US 2010/0072060 A1Published application
Biomedical Electrode and Method of Formation Thereof
AssigneeTyco Healthcare Group LP
InventorWarren Copp-Howland
Life of this patent
Estimating the term…
Abstract
The present disclosure relates to biomedical electrodes incorporating hydrophobic material and methods of formation thereof.
Claims35
A biomedical electrode, the electrode comprising:
- a conductive member defining a first side and a second side;
- a conductive composition disposed on the first side of the conductive member, wherein the conductive composition includes a therapeutically effective quantity of hydrophobic medicament;
- and
- an electrical lead in electrical communication with the conductive member.
1 more element
A method of forming an electrode, comprising the steps of:
- providing a conductive member having a first side and a second side;
- providing a conductive composition on the first side of the conductive member, wherein the conductive composition includes a therapeutically effective quantity of a hydrophobic medicament associated therewith;
- providing a backing member on the second side of the conductive member;
- and
- providing an electrical lead in electrical communication with at least one of the conductive member and the conductive composition.
2 more elements
A method of forming a biocompatible conductive composition, comprising the step of:
- weighing out a solution of sodium 2-(acrylamido)-2-methylpropanesulfonate (NaAMPS) and placing the NaAMPS is a container;
- weighing out and adding a cross-linker to the NaAMPS to form a monomer solution;
- weighing out and adding an acrylic acid to the monomer solution;
- weighing out and adding a salt to the monomer solution;
- mixing for approximately 10 minutes;
- weighing out and adding glycerol to the monomer solution;
- weighing out and adding silica to the monomer solution;
- adding sodium hydroxide, drop wise, to the monomer solution to bring the pH of the monomer solution up to about 3.50±0.05;
- weighing out a quantity of Surfactant and vitamin E acetate to the monomer solution;
- adding the Surfactant and vitamin E acetate to the monomer solution;
- weighing out and adding a catalyst to the monomer solution;
- mixing the monomer solution for approximately 30 minutes;
- coating the monomer solution on a release liner;
- and
- irradiating the coating of the monomer solution under a Xenon arc UV lamp for approximately 25 seconds.
12 more elements
The method according to claim 24, wherein approximately 45.416 grams of NaAMPS is provided.
Dependencies are inferred from the claim text.