# US 2010/0071597 A1 · Fly ash based lightweight cementitious composition with high compressive strength and fast set

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0071597 A1
- Document ID: US20100071597A1
- Status: Published application
- Kind: A1
- Application number: 12/237,634
- Filed: 2008-09-25
- Published: 2010-03-25
- Earliest claimed: 2008-09-25
- Assignees: United States Gypsum Company
- Inventors: Marianela PEREZ-PENA
- Web page: https://patentgrep.com/patent/US20100071597A1

## CPC

- C04B 14/022: {Carbon}
- C04B 28/021: {Ash cements, e.g. fly ash cements (fly ash as filler C04B18/08); Cements based on incineration residues, e.g. alkali-activated slags from waste incineration (alkali-activated combustion residues as such C04B7/243; mixtures of the lime-pozzuolane type C04B28/18); Kiln dust cements}
- C04B 28/10: Lime cements or magnesium oxide cements
- C04B 28/14: containing calcium sulfate cements {(gypsum-paper plates E04C)}
- C04B 2111/40: Porous or lightweight materials
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method of making a rapid setting lightweight cementitious composition with improved compressive strength for products such as boards is disclosed. The method mixes fly ash, alkali metal salt of citric acid and lightweight aggregate with water. Compositions which include fly ash, alkali metal salts of citric acid and lightweight aggregate are also disclosed.

## Claims

### Claim 1

A method of providing a lightweight cementitious mixture having improved compressive strength and water durability comprising:
mixing
water,
reactive powder,
an alkali metal salt of citric acid, and
lightweight aggregate
wherein the weight ratio of water to reactive powder is about 0.17 to 0.35:1.0, the reactive powder comprising 75 to 100 wt. % fly ash, and 0 to 25 wt. % hydraulic cement and gypsum.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reactive powder comprises 88.5 to 100% fly ash, no hydraulic cement and no gypsum, based upon weight of the reactive powder.

### Claim 3 (depends on 1)

The method of claim 1, wherein the initial temperature of the mixture is about 24° C. to 41° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the reactive powder comprises 88.5 to 100 wt % class C fly ash.

### Claim 5 (depends on 1)

The method of claim 1, wherein the reactive powder contains 10 to 40 wt. % lime.

### Claim 6 (depends on 1)

The method of claim 1, wherein the mixture has a compressive strength measured after 3 hours of between 2000 psi to 5000 psi (13.8 MPa to 34.5 MPa).

### Claim 7 (depends on 1)

The method of claim 1, wherein the alkali metal salt of citric acid is at least one member of the group consisting of potassium citrates, sodium citrates, and mixture thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the alkali metal salt of citric acid is in an amount of about 1.5 to 6 wt. % based on the weight of the cementitious reactive powder.

### Claim 9 (depends on 1)

The method of claim 1, wherein the alkali metal salt of citric acid is in an amount of about 1.5 to 4 wt. % based on the weight of the cementitious reactive powder.

### Claim 10 (depends on 1)

The method of claim 1, wherein the alkali metal salt of citric acid is in an amount of about 2 to 3.5 wt. % based on the weight of the cementitious reactive powder.

### Claim 11 (depends on 1)

The method of claim 1, wherein the cementitious reactive powder further comprises a non-fly-ash mineral additive.

### Claim 12 (depends on 1)

The method of claim 1, wherein the cementitious reactive powder further comprises silica fume.

### Claim 13 (depends on 1)

The method of claim 1, wherein the cementitious reactive powder and water are present in a weight ratio of about 0.20-0.23:1 part by weight water to reactive powder.

### Claim 14 (depends on 1)

The method of claim 1, further comprising admixing at least one member of the group consisting of air-entraining agent, and secondary inorganic set accelerator, to the mixture.

### Claim 15 (depends on 1)

The method of claim 1, wherein setting of the mixture is achieved 4 to 6 minutes after forming the mixture.

### Claim 16

A composition for preparing a lightweight cement board comprising a mixture of:
cementitious reactive powder;
an alkali metal salt of citric acid as an accelerator for the reactive powder;
lightweight aggregate, and
water,
wherein the ratio of water to cementitious reactive powder solids in the mixture is about 0.17 to 0.35:1,
the reactive powder comprising 75 to 100 wt. % fly ash, and 0 to 25 wt. % hydraulic cement and gypsum.

### Claim 17 (depends on 16)

The composition of claim 16, wherein the mixture comprises about 1.5 to 6.0 wt. %, based upon the weight of cementitious powder, of at least one alkali metal salt of citric acid selected from the group consisting of sodium citrates, potassium citrates and mixtures thereof.

### Claim 18 (depends on 16)

The composition of claim 16, wherein the mixture comprises about 1.5 to 4.0 wt. %, based upon the weight of cementitious powder, of at least one alkali metal salt of citric acid selected from the group consisting of sodium citrates, potassium citrates and mixtures thereof.

### Claim 19 (depends on 16)

The composition of claim 16, wherein the mixture comprises about 2.0 to 3.5 wt. % sodium citrate based on the weight of the cementitious reactive powder.

### Claim 20 (depends on 16)

The composition of claim 16, wherein the cementitious reactive powder comprises 88.5 to 100 wt % class C fly ash and optionally a silica fume.