# US 2010/0074974 A1 · Metal-rich siliceous compositions and methods of producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0074974 A1
- Document ID: US20100074974A1
- Status: Published application
- Kind: A1
- Application number: 12/628,472
- Filed: 2009-12-01
- Published: 2010-03-25
- Earliest claimed: 2006-11-08
- Assignees: Nalco Company
- Inventors: Brian T. Holland
- Web page: https://patentgrep.com/patent/US20100074974A1

## CPC

- B01J 20/103: {comprising silica}
- B01J 20/16: Alumino-silicates (B01J20/12 takes precedence)
- B01J 20/3236: {containing metal, other than zeolites, e.g. oxides, hydroxides, sulphides or salts}
- B01J 23/44: Palladium
- B01J 23/66: Silver or gold
- B01J 23/70: of the iron group metals or copper
- B01J 27/13: Platinum group metals
- B01J 29/049: {Pillared clays}
- B01J 35/23: in a colloidal state
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/45: Nanoparticles
- B01J 37/031: {Precipitation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C01B 33/141: Preparation of hydrosols or aqueous dispersions
- C01B 33/151: by progressively adding a sol to a different sol, i.e. "build-up" of particles using a "heel"
- C01G 55/00: Compounds of ruthenium, rhodium, palladium, osmium, iridium, or platinum
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/12: Surface area
- C01P 2006/14: Pore volume
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A modified sol-gel method to create metal-rich siliceous material, such as colloidal silica or aluminosilicate particles is disclosed. Initially, the metal salt of choice is added to a silicic acid solution or a silicic acid solution containing aluminum salt. The aluminum is added to vary the metal-support interaction as it forms Al—O—Si linkages within the silica matrix. Besides aluminum, other metals can be added that form M—O—Si (M=Ti, B, etc.) linkages, which do not become reduced when treated with a reducing agent. Once the metal, silicic acid and/or aluminum salt is generated, it is subjected to colloidal growth by addition to a basic heel. Upon colloidal synthesis, the metal salt containing colloidal particle is left as is to maximize colloidal stability or is reduced with hydrazine to produce the zero valence metal-containing colloidal particle. Keeping a particle colloidal before use may be an effective method of forming a catalyst material as it can be easily spray-dried or mixed with other materials for extruded catalyst particles.

## Claims

### Claim 1

A method of preparing a metal-rich siliceous material, said method comprising:
a) mixing one or more salts of one or more metals with a silicic acid solution to form a blend, said metals selected from the group consisting of: palladium, platinum, iron, gold, aluminum, copper, nickel, iron, titanium, and combinations thereof;
b) adding the blend to a basic heel solution to form colloidal silica particles in a suspension, wherein one or more of the colloidal silica particles includes incorporated metal particles;
c) optionally concentrating the suspension;
d) reducing the incorporated metal particles with a reducing agent to form a product; and
e) optionally further processing the colloidal silica particles or the product.

### Claim 2 (depends on 1)

The method of claim 1, including deionizing a sodium silicate solution to prepare the silicic acid solution.

### Claim 3 (depends on 1)

The method of claim 1, including combining aluminum chlorohydrate with the silicic acid solution prior to mixing one or more salts of one or more metals with the silicic acid solution to form the blend.

### Claim 4 (depends on 1)

The method of claim 1, including one or more salts of one or more metals selected from the group consisting of: palladium acetate; gold chloride; aluminum chlorohydrate; copper chloride; iron trinitrate; nickel nitrate; cobalt chloride; and combinations thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the basic heel solution includes one or more bases selected from the group consisting of: sodium hydroxide; lithium hydroxide; potassium hydroxide; ammonium hydroxide; primary amines; secondary amines; tertiary amines; quaternary amines; quaternary compounds; and combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, including adding the blend to the basic heel solution at a controlled rate to control colloidal silica particle size from about 1 nanometers to about 250 nanometers, said size depending on the controlled rate.

### Claim 7 (depends on 1)

The method of claim 1, including adding the blend to the basic heel solution at a controlled rate to control colloidal silica particle size from about 4 nanometers to about 150 nanometers.

### Claim 8 (depends on 1)

The method of claim 1, including heating the basic heel solution.

### Claim 9 (depends on 1)

The method of claim 1, including heating the basic heel solution from about 60° C. to about 90° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the reducing agent is selected from the group consisting of: hydrazine and hydrogen gas.

### Claim 11 (depends on 1)

The method of claim 1, wherein the incorporated metal particles are essentially homogenously dispersed within the colloidal silica particles.

### Claim 12 (depends on 1)

The method of claim 1, wherein further processing the colloidal silica particles or the product includes using one or more processes selected from the group consisting of: ultra-filtration, deionization, heating, drying, concentrating, surface functionalization, and combinations thereof.

### Claim 13 (depends on 1)

The method of claim 1, including using the colloidal silica particles or the product in an industrial application selected from the group consisting of: dental applications; protein separation; molecular sieves; nanoporous membranes; wave guides; photonic crystals; refractory applications; clarification of wine and juice; chemical mechanical planarization of semiconductor and disk drive components; catalysts; catalyst supports; retention and drainage aids in papermaking; fillers; surface coatings; ceramic materials; investment casting binders; flattening agents; proppants; cosmetic formulations; and polishing abrasives.

### Claim 14

A metal-rich siliceous composition comprising a plurality of settled silica particles produced from a mixture of a silicic acid solution and one or more salts of one or more reduced metals, wherein from about 10 weight percent to about 50 weight percent metal is associated with the colloidal silica particles, based on total solids.

### Claim 15

A metal-rich siliceous composition comprising a plurality of colloidal silica particles having an average diameter from about 1 to about 250 nanometers and which are produced from a mixture of a silicic acid solution and one or more salts of one or more reduced metals, wherein up to about 10 weight percent metal is associated with the colloidal silica particles, based on total solids.

### Claim 16 (depends on 15)

The metal-rich siliceous composition of claim 15, including a plurality of different reduced metals associated with the colloidal silica particles.

### Claim 17 (depends on 15)

The metal-rich siliceous composition of claim 15, wherein the reduced metal is selected from the group consisting of: alkali metals, alkaline earth metals, first row transition metals, second row transition metals, lanthanides, and combinations thereof.

### Claim 18 (depends on 15)

The metal-rich siliceous composition of claim 15, wherein the colloidal silica particles include closely-packed and dried colloidal silica particles.