# US 2009/0289394 A1 · Method for manufacturing shoe sole using natural latex

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0289394 A1
- Document ID: US20090289394A1
- Status: Published application
- Kind: A1
- Application number: 12/469,646
- Filed: 2009-05-20
- Published: 2009-11-26
- Earliest claimed: 2008-05-20
- Inventors: GEUN CHOUN LIM
- Web page: https://patentgrep.com/patent/US20090289394A1

## CPC

- A43B 13/04: Plastics, rubber or vulcanised fibre
- B29D 35/0054: {by compression moulding, vulcanising or the like; Apparatus therefor}
- B29D 35/122: {Soles}
- A43B: CHARACTERISTIC FEATURES OF FOOTWEAR; PARTS OF FOOTWEAR
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)

## Abstract

The present invention relates to a method for manufacturing a shoe sole using a natural latex in which a shoe sole is made of a liquid or solid natural latex, so a walking pressure is uniformly distributed during walking, and an impact is absorbed and released for a comfortable walking, and a slip does not occur with the help of a reliable non-slip function, and feet health can be enhanced along with a good ventilation and anti-microbial effect by providing a number of air cells, and an outer appearance looks good since a sole is made of a transparent material, and an environment-friendly product can be manufactured.

## Claims

### Claim 1

A method for manufacturing a shoe sole using a natural latex, comprising:
a step in which sulphur of vulcanization agent and ZnO are ground in a ball mill along with water and is mixed with a liquid natural latex and is agitated;
a step in which a vulcanization accelerator is added to the agitating mixture liquid;
a step in which an emulsifier is emulsified in water using plasticizer, and is agitated and mixed with the mixed liquid of the above step;
a step in which the mixture liquid is substantially agitated and is processed for 24 hours at a room temperature;
a step in which the processed mixture liquid is inputted into a sole mold and is heated for 15 to 20 minutes at 150° C. and is hardened; and
a step in which the hardened material is naturally cooled for thereby molding a sole.

### Claim 2

A method for manufacturing a shoe sole using a natural latex, comprising:
a step in which a solid mixture of sulphur, stearic acid and ZnO from which moisture is evaporated is mixed with a solid natural latex and is agitated;
a step in which a vulcanization accelerator is added to the agitating mixture liquid and is substantially agitated;
a step in which the mixture liquid is processed for 24 hours at a room temperature;
a step in which the processed mixture liquid is inputted into a sole mold and is sealed and is heated for 15 to 20 minutes at 150° C. and is hardened; and
a step in which the hardened mixture is naturally cooled for thereby molding a sole.