# US 2009/0275189 A1 · Method for manufacturing silicon on sapphire wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275189 A1
- Document ID: US20090275189A1
- Status: Published application
- Kind: A1
- Application number: 12/458,321
- Filed: 2009-07-08
- Published: 2009-11-05
- Earliest claimed: 2005-03-18
- Assignees: Oki Semiconductor Co., Ltd.
- Inventors: Kimiaki Shimokawa
- Web page: https://patentgrep.com/patent/US20090275189A1

## CPC

- H10P 90/1914: {using bonding}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10D 86/03: wherein the substrate comprises sapphire, e.g. silicon-on-sapphire [SOS]
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention provides an SOS wafer comprising a non-transparent polysilicon layer provided on a back surface of a sapphire substrate, a silicon nitride layer which protects the polysilicon layer, and a stress relaxing film which cancels stress produced in the silicon nitride layer, wherein the silicon nitride layer and the stress relaxing film are provided on the back surface side.

## Claims

### Claim 1

A method for manufacturing an SOS wafer provided with a sapphire substrate, comprising the steps of:
forming a polysilicon layer over the sapphire substrate;
implanting an impurity for applying conductivity in a polysilicon layer on a back surface of the sapphire substrate to form a conductive diffusion region;
forming a silicon nitride layer for protecting the polysilicon layer, on the back surface side of the sapphire substrate; and
forming a stress relaxing film for canceling stress of the silicon nitride layer, on the back surface side of the sapphire substrate.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said stress relaxing film forming step is performed prior to said silicon nitride layer forming step.

### Claim 3 (depends on 2)

The method according to claim 2, wherein when the silicon nitride layer is in a tensile stress state, said stress relaxing film forming step is set as a step for forming a silicon nitride film by a plasma CVD method.

### Claim 4 (depends on 3)

The method according to claim 3, wherein an Si—H concentration determined from an infrared absorption peak of the silicon nitride film is less than or equal to 10×1021/cm3, and a low wavenumber-end wavenumber of an Si—H absorption peak at infrared absorption of the silicon nitride film is greater than or equal to 1960/cm.

### Claim 5 (depends on 1)

The method according to claim 1, wherein said stress relaxing film forming step is performed after said silicon nitride layer forming step.

### Claim 6 (depends on 5)

The method according to claim 5, wherein when the silicon nitride layer is in a tensile stress state, said stress relaxing film forming step is set as a step for forming a silicon nitride film by a plasma CVD method.

### Claim 7 (depends on 6)

The method according to claim 6, wherein an Si—H concentration determined from an infrared absorption peak of the silicon nitride film is less than or equal to 10×1021/cm3, and a low wavenumber-end wavenumber of an Si—H absorption peak at infrared absorption of the silicon nitride film is greater than or equal to 1960/cm.

### Claim 8 (depends on 2)

The method according to claim 2, wherein when the silicon nitride layer is in a tensile stress state, said stress relaxing film forming step is set as a step for forming a silicon oxide film by a plasma CVD method.

### Claim 9 (depends on 5)

The method according to claim 5, wherein when the silicon nitride layer is in a tensile stress state, said stress relaxing film forming step is set as a step for forming a silicon oxide film by a plasma CVD method.