# US 2009/0275172 A1 · Stacking semiconductor device and production method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275172 A1
- Document ID: US20090275172A1
- Status: Published application
- Kind: A1
- Application number: 12/501,939
- Filed: 2009-07-13
- Published: 2009-11-05
- Earliest claimed: 2005-08-31
- Assignees: Canon Kabushiki Kaisha
- Inventors: TAKEHIRO SUZUKI; YASUSHI TAKEUCHI
- Web page: https://patentgrep.com/patent/US20090275172A1

## CPC

- H10W 90/00: Package configurations
- H10W 70/60: Insulating or insulated package substrates; Interposers; Redistribution layers (leadframes H10W70/40)
- H10W 72/332: {Plan-view shape, i.e. in top view}
- H10W 72/834: {Interconnections on sidewalls of chips}
- H10W 72/877: {Bump connectors and die-attach connectors}
- H10W 72/884: {Die-attach connectors and bond wires}
- H10W 72/90: Bond pads, in general
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/20: Configurations of stacked chips
- H10W 90/22: the stacked chips being on both top and bottom sides of a package substrate, interposer or RDL
- H10W 90/28: the stacked chips having different sizes, e.g. chip stacks having a pyramidal shape
- H10W 90/721: {of bump connectors}
- H10W 90/722: {between stacked chips}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/732: {between stacked chips}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/754: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In a stacking semiconductor device in which a first-layer and a second-layer semiconductor devices are stacked and bonded with a solder, warpage occurs due to a difference in thermal expansion coefficient of constituent members or a difference in elastic modulus of individual members. Therefore, between the first-layer and the second-layer semiconductor devices are provided an external connection terminal of solder and a thermosetting resin, and the stacking semiconductor device is heated at 150 to 180° C., which are the temperatures of preheating for reflow of the solder, for 30 to 90 seconds. Thereby the warpage of the first-layer semiconductor device is reduced and the thermosetting resin is cured completely in this state. Then, the temperature is raised to a reflow temperature of the solder and solder bonding using the external connection terminal is performed. Thereby, the bonding reliability of a solder-bonded portion of the stacking semiconductor device is considerably improved.

## Claims

### Claim at position 1

-8. (canceled)

### Claim 9

A method of producing a stacked semiconductor device having a first-layer semiconductor device and a second-layer semiconductor device formed by being staked on each other, comprising the steps of:
disposing the second-layer semiconductor device on the first-layer semiconductor device which is warped providing, between a first-layer semiconductor device and a second-layer semiconductor device, solder and a thermosetting resin for bonding the first-layer semiconductor device and the second-layer semiconductor device;
heating the first-layer semiconductor device and the second-layer semiconductor device to a first temperature at which the first-layer semiconductor device has a flat shape to cure the thermosetting resin;
heating the first-layer semiconductor device and the second-layer semiconductor device to a second temperature which is higher than the first temperature to melt the solder; and
cooling the first-layer semiconductor device and the second-layer semiconductor device to solidify the solder.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the curing temperature of the thermosetting resin is 150 to 180° C. and the heating time is 30 to 90 seconds.