# US 2010/0132851 A1 · Copper alloy plate and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0132851 A1
- Document ID: US20100132851A1
- Status: Published application
- Kind: A1
- Application number: 12/624,472
- Filed: 2009-11-24
- Published: 2010-06-03
- Earliest claimed: 2008-11-28
- Assignees: Dowa Metaltech Co., Ltd.
- Inventors: Weilin Gao; Hisashi Suda; Hiroto Narieda; Akira Sugawara
- Web page: https://patentgrep.com/patent/US20100132851A1

## CPC

- C22C 9/00: Alloys based on copper
- C22F 1/08: of copper or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A sheet material of a copper alloy has a chemical composition comprising 1.2 to 5.0 wt % of titanium, and the balance being copper and unavoidable impurities, the material having a mean crystal grain size of 5 to 25 μm and (maximum crystal grain size−minimum crystal grain size)/(mean crystal grain size) being 0.20 or less, assuming that the maximum, minimum and mean values of mean values, each of which is the mean value of crystal grain sizes in a corresponding one of a plurality of regions which are selected from the surface of the sheet material at random and which have the same shape and size, are the maximum, minimum and mean crystal grain sizes, respectively, and the material having a crystal orientation satisfying I{420}/I0{420}>1.0, assuming that the intensities of X-ray diffraction on the {420} crystal plane of the surface of the material and the standard powder of pure copper are I{420} and I0{420}, respectively.

## Claims

### Claim 1

A sheet material of a copper alloy having a chemical composition comprising 1.2 to 5.0 wt % of titanium, and the balance being copper and unavoidable impurities,
wherein the sheet material of the copper alloy has a mean crystal grain size of 5 to 25 μm, and (maximum crystal grain size−minimum crystal grain size)/(mean crystal grain size) is not greater than 0.20, assuming that the maximum value of mean values, each of which is the mean value of crystal grain sizes in a corresponding one of a plurality of regions which are selected from a surface of the sheet material of the copper alloy at random and which have the same shape and size, is the maximum crystal grain size, that the minimum value of the mean values is the minimum crystal grain size and that the mean value of the mean values is the mean crystal grain size, and
wherein the sheet material of the copper alloy has a crystal orientation which satisfies I{420}/I0{420}>1.0, assuming that the intensity of X-ray diffraction on the {420} crystal plane on the surface of the sheet material of the copper alloy is I{420} and that the intensity of X-ray diffraction on the {420} crystal plane of the standard powder of pure copper is I0{420}.

### Claim 2 (depends on 1)

A sheet material of a copper alloy as set forth in claim 1, wherein said crystal orientation of the sheet material of the copper alloy satisfies I{220}/I0{220}≦4.0, assuming that the intensity of X-ray diffraction on the {220} crystal plane on the surface of the sheet material of the copper alloy is I{220} and that the intensity of X-ray diffraction on the {220} crystal plane of the standard powder of pure copper is I0{220}.

### Claim 3 (depends on 1)

A sheet material of a copper alloy as set forth in claim 1, wherein said chemical composition of the sheet material of the copper alloy further comprises one or more elements which are selected from the group consisting of 1.5 wt % or less of nickel, 1.0 wt % or less of cobalt and 0.5 wt % or less of iron.

### Claim 4 (depends on 1)

A sheet material of a copper alloy as set forth in claim 1, wherein said chemical composition of the sheet material of the copper alloy further comprises one or more elements which are selected from the group consisting of 1.2 wt % or less of tin, 2.0 wt % or less of zinc, 1.0 wt % or less of magnesium, 1.0 wt % or less of zirconium, 1.0 wt % or less of aluminum, 1.0 wt % or less of silicon, 0.1 wt % or less of phosphorus, 0.05 wt % or less of boron, 1.0 wt % or less of chromium, 1.0 wt % or less of manganese, 1.0 wt % or less of vanadium, 1.0 wt % or less of silver, 1.0 wt % or less of beryllium and 1.0 wt % or less of misch metal, the total amount of these elements being 3 wt % or less.

### Claim 5 (depends on 1)

A sheet material of a copper alloy as set forth in claim 1, which has a 0.2% yield strength of 850 MPa or more, and wherein if the 90° W bending test of a first test piece, which is cut off from the sheet material of the copper alloy so that the longitudinal direction of the first test piece is the rolling direction LD of the sheet material of the copper alloy, is carried out so that the bending axis of the first test piece is a direction TD perpendicular to the rolling direction and thickness direction of the first test piece, and if the 90° W bending test of a second test piece, which is cut off from the sheet material of the copper alloy so that the longitudinal direction of the second test piece is the TD, is carried out so that the bending axis of the second test piece is the LD, the ratio R/t of the minimum bending radius R to the thickness t of each of the first and second test pieces is 1.0 or less.

### Claim 6

A method for producing a sheet material of a copper alloy, the method comprising the steps of:
melting and casting raw materials of a copper alloy to form an ingot, said copper alloy having a chemical composition which consists of: 1.2 to 5.0 wt % of titanium; optionally one or more elements which are selected from the group consisting of 1.5 wt % or less of nickel, 1.0 wt % or less of cobalt and 0.5 wt % or less of iron; optionally one or more elements which are selected from the group consisting of 1.2 wt % or less of tin, 2.0 wt % or less of zinc, 1.0 wt % or less of magnesium, 1.0 wt % or less of zirconium, 1.0 wt % or less of aluminum, 1.0 wt % or less of silicon, 0.1 wt % or less of phosphorus, 0.05 wt % or less of boron, 1.0 wt % or less of chromium, 1.0 wt % or less of manganese, 1.0 wt % or less of vanadium, 1.0 wt % or less of silver, 1.0 wt % or less of beryllium and 1.0 wt % or less of misch metal, the total amount of these elements being 3 wt % or less; and the balance being copper and unavoidable impurities;
hot-rolling the ingot in a temperature range of from 950° C. to 500° C. to form a plate of the copper alloy, by hot-rolling the ingot at a rolling reduction of not less than 30% in a temperature range of from less than 700° C. to 500° C. after carrying out an initial rolling pass in a temperature range of from 950° C. to 700° C.;
cold-rolling the plate of the copper alloy at a rolling reduction of not less than 85%;
carrying out a solution treatment which holds the plate of the copper alloy in a temperature range of from 750° C. to 1000° C. for 5 seconds to 5 minutes;
cold-rolling the plate of the copper alloy at a rolling reduction of 0 to 50% after the solution treatment;
ageing the plate of the copper alloy, which is cold-rolled after the solution treatment, at a temperature of 300 to 550° C.; and
finish cold-rolling the aged plate of the copper alloy at a rolling reduction of 0 to 30%.

### Claim 7 (depends on 6)

A method for producing a sheet material of a copper alloy as set forth in claim 6, wherein said ingot is hot-rolled at a rolling reduction of not less than 60% in the temperature range of from 950° C. to 700° C.

### Claim 8 (depends on 6)

A method for producing a sheet material of a copper alloy as set forth in claim 6, wherein said rolling reduction in cold-rolling between said hot-rolling and said solution treatment is not less than 90%.

### Claim 9 (depends on 6)

A method for producing a sheet material of a copper alloy as set forth in claim 6, wherein said solution treatment is carried out by a heat treatment which holds said plate of the copper alloy at a higher temperature than a solid solubility curve of the copper alloy by 30° C. or more, in said temperature range of from 750° C. to 1000° C. for a holding period of time which is adjusted so that the mean crystal grain size of the plate of the copper alloy after the solution treatment is in the range of from 5 μm to 25 μm.

### Claim 10 (depends on 6)

A method for producing a sheet material of a copper alloy as set forth in claim 6, wherein assuming that the ageing temperature capable of obtaining the maximum hardness in a chemical composition of said copper alloy is TM (° C.) and that the maximum hardness thereof is HM (HV), the ageing temperature in the ageing treatment is set to be a temperature which is TM±10° C. in the temperature range of from 300° C. to 550° C., and the ageing time in the ageing treatment is set so that the hardness of the sheet material of the copper alloy is in the range of from 0.90HM to 0.95HM after the ageing treatment.

### Claim 11 (depends on 6)

A method for producing a sheet material of a copper alloy as set forth in claim 6, wherein a low temperature annealing operation is carried out at a temperature of 150 to 450° C. after the finish cold rolling.

### Claim 12 (depends on 1)

A connector terminal using said sheet material of the copper alloy as set forth in claim 1, as a material thereof.