# US 2010/0074835 A1 · Production of Nano-Structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0074835 A1
- Document ID: US20100074835A1
- Status: Published application
- Kind: A1
- Application number: 11/422,914
- Filed: 2006-06-08
- Published: 2010-03-25
- Earliest claimed: 2006-06-08
- Assignees: Directa Plus S.p.A.
- Inventors: Robert A. Mercuri
- Web page: https://patentgrep.com/patent/US20100074835A1

## CPC

- C01B 32/22: Intercalation
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 32/154: Preparation
- C01B 32/16: Preparation
- C01B 32/19: by exfoliation
- Y10S 977/712: formed from plural layers of nanosized material, e.g. stacked structures
- Y10S 977/775: Nanosized powder or flake, e.g. nanosized catalyst
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A process for the production of nano-structures is presented, involving providing a graphite flake comprising graphene layers; intercalating the graphite flake to form a graphite intercalation compound exhibiting Stage I, II or III intercalation; and exfoliating the graphite intercalation compound under conditions such that a plurality of individual graphene layers are separated from the graphite intercalation compound.

## Claims

### Claim 1

A process for the production of structures which are, on average, no greater than about 1000 nanometers in at least one dimension, comprising providing a graphite flake comprising graphene layers; intercalating the graphite flake to form a graphite intercalation compound exhibiting Stage I, II or III intercalation; and exfoliating the graphite intercalation compound by exposing the graphite intercalation compound to a temperature of at least about 1300° C. such that a plurality of individual graphene layers are separated from the graphite intercalation compound, wherein the graphite intercalation compound is brought from a temperature at which it is stable to a temperature of at least about 1300° C. within a period of no more than about 1 second.

### Claim 2 (depends on 1)

The process of claim 1, wherein the graphite flake is intercalated with an intercalant comprising formic acid, acetic acid, water, or combinations thereof.

### Claim 3 (depends on 1)

The process of claim 1, wherein the graphite intercalation compound is exposed to a supercritical fluid prior to exfoliation.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

The process of claim 1, wherein the graphite intercalation compound is exposed to a temperature of at least about 1450° C.

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The process of claim 1, wherein exfoliation is accomplished by feeding the graphite intercalation compound into an inert gas plasma or directly into an arc.

### Claim 8 (depends on 7)

The process of claim 7, wherein exfoliation occurs in a reducing gas environment.

### Claim 9 (depends on 8)

The process of claim 8, wherein exfoliation occurs in a hydrogen environment.

### Claim 10 (depends on 1)

The process of claim 1, wherein the graphite intercalation compound is exfoliated by being continuously extruded as a rod through a cooled nozzle which opposes a graphite electrode, wherein the extruded graphite intercalation compound and the graphite electrode form a pair between which an arc is struck to rapidly heat the graphite intercalation compound.

### Claim 11 (depends on 10)

The process of claim 10, wherein a vacuum is drawn to accelerate exfoliation and direct the extruded stream of exfoliated graphite intercalation compound.

### Claim 12 (depends on 1)

The process of claim 1, wherein a plurality of individual graphene layers each spontaneously form a nano-tube or a Buckminster fullerene.

### Claim 13 (depends on 1)

The process of claim 1, wherein the graphite intercalation compound is brought from a temperature at which it is stable to a temperature substantially above its decomposition temperature within a period of no more than about 0.5 second.