# US 2009/0275200 A1 · Technique for reducing topography-related irregularities during the patterning of a dielectric material in a contact level of closely spaced transistors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275200 A1
- Document ID: US20090275200A1
- Status: Published application
- Kind: A1
- Application number: 12/372,006
- Filed: 2009-02-17
- Published: 2009-11-05
- Earliest claimed: 2008-04-30
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Ralf Richter; Heike Salz; Robert Seidel
- Web page: https://patentgrep.com/patent/US20090275200A1

## CPC

- H10P 14/60: of insulating materials
- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 64/68: characterised by the insulator, e.g. by the gate insulator
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 50/283: {by chemical means}
- Y02P 80/30: Reducing waste in manufacturing processes; Calculations of released waste quantities
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

In a dual stress liner approach, the surface conditions after the patterning of a first stress-inducing layer may be enhanced by appropriately designing an etch sequence for substantially completely removing an etch stop material, which may be used for the patterning of the second stress-inducing dielectric material, while, in other cases, the etch stop material may be selectively formed after the patterning of the first stress-inducing dielectric material. Hence, the dual stress liner approach may be efficiently applied to semiconductor devices of the 45 nm technology and beyond.

## Claims

### Claim 1

A method, comprising:
forming a layer stack above first and second conductive lines formed in a device level of a semiconductor device, said layer stack comprising a first stress-inducing layer and an etch stop layer formed above said first stress-inducing layer;
forming a mask so as to expose said second conductive lines and cover said first conductive lines;
performing an etch sequence for removing an exposed portion of said layer stack and reducing surface topography in a space between adjacent two of said second conductive lines;
forming a second stress-inducing dielectric layer above said second conductive lines and said space of reduced topography and on a portion of said etch stop layer located above said first conductive lines; and
selectively removing said second stress-inducing dielectric layer from above said first conductive lines by using said etch stop layer as an etch stop.

### Claim 2 (depends on 1)

The method of claim 1, wherein said first and second conductive lines have a line width of approximately 50 nm or less.

### Claim 3 (depends on 1)

The method of claim 1, further comprising forming a bottom etch stop layer as a first layer of said layer stack prior to forming said first stress-inducing layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein removing said layer stack comprises reducing a width of sidewall spacer elements formed on sidewalls of said second conductive lines.

### Claim 5 (depends on 4)

The method of claim 4, wherein said etch sequence comprises performing a first etch process on the basis of a selective etch chemistry that has a higher etch rate for said etch stop layer compared to said first stress-inducing layer.

### Claim 6 (depends on 1)

The method of claim 1, further comprising introducing an etch indicator species into a surface of said first stress-inducing dielectric layer prior to forming said etch stop layer.

### Claim 7 (depends on 6)

The method of claim 6, further comprising controlling at least one etch process of said etch sequence on the basis of said etch indicator species.

### Claim 8 (depends on 1)

The method of claim 1, wherein reducing a topography of said space comprises rounding corners of a recess formed between said adjacent two of said second conductive lines.

### Claim 9 (depends on 1)

The method of claim 1, wherein said first dielectric layer is formed with an internal tensile stress level and said second stress-inducing layer is formed with an internal compressive stress level.

### Claim 10

A method, comprising:
forming a layer stack above first and second conductive lines formed in a device level of a semiconductor device, said layer stack comprising a first stress-inducing layer and an etch stop layer formed above said first stress-inducing layer;
forming a mask so as to expose said second conductive lines and cover said first conductive lines;
performing an etch sequence to remove said first stress-inducing layer and said etch stop layer from above said second conductive lines and reduce a width of sidewall spacer elements formed on sidewalls of said second conductive lines;
forming a second stress-inducing dielectric layer above said second conductive lines and on a portion of said etch stop layer located above said first conductive lines; and
selectively removing said second stress-inducing dielectric layer from above said first conductive lines by using said etch stop layer as an etch stop.

### Claim 11 (depends on 10)

The method of claim 10, wherein performing said etch sequence comprises performing a first etch process to expose at least a portion of said first stress-inducing layer and performing a second etch process to remove a portion of said first stress-inducing dielectric layer.

### Claim 12 (depends on 10)

The method of claim 10, further comprising introducing an etch indicator species into a surface of said first stress-inducing dielectric layer prior to forming said etch stop layer and controlling at least one etch process of said sequence on the basis of said etch indicator species.

### Claim 13 (depends on 10)

The method of claim 10, further comprising rounding corners of a recess formed in an isolation region between adjacent two of said second conductive lines.

### Claim 14 (depends on 10)

The method of claim 10, further comprising introducing an etch indicator material in a surface portion of said device level prior to forming said first stress-inducing layer.

### Claim 15 (depends on 10)

The method of claim 10, further comprising forming a bottom etch stop layer as a first layer of said layer stack prior to forming said first stress-inducing dielectric layer.

### Claim 16 (depends on 10)

The method of claim 10, wherein said first dielectric layer is formed with an internal tensile stress level and said second stress-inducing layer is formed with an internal compressive stress level.

### Claim 17 (depends on 10)

The method of claim 10, wherein said first dielectric layer is formed with an internal compressive stress level and said second stress-inducing layer is formed with an internal tensile stress level.

### Claim 18

A method, comprising:
depositing a first stress-inducing layer above a plurality of first transistors and a plurality of second transistors;
forming a first portion of said first stress-inducing layer by selectively removing said first stress-inducing layer from above said plurality of second transistors;
treating a surface portion of said first portion so as to form an etch control layer;
forming a second stress-inducing layer above said plurality of first and second transistors; and
selectively removing said second stress-inducing layer from above said plurality of first transistors by performing a removal process and using said etch control layer for controlling said removal process.

### Claim 19 (depends on 18)

The method of claim 18, wherein treating said surface portion of the first stress-inducing layer is performed in an oxidizing plasma ambient.

### Claim 20 (depends on 18)

The method of claim 18, wherein said etch control layer is formed so as to have a thickness of less than approximately 10 nm.

### Claim 21 (depends on 19)

The method of claim 19, wherein said plasma ambient is established at a process temperature of approximately 400° C. or less.

### Claim 22 (depends on 18)

The method of claim 18, wherein said first stress-inducing layer has an internal tensile stress level.

### Claim 23 (depends on 18)

The method of claim 18, wherein said first stress-inducing layer has an internal compressive stress level.

### Claim 24 (depends on 18)

The method of claim 18, wherein a gate length of said plurality of first and second transistors is approximately 50 nm or less.