# US 2010/0062687 A1 · Cerium oxide powder for abrasive and cmp slurry comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0062687 A1
- Document ID: US20100062687A1
- Status: Published application
- Kind: A1
- Application number: 12/598,666
- Filed: 2008-04-30
- Published: 2010-03-11
- Earliest claimed: 2007-05-03
- Assignees: LG Chem, Ltd.
- Inventors: Myoung-Hwan Oh; Seung-Beom Cho; Jun-Seok Nho; Jong-Pil Kim; Jang-Yul Kim
- Web page: https://patentgrep.com/patent/US20100062687A1

## CPC

- C09K 3/1454: {Abrasive powders, suspensions and pastes for polishing}
- C01F 17/235: Cerium oxides or hydroxides
- C01F 17/247: Carbonates
- C09K 3/1463: {Aqueous liquid suspensions}
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/03: obtained by SEM
- C01P 2004/10: extending in one dimension, e.g. needle-like
- C01P 2004/20: extending in two dimensions, e.g. plate-like
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Disclosed are cerium oxide powder for an abrasive; CMP slurry including the same; and a shallow trench isolation (STI) process using the CMP slurry. At least two kinds of cerium oxides prepared by using cerium carbonates having different crystal structures are mixed in an appropriate ratio and used as an abrasive for CMP slurry, thereby adjusting required polishing properties of the CMP slurry. Also, in a disclosed method of preparing a cerium carbonate, the crystal structure of the cerium carbonate can be easily controlled. Based on the finding that in a cerium oxide for an abrasive, the kind of improved polishing property depends on the crystal structure of a cerium carbonate, at least one from among polishing properties, such as the polishing rate of a silicon oxide layer, the polishing rate of a silicon nitride layer, the polishing selectivity between the silicon oxide layer and the silicon nitride layer, and WIWNU, can be adjusted by using at least two kinds of cerium oxides selected from the group including (i) a cerium oxide prepared by using a lanthanite-(Ce) crystal structured cerium carbonate, (ii) a cerium oxide prepared by using an orthorhombic crystal structured cerium carbonate, and (iii) a cerium oxide prepared by using a hexagonal crystal structured cerium carbonate, as an abrasive for CMP slurry, and adjusting the mixing ratio of the cerium oxides.

## Claims

### Claim 1

CMP slurry comprising at least two kinds of cerium oxides selected from the group including (i) a cerium oxide prepared by using a lanthanite-(Ce) crystal structured cerium carbonate; (ii) a cerium oxide prepared by using an orthorhombic crystal structured cerium carbonate; and (iii) a cerium oxide prepared by using a hexagonal crystal structured cerium carbonate, as an abrasive.

### Claim 2 (depends on 1)

The CMP slurry as claimed in claim 1, wherein the cerium oxide prepared by using the lanthanite-(Ce) crystal structured cerium carbonate is used in an amount of 50 parts or more and less than 100 parts by weight per 100 parts by weight of cerium oxide powder for the abrasive.

### Claim 3 (depends on 1)

The CMP slurry as claimed in claim 1, wherein the cerium oxide prepared by using the orthorhombic crystal structured cerium carbonate is used in an amount of 50 parts or more and less than 100 parts by weight per 100 parts by weight of cerium oxide powder for the abrasive.

### Claim 4 (depends on 1)

The CMP slurry as claimed in claim 1, wherein the cerium oxide prepared by using the hexagonal crystal structured cerium carbonate is used in an amount of 50 parts or more and less than 100 parts by weight per 100 parts by weight of cerium oxide powder for the abrasive.

### Claim 5 (depends on 1)

The CMP slurry as claimed in claim 1, the CMP slurry comprising the abrasive, a dispersant, and water, wherein cerium oxide powder for the abrasive is used in an amount of 0.5 to 50 parts by weight per 100 parts by weight of the slurry; and the dispersant is used in an amount of 0.5 to 10 parts by weight per 100 parts by weight of the cerium oxide powder for the abrasive.

### Claim 6

A method of preparing a cerium carbonate by carrying out mixing and a precipitation reaction of an aqueous solution of a cerium precursor and an aqueous solution of a carbonate precursor,
wherein the cerium carbonate is controlled to have a lanthanite-(Ce) crystal structure, an orthorhombic crystal structure, or a hexagonal crystal structure by adjusting cerium concentration of the aqueous solution of the cerium precursor within a range of 0.01 to 10M, or by adjusting temperature of the precipitation reaction within a range of 0 to 99° C.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein the cerium carbonate has the lanthanite-(Ce) crystal structure by adjusting the cerium concentration of the aqueous solution of the cerium precursor within a range of 0.01 to 2.2M, and adjusting the temperature of the precipitation reaction within a range of 0 to 30° C.

### Claim 8 (depends on 6)

The method as claimed in claim 6, wherein the cerium carbonate has the orthorhombic crystal structure by adjusting the cerium concentration of the aqueous solution of the cerium precursor within a range of 1 to 10M, and adjusting the temperature of the precipitation reaction within a range of greater than 30° C. and 99° C. or less.

### Claim 9 (depends on 6)

The method as claimed in claim 6, wherein the cerium carbonate has the hexagonal crystal structure by adjusting the cerium concentration of the aqueous solution of the cerium precursor within a range of 0.01M or more and less than 1M, and adjusting the temperature of the precipitation reaction within a range of greater than 30° C. and 99° C. or less.

### Claim 10 (depends on 6)

The method as claimed in claim 6, wherein cerium carbonate powder comprising at least two kinds of cerium carbonates selected from the group including a lanthanite-(Ce) crystal structured cerium carbonate, an orthorhombic crystal structured cerium carbonate, and a hexagonal crystal structured cerium carbonate is prepared by varying the cerium concentration in the aqueous solution of the cerium precursor with time in a continuous reactor, or varying the temperature of the precipitation reaction.

### Claim 11 (depends on 6)

The method as claimed in claim 6, wherein the cerium precursor comprises trivalent or tetravalent cerium salt.

### Claim 12 (depends on 6)

The method as claimed in claim 6, wherein the cerium precursor is selected from the group including cerium nitrate, cerium sulfate, cerium chloride, diammonium cerium nitrate, and diammonium cerium nitrate hydrate.

### Claim 13 (depends on 6)

The method as claimed in claim 6, wherein the carbonate precursor is ammonium carbonate.

### Claim 14 (depends on 6)

The method as claimed in claim 6, wherein in the reaction, a molar concentration ratio of the cerium precursor to the carbonate precursor is within a range of 1:0.1 to 1:20.

### Claim 15 (depends on 6)

The method as claimed in claim 6, wherein the precipitation reaction of the cerium precursor and the carbonate precursor is performed for 30 minutes to 6 hours.

### Claim 16

Cerium oxide powder for an abrasive, which comprises at least two kinds of cerium oxides selected from the group including (i) a cerium oxide prepared by using a lanthanite-(Ce) crystal structured cerium carbonate; (ii) a cerium oxide prepared by using an orthorhombic crystal structured cerium carbonate; and (iii) a cerium oxide prepared by using a hexagonal crystal structured cerium carbonate.

### Claim 17 (depends on 16)

The cerium oxide powder as claimed in claim 16, which is prepared by
(a) carrying out calcination of cerium carbonate powder comprising at least two kinds of cerium carbonates selected from the group including the lanthanite-(Ce) crystal structured cerium carbonate, the orthorhombic crystal structured cerium carbonate, and the hexagonal crystal structured cerium carbonate; or
(b) mixing at least two kinds of cerium oxides selected from the group including the cerium oxide prepared by calcinating the lanthanite-(Ce) crystal structured cerium carbonate; the cerium oxide prepared by calcinating the orthorhombic crystal structured cerium carbonate; and the cerium oxide prepared by calcinating the hexagonal crystal structured cerium carbonate.

### Claim 18 (depends on 17)

The cerium oxide powder as claimed in claim 17, wherein the calcination is carried out within a range of 400 to 1200° C.

### Claim 19 (depends on 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 17)

The cerium oxide powder as claimed in claim 17, wherein the lanthanite-(Ce) crystal structured cerium carbonate, the orthorhombic crystal structured cerium carbonate, and the hexagonal crystal structured cerium carbonate are prepared by the method as claimed in any one of claims 6 to 15.

### Claim 20 (depends on 1, 2, 3, 4, 5)

A shallow trench isolation (STI) process using the CMP slurry as claimed in any one of claims 1 to 5.

### Claim 21

A method of adjusting at least one polishing property selected from the group including a polishing rate of a silicon oxide layer, a polishing rate of a silicon nitride layer, polishing selectivity between the silicon oxide layer and the silicon nitride layer, and within-wafer non-uniformity (WIWNU), by using at least two kinds of cerium oxides selected from the group including (i) a cerium oxide prepared by using a lanthanite-(Ce) crystal structured cerium carbonate; (ii) a cerium oxide prepared by using an orthorhombic crystal structured cerium carbonate; and (iii) a cerium oxide prepared by using a hexagonal crystal structured cerium carbonate, as an abrasive for CMP slurry.

### Claim 22 (depends on 21)

The method as claimed in claim 21, wherein the at least one polishing property selected from the group including the polishing rate of the silicon oxide layer, the polishing rate of the silicon nitride layer, the polishing selectivity between the silicon oxide layer and the silicon nitride layer, and the WIWNU, is adjusted by adjusting a mixing ratio of the at least two kinds of the cerium oxides in the abrasive.

### Claim 23 (depends on 21)

The method as claimed in claim 21, wherein the polishing rate of the silicon oxide layer is increased by increasing a content of the cerium oxide prepared by using the lanthanite-(Ce) crystal structured cerium carbonate in the abrasive.

### Claim 24 (depends on 21)

The method as claimed in claim 21, wherein the polishing rate of the silicon nitride layer is increased by increasing a content of the cerium oxide prepared by using the orthorhombic crystal structured cerium carbonate in the abrasive.

### Claim 25 (depends on 21)

The method as claimed in claim 21, wherein the polishing selectivity between the silicon oxide layer and the silicon nitride layer, and/or the WIWNU are/is increased by increasing a content of the cerium oxide prepared by using the hexagonal crystal structured cerium carbonate in the abrasive.