# US 2010/0087324 A1 · Procedure of densifying filaments for a superconductive wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0087324 A1
- Document ID: US20100087324A1
- Status: Published application
- Kind: A1
- Application number: 12/585,914
- Filed: 2009-09-29
- Published: 2010-04-08
- Earliest claimed: 2008-10-06
- Assignees: Bruker BioSpin GmbH
- Inventors: René Flüekiger
- Web page: https://patentgrep.com/patent/US20100087324A1

## CPC

- H10N 60/01: Manufacture or treatment
- H10N 60/0184: {of devices comprising intermetallic compounds of type A-15, e.g. Nb3Sn}
- H10N 60/0212: {of devices comprising molybdenum chalcogenides}
- H10N 60/0856: {of devices comprising metal borides, e.g. MgB2}
- Y10T 29/49014: Superconductor
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing a superconductive wire, whereby an elongated intermediate element is formed out of an initial element in a deformation step and whereby the superconductive filaments are formed by a final reaction heat treatment, is characterized in that prior to the final reaction heat treatment the filaments in the intermediate element are densified in one or more high pressure densification steps following up the deformation step, said densification steps comprising a simultaneous action of at least four hard surfaces perpendicular to the axis of the elongated intermediate element, building up high pressure P≧100 MPa on a part of the intermediate element having an axial length L. This leads to a substantial increase of the critical current density Jc, whereby the anisotropy factor F is be almost not affected thus enabling production of almost isotropic wires or tapes.

## Claims

### Claim 1

A method for producing a superconductive wire from an initial element, the completed superconductive wire having one or more superconductive filaments with a diameter between 2 μm and 5 mm which are enclosed in a metallic matrix, the superconducting wire also having at least one highly conductive ohmic element, the method comprising the steps of:
a) executing a deformation step in which the initial element is subjected to a sequence of swaging, drawing or rolling deformations to form an elongated intermediate element with polygonal cross section;
b) densifying, following step a), material of the filaments in said intermediate element in one or more high pressure densification steps, the densification steps effecting simultaneous action of at least 4 hard surfaces perpendicular to an axis of the elongated intermediate element, thereby exercising high pressure P≧100 MPa on a part of the intermediate element having an axial length L; and
c) forming, following step b), the superconductive filaments in a reaction heat treatment between 300° C. and 1200° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the high pressure densification steps are performed at temperatures between −100° C. and +200° C. or at room temperature.

### Claim 3 (depends on 1)

The method of claim 1, wherein the high pressure P in the high pressure densification steps is chosen in a range of 0.1 GPa≦P≦10 GPa or 1 GPa≦P≦3 GPa.

### Claim 4 (depends on 1)

The method of claim 1, wherein the reaction heat treatment following the high pressure densification steps is performed under a gas pressure up to 0.4 GPa.

### Claim 5 (depends on 1)

The method of claim 1, wherein the polygonal cross section of the elongated intermediate element has an area between 0.25 mm2 and 50 mm2 or between 2 mm2 and 15 mm2.

### Claim 6 (depends on 1)

The method of claim 1, wherein the elongated intermediate element is subjected to a repeated pressing and release cycle including several high pressure densification steps, wherein the hard surfaces are moved away after each high pressure densification step, thereby releasing the pressure on the intermediate element.

### Claim 7 (depends on 6)

The method of claim 6, wherein, after one or more high pressure densification steps, the intermediate element is subjected to a forward movement in an axial direction by a length L1, where L1<L, after which the hard surfaces are brought back to original radial positions thereof with respect to the intermediate element, followed by application of high pressure in a further high pressure densification step.

### Claim 8 (depends on 7)

The method of claim 7, wherein an overlapping region between two successive pressed lengths of the intermediate element is smaller than L/2, and a cycle consisting of densification, pressure release and forward movement is repeated up to a total length of the intermediate element.

### Claim 9 (depends on 7)

The method of claim 7, wherein a sequence of densification, pressure release and forward movement is synchronized, a number of pressing cycles varying between 1 and 100 per second or between 5 to 10 per second.

### Claim 10 (depends on 1)

The method of claim 1, wherein corners of the intermediate element are rounded off by a drawing step following the high pressure densification steps.

### Claim 11 (depends on 1)

The method of claim 1, wherein the superconductive filaments are separated from the matrix and from the conductive ohmic element by a protective metallic layer.

### Claim 12 (depends on 1)

The method of claim 1, wherein the filaments contain powder mixtures chosen from the group of Boron, Magnesium and one or more additives with a total Carbon content up to 20 wt. %, wherein a MgB2 phase is formed after an “in situ” reaction between 500° C. and 1000° C. or the filaments contain previously formed (=“ex situ”) MgB2 powder mixtures containing up to 20 wt. % Carbon, wherein the filaments are subjected to a sintering treatment at temperatures between 600° C. and 1000° C. and are separated from the metallic matrix, by a Nb,Ta, Ni or Ti barrier.

### Claim 13 (depends on 12)

The method of claim 12, wherein the metallic matrix comprises Cu.

### Claim 14 (depends on 1)

The method of claim 1, wherein the filaments contain powder mixtures of NbSn2 and one or more additives, a Nb3Sn phase being formed by a reaction at temperatures between 550° C. and 800° C. and being separated from the metallic matrix by a Nb barrier.

### Claim 15 (depends on 14)

The method of claim 14, wherein the filaments contain up to 10 wt. % Sn and Cu and the metallic matrix comprises Cu.

### Claim 16 (depends on 1)

The method of claim 1, wherein the filaments contain powder mixtures chosen from the group of Mo, Pb, Sn and S, a phase PbMo6S8 (=Chevrel phase) being formed by a reaction at temperatures between 800° C. and 1100° C. and being separated from the metallic matrix by a barrier chosen from the group of Mo, Nb and Ta.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metallic matrix comprises Cu.

### Claim 18 (depends on 1)

The method of claim 1, wherein filaments contain powder mixtures chosen from the group of As, Fe and oxides based on an earth alkaline (X1) and an alkaline element (X2), a phase X11-xX2xFe2As2 being formed by a heat treatment at temperatures between 800° C. and 1100° C. and being separated from the metallic matrix by a Nb or Ta barrier.

### Claim 19 (depends on 18)

The method of claim 18, wherein the metallic matrix comprises Cu.