# US 2009/0275487 A1 · Additive for increasing the density of an oil-based fluid and fluid comprising such additive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275487 A1
- Document ID: US20090275487A1
- Status: Published application
- Kind: A1
- Application number: 12/421,351
- Filed: 2009-04-09
- Published: 2009-11-05
- Earliest claimed: 1996-07-24
- Assignees: M-I L.L.C.
- Inventors: Andrew J. Bradbury; Jarrod Massam; Christopher A. Sawdon
- Web page: https://patentgrep.com/patent/US20090275487A1

## CPC

- C09K 8/32: Non-aqueous well-drilling compositions, e.g. oil-based
- C09K 3/00: Materials not provided for elsewhere
- C09K 8/032: {Inorganic additives}
- C09K 8/035: Organic additives
- C09K 8/16: characterised by the inorganic compounds other than clay
- C09K 2208/18: Bridging agents, i.e. particles for temporarily filling the pores of a formation; Graded salts
- Y10S 507/901: Organically modified inorganic solid
- Y10S 507/904: Process of making fluids or additives therefor
- Y10S 507/906: Solid inorganic additive in defined physical form
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method of formulating a wellbore fluid that includes grinding a solid particulate material and a polymeric dispersing agent to provide a resulting polymer coated solid material, and suspending the resulting polymer coated solid material in the wellbore fluid. At least a portion of the resulting polymer coated solid material has a particle diameter less than 2.0 microns, wherein the polymeric dispersing agent has a molecular weight greater than 10,000. Exemplary starting materials for the solid material include weighting agents including barite, calcium carbonate, dolomite, ilmenite, hematite or other iron ores, olivine, siderite and strontium sulfate as well as mixture and combinations of these and other similar weighting materials. The dispersant in one illustrative embodiment is a polymeric acrylate ester made from the monomers of stearyl methacrylate, butyacrylate, and acrylic acid.

## Claims

### Claim at position 1

-22. (canceled)

### Claim 23

A method of making a wellbore fluid, the method comprising:
grinding a solid particulate material and a polymeric dispersing agent to provide a resulting polymer coated solid material, wherein at least a portion of the resulting polymer coated solid material has a particle diameter less than 2.0 microns, and wherein the polymeric dispersing agent has a molecular weight greater than 10,000; and
suspending the polymer coated wellbore additive colloidal solid material in the wellbore fluid.

### Claim 24 (depends on 23)

The method of claim 23, wherein the polymeric dispersing agent is a polymeric acrylate ester made from the monomers of stearyl methacrylate, butyacrylate, and acrylic acid.

### Claim 25 (depends on 23)

The method of claim 23, wherein the grinding is carried out in the presence of an oleaginous base fluid.

### Claim 26 (depends on 23)

The method of claim 23, wherein the solid material is selected from the group consisting of barite, calcium carbonate, dolomite, ilmenite, iron ores olivine, siderite, strontium sulfate, and combinations thereof.

### Claim 27 (depends on 23)

The method of claim 23, wherein greater than 25% of the polymer coated colloidal solid material has a particle diameter less than 2 microns.

### Claim 28 (depends on 23)

The method of claim 23, wherein at least 60% of the polymer coated colloidal solid material has a particle diameter less than 2 microns.

### Claim 29

A method of making a wellbore fluid, the method comprising:
grinding a solid particulate material and a polymeric dispersing agent, such that the polymeric dispersing agent coats the surface of the resulting colloidal solid particles, wherein the resulting polymer coated solid material has a weight average particle diameter of less than about 2 microns, and wherein the polymeric dispersing agent is a polymeric acrylate ester made from the monomers of stearyl methacrylate, butyacrylate, and acrylic acid; and
increasing the density the wellbore fluid with the resulting polymer coated solid material.

### Claim 30 (depends on 29)

The method of claim 29, further comprising selecting the solid particulate material to have specific gravity of at least 2.68.

### Claim 31 (depends on 29)

The method of claim 29, wherein the solid material is selected from the group consisting of barite, calcium carbonate, dolomite, ilmenite, iron ores, olivine, siderite, strontium sulfate, and combinations thereof.

### Claim 32 (depends on 29)

The method of claim 29, wherein the grinding is carried out in the presence of an oleaginous base fluid.

### Claim 33 (depends on 32)

The method of claim 32, wherein the base fluid is selected from the group consisting of: diesel oil, mineral oil, white oil, n-alkanes, synthetic oils, saturated and unsaturated poly(alpha-olefins), esters of fatty acid carboxylic acids and combinations thereof.