# US 2009/0288521 A1 · Precious metal recovery using thiocyanate lixiviant

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0288521 A1
- Document ID: US20090288521A1
- Status: Published application
- Kind: A1
- Application number: 12/476,084
- Filed: 2009-06-01
- Published: 2009-11-26
- Earliest claimed: 2003-04-04
- Assignees: Newmont USA Limited
- Inventors: Rong Yu Wan; K. Marc LeVier
- Web page: https://patentgrep.com/patent/US20090288521A1

## CPC

- C22B 11/08: by cyaniding
- C22B 3/24: by adsorption on solid substances, e.g. by extraction with solid resins
- C22B 3/42: by ion-exchange extraction
- C22B 15/0076: {Cyanide groups}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Mineral materials comprising copper and precious metal are subjected to an acidic leach of the copper followed by an acidic thiocyanate leach of the precious metal.

## Claims

### Claim at position 1

1-47. (canceled)

### Claim 48

A method for removing copper and precious metal from a mineral material feed comprising copper and comprising precious metal locked in one or more sulfide mineral, the method comprising:
pressure oxidizing the mineral material feed in particulate form slurried in an aqueous liquid to decompose at least a portion of the sulfide mineral, the pressure oxidizing comprising dissolving at least a majority of the copper of the mineral material feed into the aqueous liquid;
recovering from the pressure oxidizing solid residue and acidic liquid effluent, the solid residue comprising at least a portion of the precious metal from the mineral material feed, the liquid effluent comprising in solution at least a majority of the copper of the mineral material feed;
thiocyanate leaching at least a portion of the solid residue with an acidic thiocyanate leach solution to dissolve into the thiocyanate leach solution in the form of precious metal-thiocyanate complex at least a portion of the precious metal from the solid residue; and
separating from the liquid effluent and recovering in a purified copper-containing product at least a majority of the copper dissolved in the liquid effluent.

### Claim 49 (depends on 48)

The method of claim 48, wherein the pressure oxidizing is conducted at a temperature of at least 160° C. and an oxygen gas overpressure of at least 10 psi.

### Claim 50 (depends on 48)

The method of claim 48, wherein the mineral material feed comprises at least 1 weight percent of the nonferrous nonprecious metal that dissolves into the aqueous liquid during the pressure oxidizing and that is thereafter separated from the liquid effluent during the separating.

### Claim at position 5

51-87. (canceled)

### Claim 88 (depends on 48)

The method of claim 48, wherein feed of the thiocyanate leach solution to the thiocyanate leaching comprises dissolved ferric iron and a molar ratio of the dissolved ferric iron to the dissolved thiocyanate of at least 2.

### Claim 89 (depends on 88)

The method of claim 88, wherein the feed of the thiocyanate leach solution has a pH in a range of from pH 1 to pH 3 and the feed of the thiocyanate leach solution comprises from 0.0001 to 0.05 mole per liter of the dissolved thiocyanate and at least 0.05 mole per liter of the dissolved ferric iron.

### Claim 90 (depends on 89)

The method of claim 89, wherein the ratio of the dissolved ferric iron to the dissolved thiocyanate is at least 7.

### Claim 91 (depends on 89)

The method of claim 89, wherein the feed of the thiocyanate leach solution comprises not more that 0.03 mole per liter of the dissolved thiocyanate.

### Claim at position 10

92-96. (canceled)

### Claim 97 (depends on 48)

The method of claim 48, wherein the mineral material feed comprises at least 2 weight percent sulfide sulfur.

### Claim 98 (depends on 48)

The method of claim 48, wherein the mineral material feed comprises at least 3 weight percent sulfide sulfur.

### Claim 99 (depends on 98)

The method of claim 98, wherein the mineral material feed comprises a sulfide concentrate.

### Claim 100 (depends on 48)

The method of claim 48, wherein the mineral material feed comprises at least 5 weight percent of the copper that dissolves into the aqueous liquid during the pressure oxidizing and that is thereafter separated from the liquid effluent during the separating.

### Claim 101 (depends on 48)

The method of claim 48, wherein the separating comprises solvent extraction of copper from the liquid effluent.

### Claim 102 (depends on 48)

The method of claim 48, wherein the precious metal comprises gold; and
the thiocyanate leaching comprises dissolving into the thiocyanate leach solution at least a majority of the gold from the solid residue.

### Claim 103 (depends on 48)

The method of claim 48, wherein:
the pressure oxidizing is conducted at a temperature of at least 160° C. and oxygen gas over pressure of at least 10 psi;
the feed of the thiocyanate leach solution has a pH in a range of from pH 1 to pH 3 and the feed of the thiocyanate leach solution comprises of from 0.005 to 0.05 mole per liter of the dissolved thiocyanate;
the mineral material feed comprises at least 3 weight percent sulfide sulfur and at least 0.1 weight percent of the copper;
the precious metal comprises gold and during the thiocyanate leaching, a majority of the gold is dissolved into the thiocyanate leach solution in the form of precious metal-thiocyanate complex;
the recovering comprises solvent extraction from the liquid effluent of a majority of the copper dissolved in the liquid effluent.

### Claim 104 (depends on 103)

The method of claim 103, wherein feed of the thiocyanate leach solution to the thiocyanate leaching comprises dissolved ferric iron and a molar ratio of the dissolved ferric iron to the dissolved thiocyanate of at least 2.

### Claim 105 (depends on 104)

The method of claim 104, wherein the feed of the thiocyanate leach solution comprises at least 0.05 mole per liter of the dissolved ferric iron.