# US 2010/0071579 A1 · Frangible powdered iron projectiles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0071579 A1
- Document ID: US20100071579A1
- Status: Published application
- Kind: A1
- Application number: 12/400,857
- Filed: 2009-03-10
- Published: 2010-03-25
- Earliest claimed: 2004-11-23
- Assignees: Precision Ammunition, LLC
- Inventors: Daniel L. Powers, JR.
- Web page: https://patentgrep.com/patent/US20100071579A1

## CPC

- F42B 12/72: characterised by the material (heat treatment for explosive shells C21D9/16)
- F42B 8/12: Projectiles or missiles (F42B10/48, F42B12/36, F42B19/36 take precedence)
- F42B 33/00: Manufacture of ammunition; Dismantling of ammunition; Apparatus therefor (F42B5/188 takes precedence; manufacturing processes for hollow charges F42B1/036; manufacture of blasting cartridge initiators F42B3/195)
- F42B: EXPLOSIVE CHARGES, e.g. FOR BLASTING, FIREWORKS, AMMUNITION (explosive compositions C06B; fuzes F42C; blasting F42D)

## Abstract

Frangible projectiles for firearms and processes for making such projectiles are disclosed. The projectiles include a sintered, compacted mixture of powdered iron particles with other particles, including powdered copper particles and optionally powdered tin particles. The disclosed projectiles produce a similar feel and mimic the ballistic properties of lead projectiles of similar size and caliber, yet readily break-up upon impact with a hard surface in order to minimize ricochet or splatter. The disclosed projectiles and processes for making the projectiles meet the need for inexpensive, lead-free frangible projectiles.

## Claims

### Claim 1

A lead-free, frangible, sintered firearm projectile, comprising:
a projectile core formed from an admixture of cold compacted metal powder, consisting essentially of:
powdered iron particles;
powdered copper particles; and
powdered tin particles;
wherein the powdered iron particles comprise at least 70% by volume of metal particles in the admixture, the admixture is lead-free, and wherein the projectile core is sintered at a temperature in the range of 850° F. to 1450° F. (454° to 788° C.).

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The firearm projectile of claim 1, wherein the powdered iron particles, powdered copper particles and powdered tin particles in the admixture are present in volumetric percentages of 70% powdered iron particles, volume, 20% powdered copper particles, and 10% powdered tin particles.

### Claim 4 (depends on 1)

The firearm projectile of claim 1, further comprising a lubricant when admixing the metal powders.

### Claim 5 (depends on 1)

The firearm projectile of claim 1, further comprising a silicone solution impregnated into or onto the projectile core as a seal for the projectile core.

### Claim 6 (depends on 1)

The firearm projectile of claim 1, further comprising a metal solution coated onto the projectile core as a seal for the projectile core.

### Claim 7 (depends on 1)

The firearm projectile of claim 1, further comprising a jacket plated over the projectile core.