# US 2010/0132509 A1 · Method for thiosulfate leaching of precious metal-containing materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0132509 A1
- Document ID: US20100132509A1
- Status: Published application
- Kind: A1
- Application number: 12/700,525
- Filed: 2010-02-04
- Published: 2010-06-03
- Earliest claimed: 2000-05-19
- Assignees: Placer Dome Technical Services Limited
- Inventors: Jinxing Ji; Christopher Andrew Fleming; Paul George West-Sells; Ralph Peter Hackl
- Web page: https://patentgrep.com/patent/US20100132509A1

## CPC

- C22B 11/04: {by wet processes (extraction of metal compounds by leaching in organic solutions C22B3/16; treatment or purification of solutions by liquid-liquid extraction C22B3/26)}
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/24: by adsorption on solid substances, e.g. by extraction with solid resins
- C22B 3/42: by ion-exchange extraction
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Processes are provided for recovering precious metals from refractory materials using thiosulfate lixiviants. The processes can employ lixiviants that include at most only small amounts of copper and/or ammonia and operate at a relatively low pH, reduction of polythionates, inert atmospheres to control polythionate production, and electrolytic solutions which provide relatively high rates of precious metal recovery.

## Claims

### Claim at position 1

1-96. (canceled)

### Claim 97

A method, comprising:
(a) contacting a precious metal-containing material with a thiosulfate lixiviant to dissolve the precious metal and form a pregnant leach solution containing the dissolved precious metal, wherein the contacting step (a) is performed in the presence of a molecular-oxygen enriched atmosphere relative to the ambient atmosphere and in the absence or substantial absence of at least one of added copper and ammonia; and
(b) recovering the dissolved precious metal from the pregnant leach solution.

### Claim 98 (depends on 97)

The method of claim 97, wherein a level of molecular oxygen in the molecular-enriched atmosphere is more than about 3 psia to as much as about 500 psia.

### Claim 99 (depends on 98)

The method of claim 98, wherein the level of molecular oxygen in the molecular-enriched atmosphere ranges from about 10 psia to about 115 psia.

### Claim 100 (depends on 99)

The method of claim 99, wherein the level of molecular oxygen in the molecular-enriched atmosphere ranges from about 10 psia to about 115 psia.

### Claim 101 (depends on 100)

The method of claim 100, wherein the level of molecular oxygen in the molecular-enriched atmosphere ranges from about 15 psia to about 65 psia.

### Claim 102 (depends on 97)

The method of claim 97, wherein the contacting step (a) is performed at superatmospheric pressure and wherein the total operating pressure ranges from about 15 to about 600 psia.

### Claim 103 (depends on 102)

The method of claim 102, wherein the total operating pressure ranges from about 15 to about 130 psia.

### Claim 104 (depends on 97)

The method of claim 97, wherein the at least one of added copper and ammonia is copper and wherein a total concentration of copper in the lixiviant is no more than about 20 ppm.

### Claim 105 (depends on 97)

The method of claim 97, wherein the at least one of added copper and ammonia is ammonia and wherein a total concentration of ammonia in the lixiviant is no more than about 0.05 M.

### Claim 106 (depends on 97)

The method of claim 97, wherein an oxidation-reduction potential of the lixiviant during contacting step (a) ranges from about 150 to about 300 mV (relative to the standard hydrogen electrode).

### Claim 107

A method, comprising:
(a) contacting a precious metal-containing material with a thiosulfate lixiviant to dissolve the precious metal and form a pregnant thiosulfate leach solution containing the dissolved precious metal and a polythionate;
(b) contacting at least one of the pregnant leach solution and a barren leach solution derived therefrom with a polythionate reductant selected from the group consisting essentially of hydrogen gas, hydrogen sulfide gas, elemental sulfur, carbon monoxide and mixtures thereof, whereby at least most of the polythionate is reduced to thiosulfate; and
(c) recovering the dissolved precious metal from the pregnant thiosulfate leach solution.

### Claim 108 (depends on 107)

The method of claim 107, wherein the polythionate reductant is hydrogen gas.

### Claim 109 (depends on 107)

The method of claim 107, wherein the polythionate reductant is elemental sulfur.

### Claim 110 (depends on 107)

The method of claim 107, wherein the polythionate reductant is carbon monoxide.

### Claim 111

A method, comprising:
(a) contacting a precious metal-containing material with a thiosulfate lixiviant to dissolve the precious metal and form a pregnant thiosulfate leach solution containing the dissolved precious metal and a polythionate;
(b) contacting the pregnant thiosulfate leach solution with at least one of a sulfite-containing reagent and a sulfide-containing reagent to convert at least most of the polythionates into thiosulfate;
(c) thereafter contacting the pregnant leach solution with an extraction agent to collect at least most of the dissolved precious metal on the extraction agent and form a barren thiosulfate leach solution for recycle to step (a); and
(d) recovering the collected precious metal from the precious metal loaded extraction agent.

### Claim 112 (depends on 111)

The method of claim 111, further comprising, after step (b) and before step (c):
conditioning the pregnant leach solution in an oxidizing atmosphere to redissolve any precipitated precious metal sulfides.

### Claim 113 (depends on 111)

The method of claim 111, wherein polythionates compete with dissolved precious metal complexes for loading on the extraction agent.

### Claim 114 (depends on 112)

The method of claim 112, wherein the at least one of a sulfite-containing reductant and sulfide-containing reductant is the sulfite-containing reductant and wherein the sulfite-containing reductant is at least one of a metabisulfite and sulfur dioxide.

### Claim 115 (depends on 112)

The method of claim 112, wherein the at least one of a sulfite-containing reductant and sulfide-containing reductant is the sulfide-containing reductant and wherein the sulfide-containing reductant is at least one of a bisulfide, sulfide, hydrogen sulfide gas, and a polysulfide.

### Claim 116

A method, comprising:
(a) contacting a precious metal-containing material with a thiosulfate lixiviant to dissolve the precious metal and form a pregnant thiosulfate leach solution containing the dissolved precious metal;
(b) recovering the dissolved precious metal from the pregnant thiosulfate leach solution to form a barren leach solution; and
(c) sparging an at least substantially nonoxidizing gas through at least one of the pregnant thiosulfate leach solution and barren leach solution to inhibit the formation of polythionates.

### Claim 117 (depends on 116)

The method of claim 116, wherein the substantially nonoxidizing gas is substantially free of oxidants.

### Claim 118 (depends on 116)

The method of claim 116, wherein the substantially nonoxidizing gas comprises at least about 85 vol. % of an inert gas and no more than about 5 vol. % oxidants.

### Claim 119 (depends on 107)

The method of claim 107, wherein the polythionate reductant is hydrogen sulfide gas.