# US 2010/0075053 A1 · Non-electrolytic method for metallizing a substrate by the reduction of metallic salt(s) and the spraying of aerosol(s)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0075053 A1
- Document ID: US20100075053A1
- Status: Published application
- Kind: A1
- Application number: 12/515,461
- Filed: 2007-11-26
- Published: 2010-03-25
- Earliest claimed: 2006-11-24
- Assignees: Jet Metal Technologies
- Inventors: Samuel Stremsdoerfer
- Web page: https://patentgrep.com/patent/US20100075053A1

## CPC

- C23C 18/40: using reducing agents
- C23C 18/1617: {Purification and regeneration of coating baths}
- C23C 18/1619: {Apparatus for electroless plating}
- C23C 18/1658: {with two steps starting with metal deposition followed by addition of reducing agent}
- C23C 18/166: {with two steps starting with addition of reducing agent followed by metal deposition}
- C23C 18/1675: {Process conditions}
- C23C 18/1683: {Control of electrolyte composition, e.g. measurement, adjustment (regeneration of bath C23C18/1617)}
- C23C 18/34: using reducing agents
- Y02T 50/60: Efficient propulsion technologies, e.g. for aircraft
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The invention relates to a non-electrolytic method for metallizing a substrate by projecting an aerosol containing a solution of an oxidant metallic cation and of a reducing agent; said method comprising a step of—a—wetting the substrate; starting to project a metallisation according to a succession of projecting phases alternating with relaxing phases: (i) by adjusting the duration Dp of the projection phases and the duration Dr of the relaxing phases from a metallisation constant k intrinsic for each metal; and (ii) by adjusting the projection flow-rate. The metallisation projection is carried out dynamically by displacing projection means relative to the substrate in order to carry out a periodical scanning, wherein Dp correspond to the duration during which the surface unit in question is submitted to the continuous projection of the aerosol and Dr corresponds to the duration during which the part is not submitted to projection.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

Improved non-electrolytic method for metallizing at least part of the surface of a substrate (hereafter called the surface to be metallized) by spraying, using suitable means, of at least one aqueous and/or organic aerosol containing at least one metal in cationic (oxidizing) form and at least one reducing agent, capable of converting the metallic cation to metal, of the type of those essentially consisting of:
—b—carrying out the metallization spraying according to a succession of at least two spraying phases, alternating with relaxation phases: (i) setting the duration Dp of the spraying phases between 10−2 and 5 s, for the same unit area, and the duration Dr of the relaxation phases between 10−2 and 10 s, for the same unit area, the durations Dp and Dr of these spraying and relaxation phases being identical to or different from each other, (ii) and adjusting the spraying flow rate(s), such that the Ox/Red electronic ratio is comprised between 0.01 and 15, and thus allows the formation of a metallic film which is chemically adherent to the substrate;—c—interrupting the spraying as soon as the intended level of metal deposition is reached, wherein the improvement consists in that it is envisaged:
to implement at least one preliminary stage—ap—of wetting the substrate which involves bringing the latter into contact with at least one wetting fluid, so as to form a fluid film on at least part of its surface;
and, following the wetting—ap—, to commence the spraying according to stage—b—at the latest 60 s, after the end of the wetting.

### Claim 18 (depends on 17)

Method according to claim 17, comprising a step —a—consisting in sensitizing and/or activating the surface to be metallized.

### Claim 19 (depends on 17)

Method according to claim 17, wherein the durations Dp and Dr of spraying and relaxation respectively are defined on the basis of a constant k of metallization intrinsic to each metal such that k=Dp+Dr, comprised between 10−1 and 13 S.

### Claim 20 (depends on 17)

Method according to claim 17, wherein:
at least part of the metallization spraying is carried out dynamically by moving the spraying means with respect to the substrate so as to carry out a periodic sweep of at least 80%, of the surface to be metallized;
for a given unit area comprised within the sweep zone:
the spraying phase has a duration Dp corresponding to the duration for which the unit area considered is subjected to the spraying of the aerosol,
the relaxation phase which follows this spraying phase has a duration Dr corresponding to the duration of the remainder of the surface to be metallized by the spraying means,
the movement of the spraying means is defined such that:
said spraying means are moved along a path TOA between an point of origin (O) and an arrival point (A) at a spraying movement speed VOA,
as soon as the spraying means reach the point (A), they return to the point (O) at a speed VAO of movement without spraying along a path TAO;
VAO being calculated by taking into account the distance between (A) and (O) and VOA, so that the duration Dr of the relaxation phase of each unit area of the surface to be metallized swept by the spraying means as well as the constant k intrinsic to the deposited metal is as defined above,
this calculation preferably being carried out by a processing and control unit UCC (preferably a microcomputer) controlling the spraying means and a movement system for said spraying means.

### Claim 21 (depends on 20)

Method according to claim 20, wherein the substrate is rotated, during at least part of the metallization spraying.

### Claim 22 (depends on 17)

Method according to claim 17, wherein the improvement has the following characteristics:
at least part of the metallization spraying is carried out dynamically by moving the spraying means with respect to the substrate and/or by moving the substrate with respect to the spraying means so as to carry out a periodic sweep of at least 80%, of the surface to be metallized;
for a given unit area and comprised within the sweep zone:
the spraying phase has a duration Dp corresponding to the duration during which the unit area considered is subjected to the spraying of the aerosol,
the relaxation phase which follows this spraying phase has a duration Dr corresponding to the duration of the sweep of the remainder of the surface to be metallized by the spraying means.

### Claim 23 (depends on 22)

Method according to claim 22, wherein the movement of the substrate with respect to the spraying means is a rotation.

### Claim 24 (depends on 17)

Method according to claim 17, wherein the duration Dr of the relaxation phase corresponds to the duration for which the unit area considered is not subjected to the spraying of the aerosol.

### Claim 25 (depends on 17)

Method according to claim 17, wherein that the temperature of the metallization enclosure is controlled.

### Claim 26 (depends on 17)

Method according to claim 17, wherein that the preliminary wetting stage—ap—is carried out by spraying of the vapours of wetting liquid and/or of an aerosol of wetting liquid and/or by immersion in a bath of wetting liquid, said wetting liquid being optionally heated.

### Claim 27 (depends on 17)

Method according to claim 17, wherein the wetting liquid is chosen from the group comprising deionized or non-deionized water, an alcoholic solution comprising at least one alcohol and mixtures thereof.

### Claim 28 (depends on 17)

Method according to claim 17, wherein stage b is cyclic, each cycle comprising a spraying phase and a relaxation phase, corresponding to the spraying means moving from (O) to (A) and back and in that the total number of N cycles implemented is chosen as a function of the level of deposition of metal finally sought and the level of deposition of metal obtained in each cycle, this total number of N cycles being comprised between 2 and 5000.

### Claim 29 (depends on 17)

Method according to claim 17, wherein that the substrate is rotated during stage—b—, at a speed comprised between 1 and 30 rpm.

### Claim 30 (depends on 17)

Method according to claim 17, wherein the path TAO is straight and direct.

### Claim 31 (depends on 28)

Method according to claim 28, wherein the formula for calculating VAO is as follows: VAO=AO/[k−(OA/VOA)].

### Claim 32 (depends on 28)

Method according to claim 28, wherein VOA is comprised between 0.01 and 20 m/s.

### Claim 33 (depends on 17)

Method according to claim 17, wherein:
the sludges which are produced at the end of the metallization and which contain metal oxides are recovered;
these sludges are filtered;
the retentate is dissolved using at least one strong acid;
the pH of the solution of retentate in the strong acid is increased so as to precipitate the metal hydroxide or successively the different metal hydroxides corresponding to the metal or metals used in the metallization;
the metal hydroxide precipitate(s) are collected separately.

### Claim 34 (depends on 17)

Method according to claim 17, wherein this or these metal hydroxide(s) are recycled in the metallization method.

### Claim 35 (depends on 17)

Device for the implementation of the method according to claim 17, comprising:
a holder for the substrate to be metallized, optionally equipped with means for rotation of the substrate;
an organ for preliminary wetting the substrate;
a sprayer of the metal in cationic form and reducing agent;
a system for movement of the spraying means, or even of the means of wetting and/or of the means of rinsing;
and at least one processing and control unit UCC controlling the spraying means and the system for movement of said spraying means.

### Claim 36 (depends on 17)

Device for the implementation of the method according to claim 17, comprising an organ for wetting by spraying of the liquid, in that these wetting organ is movable and this movement of the wetting organ is also controlled by a processing and control unit UCC.