# US 2010/0062265 A1 · Titanium Dioxide Coatings and Methods of Forming Titanium Dioxide Coatings Having Reduced Crystallite Size

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0062265 A1
- Document ID: US20100062265A1
- Status: Published application
- Kind: A1
- Application number: 12/207,235
- Filed: 2008-09-09
- Published: 2010-03-11
- Earliest claimed: 2008-09-09
- Assignees: Guardian Industries Corp.
- Inventors: PRAMOD K. SHARMA
- Web page: https://patentgrep.com/patent/US20100062265A1

## CPC

- A01N 59/16: Heavy metals; Compounds thereof
- B01J 35/39: Photocatalytic properties
- B01J 37/0215: {Coating}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01G 23/053: Producing by wet processes, e.g. hydrolysing titanium salts
- C03C 17/256: {Coating containing TiO2}
- C09C 1/3607: {Titanium dioxide}
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- C01P 2002/84: by UV- or VIS- data
- C03C 2217/212: TiO2
- C03C 2218/113: by sol-gel processes
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Methods for forming titanium dioxide coatings having crystals comprising reduced crystallite size are disclosed. Sol-gel compositions are prepared, formed on a substrate, and the coated substrate is heated at a temperature sufficient to form a titanium dioxide coating with crystals having a reduced crystallite size. Titanium dioxide coatings having crystals comprising reduced crystallite size and having at least one of improved antimicrobial properties, self-cleaning properties, and/or hydrophilicity are also disclosed. Substrates comprising such coatings are also disclosed.

## Claims

### Claim 1

A method of forming a titanium dioxide coating comprising crystals having a reduced crystallite size on a substrate, comprising:
preparing a titanium dioxide sol-gel composition;
coating the substrate with the sol-gel composition; and
heating the coated substrate at a temperature sufficient to form a titanium dioxide coating comprising crystals having a reduced crystallite size.

### Claim 2 (depends on 1)

The method of claim 1, wherein said coated substrate is heated at a temperature of at least 575° C.

### Claim 3 (depends on 2)

The method of claim 2, wherein said coated substrate is heated at a temperature of at least about 600° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the coated substrate is heated at a temperature sufficient to form a titanium dioxide coating comprising a water contact angle less than about 10°.

### Claim 5 (depends on 1)

The method of claim 1, wherein the titanium dioxide coating comprises crystals having a crystallite size less than about 35 nm.

### Claim 6 (depends on 5)

The method of claim 5, wherein the titanium dioxide coating comprises crystals having a crystallite size less than about 25 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the substrate comprises a glass substrate.

### Claim 8 (depends on 7)

The method of claim 7, wherein the glass substrate is chosen from clear and low-iron glass.

### Claim 9

A method of improving at least one of antimicrobial properties, self-cleaning properties, and hydrophilicity of a titanium dioxide coating, comprising:
preparing a titanium dioxide sol-gel composition;
coating a substrate with the sol-gel composition; and
heating the coated substrate to form a titanium dioxide coating comprising crystals having a reduced crystallite size.

### Claim 10 (depends on 9)

The method of claim 9, wherein the coated substrate is heated at a temperature at least about 575° C.

### Claim 11 (depends on 10)

The method of claim 10, wherein the coated substrate is heated at a temperature at least about 600° C.

### Claim 12 (depends on 9)

The method of claim 9, wherein said crystals have a crystallite size less than about 35 nm.

### Claim 13 (depends on 12)

The method of claim 12, wherein said crystals have a crystallite size less than about 25 nm.

### Claim 14 (depends on 9)

The method of claim 9, wherein the titanium dioxide coating comprises a water contact angle less than about 10°.

### Claim 15

A substrate comprising a titanium dioxide coating comprising crystals having a reduced crystallite size, wherein the titanium dioxide coating comprises crystals having a crystallite size less than about 35 nm.

### Claim 16 (depends on 15)

The substrate comprising a titanium dioxide coating comprising crystals having a reduced crystallite size of claim 15, wherein the titanium dioxide coating comprises crystals having a crystallite size less than about 25 nm.

### Claim 17 (depends on 15)

The substrate comprising a titanium dioxide coating comprising crystals having a reduced crystallite size of claim 15, wherein the titanium dioxide coating comprises a water contact angle less than about 10°.

### Claim 18 (depends on 15)

The substrate comprising a titanium dioxide coating comprising crystals having a reduced crystallite size of claim 15, wherein the substrate comprises a glass substrate.

### Claim 19 (depends on 18)

The antimicrobial coating of claim 18, wherein the glass substrate is chosen from clear and low iron glass.

### Claim 20

A titanium dioxide coating having at least one of improved antimicrobial properties, improved self-cleaning properties, and improved hydrophilicity, wherein said titanium dioxide coating is made by:
preparing a titanium dioxide sol-gel composition;
coating a substrate with the sol-gel composition; and
heating the coated substrate to form a titanium dioxide coating comprising crystals having a reduced crystallite size.

### Claim 21

A substrate comprising a titanium dioxide coating having a reduced crystallite size, wherein said titanium dioxide coating is made by:
preparing a titanium dioxide sol-gel composition;
coating the substrate with the sol-gel composition; and
heating the coated substrate at a temperature sufficient to form a titanium dioxide coating comprising crystals having a reduced crystallite size.