Method for waste stabilisation and products obtained therefrom
OwnerTsen Meng TANG, Hsing Loong Tan +1inventors
InventorsTsen Meng TANG, Hsing Loong Tan, Danmei Wang
Life of this patent
Estimating the term…
Loading patent…
OwnerTsen Meng TANG, Hsing Loong Tan +1inventors
InventorsTsen Meng TANG, Hsing Loong Tan, Danmei Wang
Estimating the term…
A method is provided for heavy metal stabilisation comprising: mixing waste, comprising heavy metals, with molecular sieve with the proviso that carbon-based molecular sieve is excluded, and clay; and vitrifying the mixture. In particular, a method comprising the steps of: preparing a pre-stabilised mixture by mixing waste, comprising heavy metals, with the molecular sieve, and optionally other chemicals; mixing the pre-stabilised mixture with clay; and vitrifying the obtained mixture is provided. It also provides a product comprising heavy metals that have been stabilised into the structure of the clay-based ceramic matrix, wherein the product is a vitrified product of a mixture of at least waste, comprising heavy metals, molecular sieve (with the proviso that carbon-based molecular sieve is excluded) and clay.
A product comprising stabilised heavy metals, wherein the product is a vitrified product of a mixture of at least waste, comprising heavy metals, molecular sieve with the proviso that carbon-based molecular sieve is excluded, and clay, wherein the mixture is aged prior to vitrification.
A product comprising stabilised heavy metals, wherein the product is a vitrified product of a mixture of at least waste, comprising heavy metals, molecular sieve with the proviso that carbon-based molecular sieve is excluded, and clay, such that pH of the mixture is adjusted to 8.0-12.0 by adding Na2SiO3 and/or Na3PO4, wherein the mixture is aged prior to vitrification.
Dependencies are inferred from the claim text.