# US 2010/0063183 A1 · Intercalation agent free compositions useful to make nanocomposite polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0063183 A1
- Document ID: US20100063183A1
- Status: Published application
- Kind: A1
- Application number: 12/515,692
- Filed: 2007-11-16
- Published: 2010-03-11
- Earliest claimed: 2006-11-30
- Assignees: Dow Global Technologies LLC; Texas A&M University
- Inventors: Luyi Sun; Jae Boo Woong; Hung-Jue Sue; Maurice J. Marks; Richard F. Fibiger; Michael S. Paquette
- Web page: https://patentgrep.com/patent/US20100063183A1

## CPC

- C08J 3/2053: {the additives only being premixed with a liquid phase}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C08J 5/005: {Reinforced macromolecular compounds with nanosized materials, e.g. nanoparticles, nanofibres, nanotubes, nanowires, nanorods or nanolayered materials}
- C08J 2363/00: Characterised by the use of epoxy resins; Derivatives of epoxy resins
- Y10S 977/778: within specified host or matrix material, e.g. nanocomposite films
- Y10S 977/779: Possessing nanosized particles, powders, flakes, or clusters other than simple atomic impurity doping
- Y10S 977/783: Organic host/matrix, e.g. lipid
- Y10S 977/785: Electrically insulating host material
- Y10S 977/786: Fluidic host/matrix containing nanomaterials
- Y10S 977/787: Viscous fluid host/matrix containing nanomaterials
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A two step method for preparing a filler composition, the filler composition useful to prepare a nanocomposite polymer. The first step is to disperse a water dispersible filler material in a liquid comprising water to form a dispersion. The second step is to replace at least a portion of the water of the liquid with an organic solvent to form the filler composition, the water concentration of the liquid of the filler composition being less than six percent by weight, the average size of at least one dimension of the filler material being less than two hundred nanometers upon examination by transmission electron microscopy of a representative freeze dried sample of the dispersion of the first step. A nanocomposite polymer can be prepared by mixing the above-made filler composition with one or more polymer, polymer component, monomer or prepolymer to produce a polymer containing a filler having an average size of at least one dimension of the filler of less than two hundred nanometers upon examination by transmission electron microscopy of a representative sample of the polymer. In addition, an epoxy resin composition useful for making a cured epoxy nanocomposite polymer, the epoxy resin composition made by a two step process. The first step is to mix an epoxy resin with the filler composition to form an epoxy resin mixture. The second step is to remove organic solvent from the epoxy resin mixture to form the epoxy resin composition. And, a nanocomposite polymer, made by the step of mixing the filler composition with one or more polymer, polymer component, monomer or prepolymer to produce a polymer containing a filler having an average size of at least one dimension of the filler of less than two hundred nanometers upon examination by transmission electron microscopy of a representative sample of the polymer.

## Claims

### Claim 1

A method for preparing a filler composition, the filler composition useful to prepare a nanocomposite polymer, comprising the steps of: (a) dispersing a water dispersible filler material in a liquid comprising water to form a dispersion; (b) replacing at least a portion of the water of the liquid with an organic solvent so that the water concentration of the liquid is less than six percent by weight to form the filler composition, the average size of at least one dimension of the filler material being less than two hundred nanometers upon examination by transmission electron microscopy of a representative freeze dried sample of the dispersion of step (a).

### Claim 2 (depends on 1)

The method of claim 1, wherein the water dispersible filler material is a cation exchanging layered material wherein the cation exchanging capacity of the cation exchanging layered material is less than twenty percent exchanged with an organic cation.

### Claim 3 (depends on 2)

The method of claim 2, wherein the cation exchanging layered material is selected from the group consisting of natural or synthetic bentonite, montmorillonite, hectorite, fluorohectorite, saponite, stevensite, nontronite, sauconite, glauconite, vermiculite, chlorite, mica, hydromica, muscovite, biotite, phlogopite, illite, talc, pyrophillite, sepiolite, attapulgite, palygorskite, berthierine, serpentine, kaolinite, dickite, nacrite, halloysite, allophane, immogolite, hydrotalcite, pyroaurite, calcite, wollastonite and mixtures thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the water dispersible filler material is a cation exchanging layered material wherein the cation exchanging capacity of the cation exchanging layered material is essentially free of organic cation.

### Claim 5 (depends on 4)

The method of claim 4, wherein the cation exchanging layered material is selected from the group consisting of natural or synthetic bentonite, montmorillonite, hectorite, fluorohectorite, saponite, stevensite, nontronite, sauconite, glauconite, vermiculite, chlorite, mica, hydromica, muscovite, biotite, phlogopite, illite, talc, pyrophillite, sepiolite, attapulgite, palygorskite, berthierine, serpentine, kaolinite, dickite, nacrite, halloysite, allophane, immogolite, hydrotalcite, pyroaurite, calcite, wollastonite and mixtures thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the water concentration of the liquid is less than three percent by weight.

### Claim 7 (depends on 1)

The method of claim 1, wherein the water concentration of the liquid is less than one percent by weight.

### Claim 8 (depends on 1)

The method of claim 1, wherein the water concentration of the liquid is less than one half percent by weight.

### Claim 9 (depends on 1)

The method of claim 1, wherein the water concentration of the liquid is less than one tenth percent by weight.

### Claim 10 (depends on 1)

A method for preparing a nanocomposite polymer by the steps of: mixing the filler composition of claim 1 with one or more polymer, polymer component, monomer or prepolymer to produce a polymer containing a filler having an average size of at least one dimension of the filler of less than two hundred nanometers upon examination by transmission electron microscopy of a representative sample of the polymer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the monomer comprises an epoxy resin and wherein the filler composition is mixed with the epoxy resin to form a mixture, which mixture is then devolatilized to remove organic solvent and then cured to produce an epoxy nanocomposite polymer.

### Claim 12 (depends on 1)

An epoxy resin composition useful for making an epoxy nanocomposite polymer, the epoxy resin composition made by the steps of: (a) mixing an epoxy resin with the filler composition of claim 1 to form an epoxy resin mixture; and (b) removing organic solvent from the epoxy resin mixture to form the epoxy resin composition.

### Claim 13 (depends on 12)

A cured epoxy nanocomposite polymer made by the steps of: (a) mixing an epoxy resin curing agent with the epoxy resin composition of claim 12 to form an uncured epoxy nanocomposite polymer; and (b) curing the uncured epoxy nanocomposite polymer to form the epoxy nanocomposite polymer containing filler having an average size of at least one dimension of the filler of less than two hundred nanometers upon examination by transmission electron microscopy of a representative sample of the epoxy nanocomposite polymer.

### Claim 14 (depends on 1)

A nanocomposite polymer, made by the steps of: mixing the filler composition of claim 1 with one or more polymer, polymer component, monomer or prepolymer to produce a polymer containing a filler having an average size of at least one dimension of the filler of less than two hundred nanometers upon examination by transmission electron microscopy of a representative sample of the polymer.

### Claim 15 (depends on 14)

The nanocomposite polymer of claim 14, wherein the polymer is selected from the group consisting of polymers and copolymers of, polyolefins, polyamids, polyesters, polycarbonates, epoxies, styrenic polymers, polyurethanes, poly(alkyl)acrylates, polyacetals, polysulfides, polysulfones, polyethers, polyarylethers, polyketones, polyarylketones, polyimides, poly(vinyl halide)s, poly(vinylidene halide)s, poly(tetrafluoroethylene), polysiloxanes, cyanate polymers, maleimide polymers, vinylester resin polymers and mixtures thereof.

### Claim 16 (depends on 1)

An epoxy nanocomposite coating made by the steps of: (a) mixing an epoxy resin with the filler composition of claims 1, (b) mixing a curing agent and optionally a catalyst, accelerator, and processing additives, (c) applying the mixture to a substrate, and (d) allowing the solvents to evaporate and the epoxy resin to cure; and optionally exchanging and/or adding organic solvents after steps (a) or (b).

### Claim 17 (depends on 1)

The method of claim 1, further comprising the step of removing liquid from the filler composition to form a gel of the filler composition.

### Claim 18 (depends on 1, 17)

A filler composition made by the method of claim 1 or claim 17.