# US 2010/0075082 A1 · Barrier film and laminated material, container for wrapping and image display medium using the same, and manufacturing method for barrier film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0075082 A1
- Document ID: US20100075082A1
- Status: Published application
- Kind: A1
- Application number: 12/631,991
- Filed: 2009-12-07
- Published: 2010-03-25
- Earliest claimed: 2002-04-18
- Assignees: Dai Nippon Printing Co., Ltd.
- Inventors: Minoru KOMADA; Yoshihiro KISHIMOTO
- Web page: https://patentgrep.com/patent/US20100075082A1

## CPC

- C23C 14/10: Glass or silica
- B32B 27/00: Layered products comprising {a layer of} synthetic resin {(fibrous or filamentary layer made of a synthetic resin B32B5/02; particulate layer made of a synthetic resin B32B5/16; foamed layer made of a synthetic resin B32B5/18)}
- B32B 33/00: Layered products characterised by particular properties or particular surface features, e.g. particular surface coatings; Layered products designed for particular purposes not covered by another single class
- C23C 14/0676: {Oxynitrides}
- B32B 2307/7244: Oxygen barrier
- B32B 2553/00: Packaging equipment or accessories not otherwise provided for
- C09K 2323/051: Inorganic, e.g. glass or silicon oxide
- H10P 14/6329: {using physical ablation of a target, e.g. physical vapour deposition or pulsed laser deposition}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- Y10T 428/1334: Nonself-supporting tubular film or bag [e.g., pouch, envelope, packet, etc.]
- Y10T 428/1352: Polymer or resin containing [i.e., natural or synthetic]
- Y10T 428/265: 1 mil or less
- Y10T 428/28: Web or sheet containing structurally defined element or component and having an adhesive outermost layer
- Y10T 428/31667: Next to addition polymer from unsaturated monomers, or aldehyde or ketone condensation product
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An object of the present invention is to provide a barrier film having the extremely high barrier property and the better transparency, a method for manufacturing the same, and a laminated material, a container for wrapping and an image displaying medium using the barrier film. According to the present invention, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, wherein the barrier layer is a silicon oxide film having an atomic ratio in a range of Si:O:C=100:140 to 170:20 to 40, peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1060 to 1090 cm−1, a film density in a range of 2.6 to 2.8 g/cm3, and a distance between grains of 30 nm or shorter. Still more, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, has a composition wherein the barrier layer is a silicon oxi-nitride film, and the silicon oxi-nitride film has an atomic ratio in a range of Si:O:N:C=100:60 to 90:60 to 90:20 to 40, a maximum peak of infrared-ray absorption due to Si—O stretching vibration and Si—N stretching vibration is in a range of 820 to 930 cm−1, a film density is in a range of 2.9 to 3.2 g/cm3, and a distance between grains is 30 nm or shorter.

## Claims

### Claim 1

A barrier film provided with a barrier layer on at least one surface of a substrate film, wherein
the barrier layer is a silicon oxide film, and the silicon oxide film has an atomic ratio in a range of Si:O:C=100:140 to 170:20 to 40, peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1060 to 1090 cm−1, a film density in a range of 2.6 to 2.8 g/cm3, and a distance between grains of 30 nm or shorter.

### Claim 2 (depends on 1)

The barrier film according to claim 1, wherein the barrier layer is provided on the substrate film via a resin layer.

### Claim 3 (depends on 1)

The barrier film according to claim 1, wherein a resin layer is provided on the barrier layer.

### Claim 4 (depends on 1)

The barrier film according to claim 1, wherein an oxygen transmission rate thereof is 0.1 cc/m2/day·atm or less, and a water vapor transmission rate thereof is 0.1 g/m2/day or less.

### Claim 5 (depends on 1)

A laminated material, wherein a heat sealable resin layer is provided on at least one surface of the barrier film according to claim 1.

### Claim 6 (depends on 5)

A container for wrapping, wherein the container is obtained by making a bag or a can by heat anastomosing the heat sealable resin layer using the laminated material according to claim 5.

### Claim 7 (depends on 1)

A laminated material, wherein a conductive layer is provided on at least one surface of the barrier film according to claim 1.

### Claim 8 (depends on 7)

An image displaying medium, wherein an image displaying layer is provided on the conductive layer using the laminated material according to claim 7 as the substrate.

### Claim 9

A method for manufacturing a barrier film, comprising forming, as a barrier layer, a silicon oxide film having an atomic ratio in a range of Si:O:C=100:140 to 170:20 to 40, peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1060 to 1090 cm−1, a film density in a range of 2.6 to 2.8 g/cm3 and a distance between grains of 30 nm or shorter, on a substrate film, using either of silicon having a sintered density of 80% or higher or silicon monoxide having a sintered density of 80% or higher as a target, in the presence of an oxygen gas by a sputtering method.

### Claim 10 (depends on 9)

The method for manufacturing a barrier film according to claim 9, wherein the sputtering method is any of a RF sputtering method and a dual magnetron sputtering method.

### Claim 11 (depends on 9)

The method for manufacturing a barrier film according to claim 9, wherein a resin layer is provided on the substrate film in advance, and the barrier layer is formed on the resin layer.

### Claim 12

A barrier film provided with a barrier layer on at least one surface of a substrate film, wherein
the barrier layer is a silicon oxi-nitride film, and the silicon oxi-nitride film has an atomic ratio in a range of Si:O:N:C=100:60 to 90:60 to 90:20 to 40, a maximum peak of infrared-ray absorption due to Si—O stretching vibration and Si—N stretching vibration is in a range of 820 to 930 cm−1, a film density in a range of 2.9 to 3.2 g/cm3, and a distance between grains of 30 nm or shorter.

### Claim 13 (depends on 12)

The barrier film according to claim 12, wherein the barrier layer is provided on the substrate film via a resin layer.

### Claim 14 (depends on 12)

The barrier film according to claim 12, wherein a resin layer is provided on the barrier layer.

### Claim 15 (depends on 12)

The barrier film according to claim 12, wherein an oxygen transmission rate thereof is 0.1 cc/m2/day·atm or less, and a water vapor transmission rate thereof is 0.1 g/m2/day or less.

### Claim 16 (depends on 12)

A laminated material, wherein a heat sealable resin layer is provided on at least one surface of the barrier film according to claim 12.

### Claim 17 (depends on 16)

A container for wrapping, wherein the container is obtained by making a bag or a can by heat anastomosing the heat sealable resin layer using the laminated material according to claim 16.

### Claim 18 (depends on 12)

A laminated material, wherein a conductive layer is provided on at least one surface of the barrier film according to claim 12.

### Claim 19 (depends on 18)

An image displaying medium, wherein an image displaying layer is provided on the conductive layer using the laminated material according to claim 18 as the substrate.