is set to 0.1 times or less parallel magnetic field strength (in gauss) on a surface of the target.

### Claim 2 (depends on 1)

The magnetron sputtering apparatus according to claim 1, wherein the parallel magnetic field strength on the surface of the target is set to 200 gauss or more and 1000 gauss or less.

### Claim 3 (depends on 1)

The magnetron sputtering apparatus according to claim 1, wherein the magnetic field generating apparatus has a sub-magnet array structure in which sub-magnets are located along rows and columns so that neighboring sub-magnets are in a relationship of having opposite magnetic polarities to each other.

### Claim 4 (depends on 1)

The magnetron sputtering apparatus according to claim 1, wherein the magnetic field generating apparatus can oscillate in a direction horizontal to a plane of the cathode or the surface of the target.

### Claim 5 (depends on 1)

The magnetron sputtering apparatus according to claim 1, wherein the target contains a lanthanide compound containing at least one element selected from light elements and at least one element selected from lanthanide elements.

### Claim 6 (depends on 5)

The magnetron sputtering apparatus according to claim 5, wherein the light element is at least one selected from the group consisting of lithium, beryllium, boron, carbon, fluorine, sodium, magnesium, phosphorus, and sulfur.

### Claim 7 (depends on 5)

The magnetron sputtering apparatus according to claim 5, wherein the target includes a boron-lanthanum compound containing boron and lanthanum.

### Claim 8 (depends on 1)

The magnetron sputtering apparatus according to claim 1, wherein the parallel magnetic field strength on the surface of the substrate is set to 20 gauss or less.

### Claim 9 (depends on 1)

The magnetron sputtering apparatus according to claim 1, wherein the parallel magnetic field strength on the surface of the substrate is set to 0.01 times or less parallel magnetic field strength on a surface of the target.

### Claim 10

A method for manufacturing a thin film, comprising the steps of:
preparing a substrate; and
depositing a thin film of a lanthanide compound containing at least one element selected from light elements and at least one element selected from lanthanide elements on the substrate by a magnetron sputtering method using a target of the lanthanide compound,
wherein parallel magnetic field strength (in gauss) on a surface of the substrate is set to 0.1 times or less parallel magnetic field strength (in gauss) on a surface of the target.

### Claim 11 (depends on 10)

The method for manufacturing a thin film according to claim 10, wherein the light element is at least one selected from the group consisting of lithium, beryllium, boron, carbon, fluorine, sodium, magnesium, phosphorus, and sulfur.

### Claim 12 (depends on 10)

The method for manufacturing a thin film according to claim 10, wherein the target includes a boron-lanthanum compound containing boron and lanthanum.