# US 2009/0275166 A1 · Method for manufacturing infrared detecting device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275166 A1
- Document ID: US20090275166A1
- Status: Published application
- Kind: A1
- Application number: 12/382,067
- Filed: 2009-03-06
- Published: 2009-11-05
- Earliest claimed: 2008-03-11
- Assignees: Oki Semiconductor Co., Ltd.
- Inventors: Taikan Iinuma
- Web page: https://patentgrep.com/patent/US20090275166A1

## CPC

- G01J 5/02: Constructional details
- G01J 5/023: {Particular leg structure or construction or shape; Nanotubes}
- G01J 5/024: {Special manufacturing steps or sacrificial layers or layer structures}
- H10F 39/107: {having multiple elements covered by H10F30/00 in a repetitive configuration, e.g. radiation detectors comprising photodiode arrays}
- H10F 71/121: {The active layers comprising only Group IV materials}
- G01J 5/0853: {having infrared absorbers other than the usual absorber layers deposited on infrared detectors like bolometers, wherein the heat propagation between the absorber and the detecting element occurs within a solid}
- H10F 39/014: {of CMOS image sensors}
- H10F 39/184: {Infrared image sensors}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- G01J: MEASUREMENT OF INTENSITY, VELOCITY, SPECTRAL CONTENT, POLARISATION, PHASE OR PULSE CHARACTERISTICS OF INFRARED, VISIBLE OR ULTRAVIOLET LIGHT; COLORIMETRY; RADIATION PYROMETRY (light sources F21, H01J, H01K, H05B; investigating properties of materials by optical means G01N)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A semiconductor layer is prepared in which a silicon substrate, a BOX layer and an SOI layer are laminated in this order. A silicon diode section used as an infrared detection portion is formed in the SOI layer. Further, an isolation portion is formed so as to extend from the SOI layer to a predetermined depth of the silicon substrate via the BOX layer. The isolation portion is formed so as to surround an area in which the silicon diode section is formed, and have the form of a circle or a regular polygon more than a regular pentagon in shape. A protective film is formed on the surface of the SOI layer. Thereafter, etching holes that penetrate the protective film, the SOI layer and the BOX layer are formed. The silicon substrate corresponding to each area surrounded by the isolation portion is etched using the etching holes.

## Claims

### Claim 1

A method for manufacturing an infrared detecting device, comprising:
preparing an SOI substrate provided with a silicon layer over a support substrate through an oxide layer interposed therebetween;
forming a isolation layer which surrounds an infrared detection portion forming area formed in the SOI substrate and extends from the silicon layer to a predetermined depth of the support substrate through the oxide layer;
forming a protective film over the surface of the silicon layer corresponding to the infrared detection portion forming area;
forming through holes which penetrate the silicon layer, the oxide layer and the protective film; and
etching the support substrate corresponding to the infrared detection portion forming area surrounded by the isolation layer to a predetermined depth of the support substrate using the through holes,
wherein the isolation layer has a circular form or a form of a regular polygonal more than a regular pentagon in shape.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in the through hole forming step, one of the through holes is formed in a central part of the infrared detection portion forming area or the through holes are formed in plural form at equal intervals on a circumference with the center of the infrared detection portion forming area as the center.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the isolation layer has an orthohexagonal shape at the surface of the silicon layer.

### Claim 4 (depends on 1)

The method according to any one of claim 1, wherein the infrared detection portion forming area and other infrared detection portion forming areas are separated by the isolation layer.

### Claim 5 (depends on 1)

The method according-to any one of claim 1, further including:
forming an infrared reflection layer for reflecting infrared radiation over the protective film, and
forming an infrared absorbing portion over the infrared reflection layer.

### Claim 6 (depends on 1)

The method according to any one of claim 1, wherein infrared detection portions formed in the adjoining infrared detection portion forming areas separated by the isolation layer are respectively electrically connected via a metal layer uncovered with the protective film, further including:
forming a conduction preventing film over the protective film and the metal layer,
forming an infrared reflection layer for reflecting infrared radiation over the conduction preventing film, and
forming the infrared absorbing portion over the infrared reflection layer.

### Claim 7 (depends on 5)

The method according to claim 5, wherein in the infrared absorbing portion forming step, a sacrifice layer is formed over the infrared reflection layer and the sacrifice layer is removed after the formation of the infrared absorbing portion over the sacrifice layer, thereby forming the infrared absorbing portion in such a manner that space is formed between at least part of the infrared absorbing portion and the infrared reflection film.