# US 2009/0275202 A1 · Silicon structure having an opening which has a high aspect ratio, method for manufacturing the same, system for manufacturing the same, and program for manufacturing the same, and method for manufacturing etching mask for the silicon structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275202 A1
- Document ID: US20090275202A1
- Status: Published application
- Kind: A1
- Application number: 12/515,726
- Filed: 2007-09-19
- Published: 2009-11-05
- Earliest claimed: 2006-11-22
- Inventors: Masahiko Tanaka; Akimitsu Oishi
- Web page: https://patentgrep.com/patent/US20090275202A1

## CPC

- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 50/242: {of Group IV materials}
- H10P 50/244: {comprising alternated and repeated etching and passivation steps}
- H10P 50/283: {by chemical means}
- H10P 70/20: {Cleaning during device manufacture}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Provided are a silicon structure having an opening which has a high aspect ratio and an etching mask for forming the silicon structure. A step of performing hole etching or trench etching of silicon so as to substantially expose a portion of at least a bottom surface of etched silicon and a step of forming a silicon oxide film by a CVD method on the silicon structure formed by the step of performing the hole etching or the trench etching are conducted. Thereafter, a step of exposing the formed silicon oxide film to a gas containing a hydrogen fluoride vapor is conducted. Further, the above-mentioned step of performing the hole etching or the trench etching is conducted again.

## Claims

### Claim 1

A method for manufacturing a silicon structure having an opening which has a high aspect ratio, the method comprising the steps of:
performing hole etching or trench etching of silicon so as to substantially expose a portion of at least a bottom surface of etched silicon;
forming a silicon oxide film by a CVD method on the silicon structure formed by the step of performing the hole etching or the trench etching;
exposing the silicon oxide film to a gas containing a hydrogen fluoride vapor after the step of forming the silicon oxide film; and
performing again the hole etching or the trench etching after the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor.

### Claim 2

A method for manufacturing a silicon structure having an opening which has a high aspect ratio, the method comprising the steps of:
performing hole etching or trench etching of silicon by plasma generated by alternately rendering an etching gas and an organic deposit forming gas in a plasma state or generated by mixing the etching gas and the organic deposit forming gas;
etching, by plasma generated by using oxygen or an oxygen-containing gas, an organic deposit on the silicon structure formed by the step of performing the hole etching or the trench etching;
forming a silicon oxide film on the silicon structure by a CVD method after the step of etching the organic deposit;
exposing the silicon oxide film to a gas containing a hydrogen fluoride vapor after the step of forming the silicon oxide film; and
performing again the hole etching or the trench etching after the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor.

### Claim 3 (depends on 2)

The method for manufacturing the silicon structure according to claim 2, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a hole is greater than or equal to 15.

### Claim 4 (depends on 2)

The method for manufacturing the silicon structure according to claim 2, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a trench is greater than or equal to 30.

### Claim 5 (depends on 2)

The method for manufacturing the silicon structure according to claim 2, wherein the silicon structure which has undergone the hole etching or the trench etching includes a resist mask before the hole etching or the trench etching is initially performed.

### Claim 6 (depends on 2)

The method for manufacturing the silicon structure according to claim 2, wherein a shortest width of an entrance of the hole is less than or equal to 30 μm.

### Claim 7 (depends on 2)

The method for manufacturing the silicon structure according to claim 2, wherein a shortest width of an entrance of the trench is less than or equal to 15 μm.

### Claim at position 8

8-13. (canceled)

### Claim 14

A program for manufacturing a silicon structure having an opening which has a high aspect ratio, comprising the steps of:
performing hole etching or trench etching of silicon so as to substantially expose a portion of at least a bottom surface of etched silicon;
forming a silicon oxide film by a CVD method on the silicon structure formed by the step of performing the hole etching or the trench etching;
exposing the silicon oxide film to a gas containing a hydrogen fluoride vapor after the step of forming the silicon oxide film; and
performing again the hole etching or the trench etching after the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor.

### Claim 15

A program for manufacturing a silicon structure having an opening which has a high aspect ratio, comprising the steps of:
performing hole etching or trench etching of silicon by plasma generated by alternately rendering an etching gas and an organic deposit forming gas in a plasma state or generated by mixing the etching gas and the organic deposit forming gas;
etching, by plasma generated by using oxygen or an oxygen-containing gas, an organic deposit on the silicon structure formed by the step of performing the hole etching or the trench etching;
forming a silicon oxide film on the silicon structure by a CVD method after the step of etching the organic deposit;
exposing the silicon oxide film to a gas containing a hydrogen fluoride vapor after the step of forming the silicon oxide film; and
performing again the hole etching or the trench etching after the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor.

### Claim 16 (depends on 15)

A storage medium having stored therein a manufacturing program according to claim 15.

### Claim 17 (depends on 15)

A system for manufacturing a silicon structure having an opening which has a high aspect ratio, comprising a controller controlled by using a manufacturing program according to claim 15.

### Claim 18

A method for manufacturing an etching mask for a silicon structure having an opening which has a high aspect ratio, the method comprising the steps of:
forming a silicon oxide film by a CVD method on a silicon structure which has undergone etching of a hole or etching of a trench and whose silicon of at least a bottom surface of the hole or the trench is substantially exposed; and
exposing the silicon oxide film to a gas containing a hydrogen fluoride vapor after the step of forming the silicon oxide film.

### Claim 19

A method for manufacturing an etching mask for a silicon structure having an opening which has a high aspect ratio, the method comprising the steps of:
etching an organic deposit, by plasma generated by using oxygen or an oxygen-containing gas, on a silicon structure for which hole etching or trench etching has been performed by plasma generated by alternately rendering an etching gas and an organic deposit forming gas in a plasma state or generated by mixing the etching gas and the organic deposit forming gas;
forming a silicon oxide film on the silicon structure by a CVD method after the step of etching the organic deposit; and
exposing the silicon oxide film to a gas containing a hydrogen fluoride vapor after the step of forming the silicon oxide film.

### Claim 20

A method for manufacturing an etching mask for a silicon structure having an opening which has a high aspect ratio, the method comprising the steps of:
etching an organic deposit, by plasma generated by using oxygen or an oxygen-containing gas, on a silicon structure for which hole etching or trench etching has been performed by plasma generated by alternately rendering an etching gas and an organic deposit forming gas in a plasma state or generated by mixing the etching gas and the organic deposit forming gas;
forming a silicon oxide film on the silicon structure by a CVD method after the step of etching the organic deposit;
exposing the silicon oxide film to a gas containing a hydrogen fluoride vapor after the step of forming the silicon oxide film; and
repeating at least once more, after a step of performing the hole etching or the trench etching, the steps of etching the organic deposit, of forming the silicon oxide film, and of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor.

### Claim 21 (depends on 20)

The method for manufacturing the etching mask according to claim 20, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a hole is greater than or equal to 15.

### Claim 22 (depends on 20)

The method for manufacturing the etching mask according to claim 20, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a trench is greater than or equal to 30.

### Claim 23 (depends on 20)

The method for manufacturing the etching mask according to claim 20, wherein the silicon structure which has undergone the hole etching or the trench etching includes a resist mask before the hole etching or the trench etching is initially performed.

### Claim 24 (depends on 20)

The method for manufacturing the etching mask according to claim 20, wherein a shortest width of an entrance of the hole is less than or equal to 30 μm.

### Claim 25 (depends on 20)

The method for manufacturing the etching mask according to claim 20, wherein a shortest width of an entrance of the trench is less than or equal to 15 μm.

### Claim 26 (depends on 1)

The method for manufacturing the silicon structure according to claim 1, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a hole is greater than or equal to 15.

### Claim 27 (depends on 1)

The method for manufacturing the silicon structure according to claim 1, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a trench is greater than or equal to 30.

### Claim 28 (depends on 1)

The method for manufacturing the silicon structure according to claim 1, wherein the silicon structure which has undergone the hole etching or the trench etching includes a resist mask before the hole etching or the trench etching is initially performed.

### Claim 29 (depends on 1)

The method for manufacturing the silicon structure according to claim 1, wherein a shortest width of an entrance of the hole is less than or equal to 30 μm.

### Claim 30 (depends on 1)

The method for manufacturing the silicon structure according to claim 1, wherein a shortest width of an entrance of the trench is less than or equal to 15 μm.

### Claim 31 (depends on 11)

The silicon structure, according to claim 11, having an opening which has a high aspect ratio,
the silicon structure formed by repeating at least once more the steps of: forming the silicon oxide film; thereafter, exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor; and thereafter, performing the hole etching or the trench etching.

### Claim 32 (depends on 14)

A storage medium having stored therein a manufacturing program according to claim 14.

### Claim 33

A system for manufacturing a silicon structure having an opening which has a high aspect ratio, comprising a controller controlled by using a manufacturing program according to claim.

### Claim 34 (depends on 18)

The method for manufacturing the etching mask according to claim 18, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a hole is greater than or equal to 15.

### Claim 35 (depends on 18)

The method for manufacturing the etching mask according to claim 18, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a trench is greater than or equal to 30.

### Claim 36 (depends on 18)

The method for manufacturing the etching mask according to claim 18, wherein the silicon structure which has undergone the hole etching or the trench etching includes a resist mask before the hole etching or the trench etching is initially performed.

### Claim 37 (depends on 18)

The method for manufacturing the etching mask according to claim 18, wherein a shortest width of an entrance of the hole is less than or equal to 30 μm.

### Claim 38 (depends on 18)

The method for manufacturing the etching mask according to claim 18, wherein a shortest width of an entrance of the trench is less than or equal to 15 μm.

### Claim 39 (depends on 19)

The method for manufacturing the etching mask according to claim 19, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a hole is greater than or equal to 15.

### Claim 40 (depends on 19)

The method for manufacturing the etching mask according to claim 19, wherein the step of forming the silicon oxide film and the step of exposing the silicon oxide film to the gas containing the hydrogen fluoride vapor are conducted when an aspect ratio of a trench is greater than or equal to 30.

### Claim 41 (depends on 19)

The method for manufacturing the etching mask according to claim 19, wherein the silicon structure which has undergone the hole etching or the trench etching includes a resist mask before the hole etching or the trench etching is initially performed.

### Claim 42 (depends on 19)

The method for manufacturing the etching mask according to claim 19, wherein a shortest width of an entrance of the hole is less than or equal to 30 μm.

### Claim 43 (depends on 19)

The method for manufacturing the etching mask according to claim 19, wherein a shortest width of an entrance of the trench is less than or equal to 15 μm.