# US 2009/0275146 A1 · Method and apparatus for manufacturing device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0275146 A1
- Document ID: US20090275146A1
- Status: Published application
- Kind: A1
- Application number: 12/428,096
- Filed: 2009-04-22
- Published: 2009-11-05
- Earliest claimed: 2008-04-23
- Assignees: Ulvac, Inc.; Seiko Epson Corporation
- Inventors: Katsuo TAKANO; Takeshi KOKUBUN; Yutaka KOKAZE; Masahisa UEDA; Mitsuhiro ENDOU; Koukou SUU; Toshiya MIYAZAKI; Toshiyuki NAKAMURA
- Web page: https://patentgrep.com/patent/US20090275146A1

## CPC

- H10P 50/283: {by chemical means}
- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10P 50/266: {by vapour etching only}
- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for manufacturing a device, includes: (A) forming a first electrode layer on a substrate; (B) forming a ferroelectric layer on the first electrode layer; (C) forming a second electrode layer on the ferroelectric layer; (D) forming a mask having a predetermined pattern on the second electrode layer; (E) forming a memory element by selectively removing the first electrode layer, the ferroelectric layer, and the second electrode layer using the mask; and (F) removing the mask, where at least, the processes (D) and (E), or the processes (E) and (F) are continuously performed under a reduced pressure.

## Claims

### Claim 1

A method for manufacturing a device, comprising:
(A) forming a first electrode layer on a substrate;
(B) forming a ferroelectric layer on the first electrode layer;
(C) forming a second electrode layer on the ferroelectric layer;
(D) forming a mask having a predetermined pattern on the second electrode layer;
(E) forming a memory element by selectively removing the first electrode layer, the ferroelectric layer, and the second electrode layer using the mask; and
(F) removing the mask, wherein
at least, the processes (D) and (E), or the processes (E) and (F) are continuously performed under a reduced pressure.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the process (D) and the process (F) are performed at a normal temperature, and the process (E) is performed at a high temperature.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the process (D), the process (E), and the process (F) are continuously performed under a reduced pressure.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising:
(G) preheating the substrate at a stage previous to the process (E).

### Claim 5 (depends on 4)

The method according to claim 4, wherein a chamber in which the process (E) is performed is different from a chamber in which the process (G) is performed, and the process (E) and the process (G) are continuously performed under a reduced pressure.

### Claim 6 (depends on 1)

The method according to claim 1, wherein a gas remaining in the substrate is removed at a stage subsequent to the process (F) in a chamber different from the chamber in which the process (F) is performed.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the first electrode layer and the second electrode layer includes one, two, or more selected from the group consisting of platinum, iridium, ruthenium, rhodium, palladium, osmium, iridium oxide, ruthenium oxide, and strontium ruthenate, and wherein the ferroelectric layer is one selected from the group consisting of PZT (Pb(Zr, Ti)O3), SBT (SrBi2Ta2O9), BTO (Bi4Ti3O12), BLT ((Bi, La)4Ti3O12), and BTO (BaTiO3).

### Claim 8

An apparatus for manufacturing a device, comprising:
a transfer chamber including a transfer mechanism transferring a substrate;
a normal-temperature etching chamber coupled to the transfer chamber;
a high-temperature etching chamber coupled to the transfer chamber; and
one or more load lock chambers coupled to the transfer chamber, wherein the transfer mechanism continuously transfers the substrate between the normal-temperature etching chamber, the high-temperature etching chamber, and the load lock chamber under vacuum.

### Claim 9 (depends on 8)

The apparatus according to claim 8, further comprising:
an ashing chamber; and
a pre-heat chamber, wherein either or both of the ashing chamber and the pre-heat chamber is provided at the transfer chamber, and the transfer mechanism continuously transfers the substrate under vacuum between the ashing chamber, the pre-heat chamber, the normal-temperature etching chamber, the high-temperature etching chamber, and the load lock chamber.