# US 2010/0062558 A1 · Method for producing transparent conductive layer comprising TIO2 and method for producing semiconductor light-emitting element utilizing said method for producing transparent conductive layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0062558 A1
- Document ID: US20100062558A1
- Status: Published application
- Kind: A1
- Application number: 12/585,015
- Filed: 2009-08-31
- Published: 2010-03-11
- Earliest claimed: 2008-09-01
- Assignees: Toyoda Gosei Co., Ltd.; Kanagawa Academy of Science and Technology
- Inventors: Koichi Goshonoo; Miki Moriyama; Taro Hitosugi; Tetsuya Hasegawa; Junpei Kasai
- Web page: https://patentgrep.com/patent/US20100062558A1

## CPC

- H10H 20/84: Coatings, e.g. passivation layers or antireflective coatings
- H10H 20/01: Manufacture or treatment
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

When a p-layer 4 composed of GaN is maintained at ordinary temperature and TNO is sputtered thereon by an RF magnetron sputtering method, a laminated TNO layer 5 is in an amorphous state. Then, there is included a step of thermally treating the amorphous TNO layer in a reduced-pressure atmosphere where hydrogen gas is substantially absent to thereby crystallize the TNO layer. At the sputtering, an inert gas is passed through together with oxygen gas, and volume % of the oxygen gas contained in the gas passed through is 0.10 to 0.15%. In this regard, oxygen partial pressure is 5×10−3 Pa or lower. The temperature of the thermal treatment is 500° C. for about 1 hour.

## Claims

### Claim 1

A method for producing a transparent conductive layer comprising TiO2 on a Group III nitride-based compound semiconductor layer, the method comprising:
a lamination step of laminating an amorphous TiO2 layer on the Group III nitride-based compound semiconductor layer; and
a thermal treatment step of thermally treating the amorphous TiO2 layer in an atmosphere where hydrogen gas is substantially absent to so as to crystallize the TiO2 layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the TiO2 layer is doped with one or more elements selected from the group consisting of Nb, Ta, Mo, As, Sb, Al and W.

### Claim 3 (depends on 1)

The Method according to claim 1, wherein the thermal treatment step is performed at 400° C. to 800° C. in an atmosphere where hydrogen gas is substantially not contained.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the lamination step is preformed by a sputtering method, an inert gas is passed through together with oxygen gas, and a ratio of the oxygen in the gas passed through is 0.05 to 0.20% by volume.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the ratio of the oxygen in the gas passed through is 0.10 to 0.15% by volume.

### Claim 6 (depends on 1)

The method according to claim 1, further comprising:
a step of patterning the amorphous TiO2.

### Claim 7 (depends on 6)

A method for producing a semiconductor light-emitting element, the method comprising:
a step of forming a p-type Group III nitride-based compound semiconductor layer, and
a step of subsequently forming a transparent conductive layer comprising TiO2 on the p-type Group III nitride-based compound semiconductor layer by performing the method according to the claim 6.