# US 2009/0291383 A1 · Toner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0291383 A1
- Document ID: US20090291383A1
- Status: Published application
- Kind: A1
- Application number: 12/511,641
- Filed: 2009-07-29
- Published: 2009-11-26
- Earliest claimed: 2008-02-25
- Assignees: Canon Kabushiki Kaisha
- Inventors: Yasukazu Ayaki; Atsushi Tani; Tsuneyoshi Tominaga
- Web page: https://patentgrep.com/patent/US20090291383A1

## CPC

- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/0821: {characterised by physical parameters (magnetic parameters G03G9/083)}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G 9/09314: {Macromolecular compounds}
- G03G 9/09357: {Macromolecular compounds}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

Toner characterized in that assuming that the glass transition point of the toner measured by a differential scanning calorimeter (DSC) is represented by T1 (° C.), in a micro compression test at T1−10 (° C.), when a load from 0.00 N (0.00 mgf) to 7.85×10−4 N (80.00 mgf) is applied at the intervals of 7.85×10−7 N (0.08 mgf) to a single particle of the toner, the strain value A80a (%) at 7.85×10−4 N is 35.0 to 75.0%; and in a load (x-axis)-strain (y-axis) curve obtained by the micro compression test, the ratio of an area (S1a) of a specific region, relative to an area (S2a) of a specific region, (S1a/S2a), is 1.5 to 3.5.

## Claims

### Claim 1

A toner comprising toner particles containing at least a binder resin, a colorant and wax, and inorganic fine powder, wherein, assuming that the glass transition point of the toner measured by a differential scanning calorimeter (DSC) is represented by T1 (° C.), in a micro compression test for the toner at T1-10 (° C.), when a load from 0.00N (0.00 mgf) to 7.85×10−4 N (80.00 mgf) is applied at the intervals of 7.85×10−7 N (0.08 mgf) to a single particle of the toner, the strain value A80a (%) at 7.85×10−4 N is 35.0 to 75.0%; and in a load (x-axis)-strain (y-axis) curve obtained by the micro compression test, the ratio of an area (S1a) of a region, which is surrounded by the curve, a linear line of x=7.85×10−4 N and the x-axis, relative to an area (S2a) of a region, which is surrounded by a linear line connecting a point on the curve at x=3.92×10−5 N (4.00 mgf) to a point on the curve at x=7.85×10−5 N (8.00 mgf), a linear line of x=7.85×10−4 N and the x-axis, that is, the ratio (S1a/S2a) is 1.5 to 3.5.

### Claim 2 (depends on 1)

The toner according to claim 1, wherein, assuming that the number average particle size of the toner is represented by D1T (μm), in a particle size (x-axis)-strain (y-axis) curve (R-A80 curve) obtained in the micro compression test, a change rate φ (%) between B10 (%), which is a strain value corresponding to D1T, and A80a, [φ=(A80a−B10)×100/B10] is 15.0% or less; and assuming that a strain value corresponding to a particle size which is 1.2 times D1T is represented by B12 (%) and a strain value corresponding to a particle size which is 0.8 times D1T is represented by B08 (%), the inclination α of B12 and B08, that is, [α=(B12−B08)/(D1T×0.4)] is −15.0 or less.

### Claim 3 (depends on 1)

The toner according to claim 1, wherein, in a particle size (x-axis)-inflection point (y-axis) curve (R-C curve) obtained in the micro compression test, assuming that a value of inflection point C corresponding to D1T is represented by C10 (N), C10 falls within the range of 9.81×10−5 to 3.43×10−4N (10.00 to 35.00 mgf); and assuming that a value of inflection point C corresponding to a particle size which is 1.2 times D1T is represented by C12 (N) and a value of inflection point C corresponding to a particle size which is 0.8 times D1T is represented by C08 (N), the inclination β of C12 and C08, [β=(C12−C08)/(D1T×0.4)] is 15.0 or less.

### Claim 4 (depends on 1)

The toner according to claim 1, wherein, in a load (x-axis)-strain (y-axis) curve obtained in the micro compression test of the toner at T1+5 (° C.), assuming that an area of a region which is surrounded by the curve, a linear line of x=7.85×10−4 N and the x-axis is represented by S1b and an area of a region which is surrounded by a linear line connecting a point on the curve at a load of 3.92×10−5 N to a point on the curve at a load of 7.85×10−5 N, a linear line of x=7.85×104 N and the x-axis is represented by S2b, the ratio of S1b and S1a, (S1b/S1a), is 1.2 to 3.0 and the ratio of S2b and S2a, (S2b/S2a), is 2.0 to 6.0.

### Claim 5 (depends on 1)

The toner according to claim 1, wherein the toner particles contain at least wax and a colorant and have a core-shell structure having a core phase containing a binder resin as a main component and a shell phase containing a surface-layer resin as a main component and covering the core phase.

### Claim 6 (depends on 5)

The toner according to claim 5, wherein the toner contains the surface-layer resin in an amount of 1.0 to 10.0 parts by mass relative to 100.0 parts by mass of core particles; the surface-layer resin has, in a loss tangent (tan δ) curve obtained in a dynamic viscoelasticity test, a maximum value of tan δ at a temperature Ts (° C.) within a range of 45.0 to 85.0° C. and, in a storage elastic modulus (G′) curve obtained in the dynamic viscoelasticity test, a value of G′ (G′10) at a temperature of Ts+10 (° C.), of 1.0×105 to 5.0×106 Pa and a value of G′ (G′30) at a temperature of Ts+30 (° C.), of 1.0×104 to 5.0×105 Pa.