# US 2010/0091360 A1 · Optical component made from synthetic quartz glass with enhanced radiation resistance, and method for producing the component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0091360 A1
- Document ID: US20100091360A1
- Status: Published application
- Kind: A1
- Application number: 12/449,790
- Filed: 2008-02-20
- Published: 2010-04-15
- Earliest claimed: 2007-02-27
- Assignees: Heraeus Quarzglas GmbH & Co. KG
- Inventors: Bodo Kuehn; Stefan Ochs; Juergen Weber
- Web page: https://patentgrep.com/patent/US20100091360A1

## CPC

- C03B 19/1453: {Thermal after-treatment of the shaped article, e.g. dehydrating, consolidating, sintering}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- G03F 7/70958: {Optical materials or coatings, e.g. with particular transmittance, reflectance or anti-reflection properties}
- C03B 2201/075: Hydroxyl ion (OH)
- C03B 2201/10: doped with boron (C03B2201/14 takes precedence)
- C03B 2201/21: doped with molecular hydrogen
- C03B 2201/23: doped with hydroxyl groups
- C03B 2201/24: doped with nitrogen, e.g. silicon oxy-nitride glasses
- C03B 2201/32: doped with aluminium (C03B2201/36 takes precedence)
- C03B 2201/34: doped with rare earth metals, i.e. with Sc, Y or lanthanides, e.g. for laser-amplifiers
- C03B 2201/40: doped with transition metals other than rare earth metals, e.g. Zr, Nb, Ta or Zn
- C03C 2201/10: containing boron (C03C2201/14 takes precedence)
- C03C 2201/21: containing molecular hydrogen
- C03C 2201/23: containing hydroxyl groups
- C03C 2201/24: containing nitrogen, e.g. silicon oxy-nitride glasses
- C03C 2201/32: containing aluminium (C03C2201/36 takes precedence)
- C03C 2201/3411: Yttrium
- C03C 2201/3441: Samarium
- C03C 2201/40: containing transition metals other than rare earth metals, e.g. Zr, Nb, Ta or Zn
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

To provide an optical component of quartz glass for use in a projection objective for immersion lithography at an operating wavelength below 250 nm, which component is optimized for use with linearly polarized UV laser radiation and particularly with respect to compaction and birefringence induced by anisotropic density change, it is suggested according to the invention that the quartz glass should contain hydroxyl groups in the range of from 1 wtppm to 60 wtppm and chemically bound nitrogen, and that the mean hydrogen content of the quartz glass should be in the range of 5×1015 molecules/cm to 1×1017 molecules/cm3.

## Claims

### Claim 1

An optical component used in immersion lithography at an operating wavelength below 250 nm, said optical component comprising: synthetic quartz glass that contains hydroxyl groups in a range of 1 wtppm to 60 wtppm and chemically bound nitrogen, and wherein said quartz glass has a mean hydrogen content in a range of 5×1015 molecules/cm3 to 1×1017 molecules/cm3.

### Claim 2 (depends on 1)

The component according to claim 1, wherein the quartz glass has a nitrogen content in a range between 1 wtppm and 150 wtppm.

### Claim 3 (depends on 2)

The component according to claim 2, wherein the quartz glass has a nitrogen content in a range between 10 wtppm and 100 wtppm,

### Claim 4

An optical component used in a projection objective for immersion lithography at an operating wavelength below 250 nm, said optical component comprising: synthetic quartz glass that comprises hydroxyl groups in a range of 1 wtppm to 60 wtppm and that is doped with boron, the the quartz glass having a content of boron oxide in a range between 1 wtppm and 250 wtppm.

### Claim 5 (depends on 4)

The component according to claim 4, wherein the content of boron oxide is in a range between 10 wtppm and 120 wtppm.

### Claim 6 (depends on 1)

The component according to claim 1, wherein the quartz glass is doped with nitrogen and with boron.

### Claim 7 (depends on 1)

The component according to claim 1, wherein the quartz glass is doped with oxides or nitrides of trivalent network formers, said trivalent network formers being selected from the group consisting of Y, Sm and Zr.

### Claim 8 (depends on 1)

The component according to claim 1, wherein the quartz glass is doped with aluminum.

### Claim 9 (depends on 8)

The component according to claim 8, wherein the quartz glass has a mean content of aluminum oxide that is more than 1.2 wt ppm.

### Claim 10 (depends on 9)

The component according to claim 9, wherein the quartz glass has a mean content of aluminum oxide that is at least 10 wtppm.

### Claim 11 (depends on 1)

The component according to claim 1, wherein the quartz glass has a content of hydroxyl groups of less than 40 wtppm.

### Claim 12 (depends on 1)

The component according to claim 1, wherein the quartz glass has a viscosity of at least 1013 dPa's at a temperature of 1200° C.

### Claim 13 (depends on 1)

The component according to claim 1, wherein the quartz glass has a content of chlorine of less than 50 wtppm.

### Claim 14 (depends on 1)

The component according to claim 1, wherein the quartz glass shows absorption of less than 0.5/cm for UV radiation of a wavelength of 163 nm.

### Claim 15

A method for producing synthetic quartz glass with a predetermined hydroxyl group content, comprising the following method steps:
(a) producing a porous SiO2 soot body by flame hydrolysis or oxidation of a silicon-containing start compound and by layerwise deposition of SiO2 particles on a carrier,
(b) subjecting the soot body to a dehydration treatment in a drying atmosphere so as to remove hydroxyl groups, so that the soot body has a mean hydroxyl group content of less than 60 wt ppm,
(c) vitrifying the SiO2 soot body so as to obtain a body made from the synthetic quartz glass, and
(d) wherein the quartz glass has a mean hydrogen content set to a value in the range of less than 2×1017 molecules/cm3,
wherein the soot body is nitrided during or after the dehydration treatment using a nitrogen-containing reaction gas, and the mean hydrogen content of the quartz glass is set to a value in the range of 5×1015 molecules/cm3 to 1×1017 molecules/cm3.

### Claim 16 (depends on 15)

The method according to claim 15, wherein nitriding is carried out during the dehydration treatment according to method step (b).

### Claim 17 (depends on 15)

The method according to claim 15, wherein nitriding is carried out between the dehydration treatment according to method step (b) and vitrification according to method step (c).

### Claim 18 (depends on 15)

The method according to claim 15, wherein nitriding is carried out during the vitrifying according to method step (c).

### Claim 19 (depends on 15)

The method according to claim 15, wherein the nitrogen-containing reaction gas is NH3, ND3, NO2 or N2O.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the doping treatment is carried out using NH3 or ND3 at a low nitriding temperature in a range between 800° C. and 1250° C.

### Claim 21 (depends on 15)

The method according to claim 15, wherein chlorine is used during the dehydration treatment according to method step (b).

### Claim 22 (depends on 15)

The method according to claim 15, wherein nitriding is carried out under an overpressure of the nitrogen-containing reaction gas.

### Claim 23 (depends on 15)

The method according to claim 15, wherein at the beginning of the dehydration treatment the soot body shows a density of not more than 30% of the density of quartz glass.

### Claim 24 (depends on 2)

The component according to claim 2, wherein the nitrogen content of the quartz glass is at least 30 wtppm.

### Claim 25 (depends on 4)

The component according to claim 4, wherein the content of boron oxide is in a range between 30 wtppm and 60 wtppm.

### Claim 26 (depends on 9)

The component according to claim 9, wherein the mean content of aluminum oxide is at least 20 wtppm.

### Claim 27 (depends on 1)

The component according to claim 1, wherein the quartz glass has a content of hydroxyl groups of less than 25 wtppm.

### Claim 28 (depends on 1)

The component according to claim 1, wherein the quartz glass has a content of hydroxyl groups of less than 15 wtppm.

### Claim 29 (depends on 19)

The method according to claim 19, wherein the doping treatment is carried out using NH3 or ND3 at a low nitriding temperature in the range below 1200° C.