# US 2010/0059900 A1 · Translucent, Flame Resistant Composite Materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0059900 A1
- Document ID: US20100059900A1
- Status: Published application
- Kind: A1
- Application number: 12/577,618
- Filed: 2009-10-12
- Published: 2010-03-11
- Earliest claimed: 2003-12-24
- Assignees: The Boeing Company
- Inventors: Daniel W. Cushing; Eugene A. Jackson; Keith H. Novak; David N. Dunn; Gregory R. Bell
- Web page: https://patentgrep.com/patent/US20100059900A1

## CPC

- B32B 27/08: of synthetic resin
- B32B 27/04: as impregnant, bonding, or embedding substance {(not used)}
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 27/28: comprising synthetic resins not wholly covered by any one of the sub-groups {B32B27/30 - B32B27/42}
- C08J 5/043: {with glass fibres}
- B32B 2260/021: Fibrous or filamentary layer
- B32B 2260/046: Synthetic resin
- B32B 2307/3065: Flame resistant or retardant, fire resistant or retardant
- B32B 2307/414: Translucent
- B32B 2605/18: Aircraft
- C08J 2381/06: Polysulfones; Polyethersulfones
- Y10T 442/2631: Coating or impregnation provides heat or fire protection
- Y10T 442/2992: Coated or impregnated glass fiber fabric
- Y10T 442/3472: Woven fabric including an additional woven fabric layer
- Y10T 442/3976: Including strand which is stated to have specific attributes [e.g., heat or fire resistance, chemical or solvent resistance, high absorption for aqueous composition, water solubility, heat shrinkability, etc.]
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A translucent composite material that can be used in various airplane interior applications that allows sufficient light transmissivity while preferably meeting Federal Aviation Administration (FAA) flammability requirements for overhead materials in the cabin of a commercial aircraft. The material also meets FAA standards regarding vertical burn, smoke emissions tests, and toxic fume emissions tests. The composite material is formed by laminating long glass fibers and (PPSU) into a composite sheet under controlled heat and pressure. The composite sheet is then cut, bent or thermoformed to form the desired part. The parts formed are available for a wide variety of uses within the passenger cabin of a commercial aircraft. The long glass fibers may be unidirectional or weaved into a glass cloth like material. While preferably formed for airplane interior applications, these components may also be used in other aerospace or non-aerospace applications.

## Claims

### Claim at position 1

1-18. (canceled)

### Claim 19

A method for forming a composite material for use in translucent, flame-resistant components, the method comprising:
introducing a layer of polyphenylsulfone substrate material to a mold;
introducing a fibrous material onto an entire top surface of said polyphenylsulfone substrate material within said mold, said fibrous material comprising a plurality of long glass fibers;
preheating said mold to a first temperature to soften said polyphenylsulfone substrate material;
laminating said fibrous material to said polyphenylsulfone substrate material such that said plurality of long glass fibers are substantially encapsulated within said polyphenylsulfone substrate material while substantially preventing said polyphenylsulfone substrate from outgassing;
cooling said mold under controlled heat and pressure to form the composite material; and
removing said composite material from said mold.

### Claim 20 (depends on 19)

The method of claim 19, wherein introducing a fibrous material comprises introducing a plurality of unidirectional long glass fibers onto an entire top surface of said polyphenylsulfone substrate material within said mold.

### Claim 21 (depends on 19)

The method of claim 19, wherein introducing a fibrous material comprises introducing a weaved glass fiber layer onto an entire top surface of said polyphenylsulfone substrate material within said mold, said weaved glass fiber layer comprising a plurality of long glass fibers.

### Claim 22 (depends on 19)

The method of claim 19, wherein preheating said mold comprises preheating said mold to about 535 degrees Fahrenheit over about 15 minutes to soften said polyphenylsulfone substrate material.

### Claim 23 (depends on 22)

The method of claim 22, wherein laminating said fibrous material to said polyphenylsulfone substrate material comprises:
holding said mold at about 535 degrees Fahrenheit for 0 minutes to about 55 minutes;
increasing said pressure of said mold at 0 minutes to about 15 pounds per square inch part pressure;
holding said mold at about 15 pounds per square inch part pressure between about 0 minutes and about 5 minutes;
increasing said pressure from about 15 pounds per square inch part pressure to about 50 pounds per square inch part pressure at 5 minutes;
holding said mold at about 50 pounds per square inch part pressure between about 5 minutes and about 27 minutes;
increasing said pressure from about 50 pounds per square inch part pressure to about 100 pounds per square inch part pressure at 27 minutes;
holding said mold at about 100 pounds per square inch part pressure between about 27 minutes and about 47 minutes;
increasing said pressure from about 100 pounds per square inch part pressure to about 200 pounds per square inch part pressure at 47 minutes; and
holding said mold at about 200 pounds per square inch part pressure between about 47 minutes and about 55 minutes.

### Claim 24 (depends on 23)

The method of claim 23, wherein cooling said mold comprises:
slowly cooling said mold from about 535 degrees Fahrenheit to about 235 degrees Fahrenheit at 200 pounds per square inch part pressure at a cooling rate of about 5 degrees Fahrenheit per minute; and
further cooling said mold to about 150 degrees Fahrenheit at about 100 pounds per square inch part pressure.

### Claim 25

A method for forming a composite material for use in translucent, flame-resistant components, the method comprising:
introducing a polyphenylsulfone substrate material to an extruder;
melting said polyphenylsulfone substrate material within said extruder;
introducing said melted polyphenylsulfone substrate material to a calendar roll stack;
introducing a fibrous material layer onto a top surface of said first portion within said calendar roll stack, said fibrous substrate material layer comprising a plurality of long glass fibers;
pressing said fibrous substrate material layer within said melted polyphenylsulfone substrate material within said calendar roll stack to form the composite material such that said plurality of long glass fibers are substantially encapsulated within said melted polyphenylsulfone substrate material; and
removing the composite material from the calendar roll stack.

### Claim 26 (depends on 25)

The method of claim 25, wherein introducing a fibrous material layer comprises introducing a layer of unidirectional long glass fibers onto an entire top surface of said melted polyphenylsulfone substrate material within said calendar roll stack.

### Claim 27 (depends on 25)

The method of claim 25, wherein introducing a fibrous material layer comprises introducing a weaved glass fiber layer onto an entire top surface of said melted polyphenylsulfone substrate material within said calendar roll stack, said weaved glass fiber layer comprising a plurality of long glass fibers.

### Claim 28

A method for forming a composite material for use in translucent, flame-resistant components, the method comprising:
introducing a first layer of a polyphenylsulfone substrate material to a mold;
introducing a fibrous material onto an entire top surface of said polyphenylsulfone substrate material within said mold, said fibrous material comprising a plurality of long glass fibers;
introducing a second layer of said polyphenylsulfone substrate material to a mold such that said fibrous material is sandwiched between said first layer and said second layer;
preheating said mold to a first temperature to soften said first layer and said second layer;
laminating said fibrous material to said first layer and said second layer such that said plurality of long glass fibers are substantially encapsulated within said polyphenylsulfone substrate material while substantially preventing said first layer and said second layer from outgassing;
cooling said mold under controlled heat and pressure to form the composite material; and
removing said composite material from said mold.

### Claim 29 (depends on 28)

The method of claim 28, wherein introducing a fibrous material comprises introducing a plurality of unidirectional long glass fibers onto an entire top surface of said polyphenylsulfone substrate material within said mold.

### Claim 30 (depends on 28)

The method of claim 28, wherein introducing a fibrous material comprises introducing a weaved glass fiber layer onto an entire top surface of said polyphenylsulfone substrate material within said mold, said weaved glass fiber layer comprising a plurality of long glass fibers.

### Claim 31 (depends on 28)

The method of claim 28, wherein preheating said mold comprises preheating said mold to about 535 degrees Fahrenheit over about 15 minutes to soften said polyphenylsulfone substrate material.

### Claim 32 (depends on 31)

The method of claim 31, wherein laminating said fibrous material to said polyphenylsulfone substrate material comprises:
holding said mold at about 535 degrees Fahrenheit for 0 minutes to about 55 minutes;
increasing said pressure of said mold at 0 minutes to about 15 pounds per square inch part pressure;
holding said mold at about 15 pounds per square inch part pressure between about 0 minutes and about 5 minutes;
increasing said pressure from about 15 pounds per square inch part pressure to about 50 pounds per square inch part pressure at 5 minutes;
holding said mold at about 50 pounds per square inch part pressure between about 5 minutes and about 27 minutes;
increasing said pressure from about 50 pounds per square inch part pressure to about 100 pounds per square inch part pressure at 27 minutes;
holding said mold at about 100 pounds per square inch part pressure between about 27 minutes and about 47 minutes;
increasing said pressure from about 100 pounds per square inch part pressure to about 200 pounds per square inch part pressure at 47 minutes; and
holding said mold at about 200 pounds per square inch part pressure between about 47 minutes and about 55 minutes.

### Claim 33 (depends on 32)

The method of claim 32, wherein cooling said mold comprises:
slowly cooling said mold from about 535 degrees Fahrenheit to about 235 degrees Fahrenheit at 200 pounds per square inch part pressure at a cooling rate of about 5 degrees Fahrenheit per minute; and
further cooling said mold to about 150 degrees Fahrenheit at about 100 pounds per square inch part pressure.

### Claim 34

A method for forming a translucent, flame resistant component for use in the cabin area of a commercial aircraft, the method comprising:
forming a composite material, said composite material comprising a polyphenylsulfone substrate material substantially encapsulating a plurality of long glass fibers, wherein said composite material has an average allowable heat release not to exceed a 65/65 standard; and
post processing said composite material to form the translucent, flame resistant component.

### Claim 35 (depends on 34)

The method of claim 34, wherein said translucent, flame resistant component is selected from the group consisting of a countertop, a cabinet enclosure, a tray table, a backlit lighted sign, an illuminating window panel, a window bezel, a class divider, a privacy partition, a backlit ceiling panel, a direct lighting ceiling panel, a backlit control panel, a lighted door, a lighted door latch, a doorway lining, a proximity light, a stow bin door, a privacy curtain, a translucent door handle, a translucent amenities cabinet, a translucent sink deck a doorway liner, a stow bin latch handle, and a lighted phone.

### Claim 36 (depends on 34)

The method of claim 34, wherein forming a composite material comprises:
introducing a layer of polyphenylsulfone substrate material to a mold;
introducing a fibrous material onto an entire top surface of said polyphenylsulfone substrate material within said mold, said fibrous material comprising a plurality of long glass fibers;
preheating said mold to a first temperature to soften said polyphenylsulfone substrate material;
laminating said fibrous material to said polyphenylsulfone substrate material such that said plurality of long glass fibers are substantially encapsulated within said polyphenylsulfone substrate material while substantially preventing said polyphenylsulfone substrate from outgassing;
cooling said mold under controlled heat and pressure to form the composite material; and
removing said composite material from said mold.

### Claim 37 (depends on 34)

The method of claim 34, wherein forming a composite material comprises:
introducing a first layer of a polyphenylsulfone substrate material to a mold;
introducing a fibrous material onto an entire top surface of said polyphenylsulfone substrate material within said mold, said fibrous material comprising a plurality of long glass fibers;
introducing a second layer of said polyphenylsulfone substrate material to a mold such that said fibrous material is sandwiched between said first layer and said second layer;
preheating said mold to a first temperature to soften said first layer and said second layer;
laminating said fibrous material to said first layer and said second layer such that said plurality of long glass fibers are substantially encapsulated within said polyphenylsulfone substrate material while substantially preventing said first layer and said second layer from outgassing;
cooling said mold under controlled heat and pressure to form the composite material; and
removing said composite material from said mold.

### Claim 38 (depends on 34)

The method of claim 34, wherein forming a composite material comprises:
introducing a polyphenylsulfone substrate material to an extruder;
melting said polyphenylsulfone substrate material within said extruder;
introducing said melted polyphenylsulfone substrate material to a calendar roll stack;
introducing a fibrous material layer onto a top surface of said first portion within said calendar roll stack, said fibrous substrate material layer comprising a plurality of long glass fibers;
pressing said fibrous substrate material layer within said melted polyphenylsulfone substrate material within said calendar roll stack to form the composite material such that said plurality of long glass fibers are substantially encapsulated within said melted polyphenylsulfone substrate material; and
removing the composite material from the calendar roll stack.

### Claim 39 (depends on 34)

The method of claim 34, wherein post processing said composite material is selected from the group consisting of cutting said composite material to a desired shape and size, thermoforming said composite material to a desired shape and size and bending said composite material to a desired shape and size.