# US 2010/0062276 A1 · Method for modifying wood and wood thereby obtained

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0062276 A1
- Document ID: US20100062276A1
- Status: Published application
- Kind: A1
- Application number: 12/305,080
- Filed: 2007-06-18
- Published: 2010-03-11
- Earliest claimed: 2006-06-21
- Assignees: Transfurans Chemicals
- Inventors: Wim Van Rhijn
- Web page: https://patentgrep.com/patent/US20100062276A1

## CPC

- B27K 3/343: {Heterocyclic compounds}
- B27K 3/153: {Without in-situ polymerisation, condensation, or cross-linking reactions}
- Y10T 428/662: Wood timber product [e.g., piling, post, veneer, etc.]
- B27K: PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR (applying liquids or other fluent materials to surfaces in general B05; coating wood or similar material B44D); CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for modifying wood includes steps of impregnating the wood followed by curing the wood at temperatures between 70 and 200° C. The impregnation composition includes di-, tri-, and/or polysubstituted furan compounds.

## Claims

### Claim 1

A method for modifying wood comprising the steps of:
a) impregnating said wood with a polymerizable composition comprising a compound of formula I and/or formula II
wherein n is 0, 1, 2, 3, 4 or 5,
wherein t and s each independently are 1 or 2,
wherein w and z each independently are 0 or 1,
wherein X and Y each independently are O, S or N—R21 and
wherein R2, R3, R4, R5, R6, R7, R9, R10, R11, R12, R13, R14, R15, R16, R17, R18, R19, R21 are each independently hydrogen or selected from the group consisting of C1-C2 alkyl, carboxaldehyde, hydroxyalkyl, carboxyl, aminoalkyl, alkylaminoalkyl hydroxyalkylfurylalkyl, alkyloxy, alkoxyalkyl, alkylcarbonylalkenyl, alkylcarbonyloxyalkyl, alkyloxycarbonylalkenyl, alkenylcarbonyloxyalkyl, oxiranyl, isocyanate, isocyanate-alkyl, alkylcarboxy, alkenylcarboxy, alkylcarbonyl, alkenylcarbonyl, halocarbonyl, haloalkyl, haloaryl, haloalkenyl, imino, thioalkyl, alkylthioalkyl, cyano and any mixtures thereof,
whereby each group is optionally substituted with one or more substituents selected from C1-C2 alkyl, C2-C4 alkenyl, C2-C4 alkynyl, hydroxyl, carboxyl, nitro, amino, alkylfuryl, hydroxyalkylfurylalkyl, isocyanate, formyl, halocarbonyl, and thiol,
wherein R1, R8, R17 and R20 are each independently selected from the group consisting of carboxaldehyde, hydroxyalkyl, carboxyl, aminoalkyl, alkylaminoalkyl, hydroxyalkylfurylalkyl, alkyloxy, alkoxyalkyl, alkylcarbonylalkenyl, alkylcarbonyloxyalkyl, alkyloxycarbonylalkenyl, alkenylcarbonyloxyalkyl, oxiranyl, isocyanate, isocyanate-alkyl, alkylcarboxy, alkenylcarboxy, alkylcarbonyl, alkenylcarbonyl, halocarbonyl, haloalkyl, haloaryl, haloalkenyl, imino, thioalkyl, alkylthioalkyl, cyano and any mixtures thereof,
whereby each group is optionally substituted with one or more substituents selected from C1-C2 alkyl, C2-C4 alkenyl, C2-C4 alkynyl, hydroxyl, carboxyl, nitro, amino, alkylfuryl, hydroxyalkylfurylalkyl, isocyanate, formyl, halocarbonyl, and thiol, and
wherein the dotted line represents a double bond,
wherein said compounds are diluted in water, and
wherein said composition further comprises a catalyst which is an ammonium salt, an organic acid, an anhydride, an inorganic acid, magnesium chloride, magnesium sulfate, magnesium nitrate, zinc chloride, zinc nitrate, aluminum chloride, aluminum nitrate, aluminum sulfate or any mixtures thereof,
and
b) reacting said impregnated wood at a temperature of between 70 and 200° C.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said impregnated wood is reacted in step b) at a temperature of between 70 and 150° C. for 1 to 48 hours.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said composition is applied at a loading of between 25 and 1000 kg per m3 wood.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising the step of drying said impregnated wood prior to reacting to a moisture content of between 1 and 50%.

### Claim 5 (depends on 1)

The method according to claim 1, wherein said wood is impregnated in step a) with a polymerizable composition which comprises a compound selected from the group consisting of 2,5-bis(hydroxymethyl)furan; 2,3,5-tris(hydroxymethyl)furan; 5-methyl-2-furfuryl alcohol; 3-hydroxymethyl-5-methyl-2-furfurylalcohol; 2,2′-(hydroxymethyl)difurylmethane; 2,2′,3,3′-(hydroxymethyl)difurylmethane; 2,2′,4,4′-(hydroxymethyl)difurylmethane; 5-hydroxymethyl-α-(methyl)furfurylalcohol; 5-hydroxymethyl-2-furancarboxaldehyde; 3,5-hydroxymethyl-2-furancarboxaldehyde; 4,5-hydroxymethyl-2-furancarboxaldehyde; 5-hydroxymethyl-2-furfurylamine; 5-methyl-2-furfurylamine; 5-carboxaldehyde-2-furfurylamine; 5-carboxy-2-furfurylamine; 2,5-bis(aminomethyl)furan; 5-hydroxymethyl-2-furancarboxaldehyde; and 5-hydroxymethyl-2-furfurylamine; or any mixtures thereof.

### Claim 6 (depends on 1)

The method according to claim 1, wherein said wood is impregnated in step a) with a polymerizable composition comprising a compound selected from the group consisting of 2,5-bis(hydroxymethyl)furan (BHMF); 2,3,5-tris(hydroxymethyl)furan (THMF); 2,2′-(hydroxymethyl)difurylmethane (HMDM); 2,2′,3,3′-(hydroxymethyl)difurylmethane; 2,2′,4,4′-(hydroxymethyl)difurylmethane; 5-hydroxymethyl-2-furancarboxaldehyde; and 5-hydroxymethyl-2-furfurylamine; and 2,5-bis(aminomethyl)furan, or any mixtures thereof.

### Claim 7 (depends on 1)

The method according to claim 1, wherein said wood is impregnated in step a) with a polymerizable composition comprising a compound selected from the group consisting of 2,5-bis(hydroxymethyl)furan (BHMF); 2,3,5-tris(hydroxymethyl)furan (THMF); 2,2′(hydroxymethyl)difurylmethane (HMDM); and optionally condensation products thereof, or mixtures thereof.

### Claim 8 (depends on 7)

The method according to claim 7, wherein said compounds are obtained by hydroxymethylation of at least one furfuryl alcohol compound with a formaldehyde source.

### Claim 9 (depends on 1)

The method according to claim 1, wherein said compound of formula I and/or formula II is present in said composition in an amount of between 3 and 100% by weight.

### Claim 10

(canceled)

### Claim 11 (depends on 1)

Wood obtainable by the method of claim 1 having a weight percentage gain (WPG) of at least 3%.

### Claim 12 (depends on 11)

A method for manufacturing a product comprising constructing the product from wood according to claim 11, wherein the product is selected from the group consisting of knife handles, kitchenware (spoons, forks, cutting boards, bowls), furniture, indoor flooring, countertops, building parts (facia, cornice, siding, sills, frames, millwork), boat parts (frames, planking, decks, rails, flooring, deck trim, deck flooring, furniture, fittings), marine items (docks, piers, lobster traps, weir poles), outdoor items (furniture, decks, railings and stairs, walkways, boardwalks, playground equipment), bridge parts (beams, railings, decking), gunstocks and pistol grips, musical instrument parts (piano keys, violin and guitar fingerboards and bridges), railway sleepers, cooling tower slats, utility poles, outdoor walkways, flooring, heavy timbers, fenceposts, stakes, highway items (guard rail posts, guard rail plates, sign posts, light poles), containers (tanks, buckets), machine parts (conveyor slats, saw guides, saw and planer table tops), joinery parts (window frames, doors).

### Claim 13 (depends on 1)

Wood obtainable by the method of claim 1 having a weight percentage gain (WPG) of between 3 and 150%.