# US 2009/0275148 A1 · Mitigation of edge degradation in ferroelectric memory devices through plasma etch clean

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275148 A1
- Document ID: US20090275148A1
- Status: Published application
- Kind: A1
- Application number: 12/502,571
- Filed: 2009-07-14
- Published: 2009-11-05
- Earliest claimed: 2006-05-30
- Assignees: Texas Instruments Incorporated
- Inventors: Kezhakkedath R. UDAYAKUMAR; Lindsey H. HALL; Francis G. CELII
- Web page: https://patentgrep.com/patent/US20090275148A1

## CPC

- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10D 1/694: {comprising noble metals or noble metal oxides}
- H10P 50/267: {using plasmas}
- H10P 70/23: {during, before or after processing of insulating materials}
- H10P 70/273: {the processing being a delineation of conductive layers, e.g. by RIE}
- H10B 53/00: Ferroelectric RAM [FeRAM] devices comprising ferroelectric memory capacitors
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A ferroelectric memory device is fabricated while mitigating edge degradation. A bottom electrode is formed over one or more semiconductor layers. A ferroelectric layer is formed over the bottom electrode. A top electrode is formed over the ferroelectric layer. The top electrode, the ferroelectric layer, and the bottom electrode are patterned or etched. A dry clean is performed that mitigates edge degradation. A wet etch/clean is then performed.

## Claims

### Claim 1

A method of fabricating a ferroelectric memory device, the method comprising:
forming a bottom electrode over one or more semiconductor layers;
forming a ferroelectric layer over the bottom electrode;
forming a top electrode over the ferroelectric layer;
selectively etching the top electrode;
selectively etching the ferroelectric layer;
performing a dry clean process subsequent to etching the ferroelectric layer with a plasma that generates isotropic fluoride species that react with debris to form residual reaction products; and
selectively etching the bottom electrode subsequent to performing the dry clean process.

### Claim 2 (depends on 1)

The method of claim 1, further comprising performing a wet clean process with phosphoric acid to remove the residual reaction products subsequent to performing the dry clean process.

### Claim 3 (depends on 1)

The method of claim 1, further comprising forming a bottom electrode diffusion barrier layer over one or more semiconductor layers prior to forming the bottom electrode.

### Claim 4 (depends on 1)

The method of claim 1, further comprising forming a hard mask on the top electrode covering a target portion of the top electrode prior to etching the top electrode.

### Claim 5 (depends on 1)

The method of claim 1, further comprising performing a second dry clean subsequent to selectively etching the bottom electrode diffusion barrier layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the plasma is comprised of CF4/O2.

### Claim 7 (depends on 1)

The method of claim 1, wherein the plasma is comprised of CF4/O2/Ar.